JPH0222242Y2 - - Google Patents

Info

Publication number
JPH0222242Y2
JPH0222242Y2 JP1983053930U JP5393083U JPH0222242Y2 JP H0222242 Y2 JPH0222242 Y2 JP H0222242Y2 JP 1983053930 U JP1983053930 U JP 1983053930U JP 5393083 U JP5393083 U JP 5393083U JP H0222242 Y2 JPH0222242 Y2 JP H0222242Y2
Authority
JP
Japan
Prior art keywords
cracks
cut
round
cuts
board
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP1983053930U
Other languages
Japanese (ja)
Other versions
JPS59160207U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP5393083U priority Critical patent/JPS59160207U/en
Publication of JPS59160207U publication Critical patent/JPS59160207U/en
Application granted granted Critical
Publication of JPH0222242Y2 publication Critical patent/JPH0222242Y2/ja
Granted legal-status Critical Current

Description

【考案の詳細な説明】 樹木を輪切にして、乾燥させると、割れ目がは
いつてしまう、建築用木材の様に樹木を板目や柾
目に引いた場合にも、割れ目がはいるが、これ
は、ひび割れ程度の物であるのに対して、輪切り
板の割れ目は、直径十六センチメートル程の物
で、周辺部分で三センチメートル以上の物が中心
部分から三角形状に出来てしまう。
[Detailed explanation of the idea] If you cut a tree into rings and dry it, cracks will appear.Cracks will also appear if the tree is cut into planks or straight grains like wood for construction. This is just a crack, whereas the crack in the round plate is about 16 centimeters in diameter, and a triangular shape of 3 centimeters or more is formed at the periphery from the center.

従来の輪切り台は、樹木の根部分を、斜めに切
つて作つた、樹木の根部分は、木の目が複雑にな
つているので、それを斜めに切る事で割れるのを
防ぐ事が出来る、でも、根は堀り出すのに手間が
かかり、又、根には石がはいつているので、これ
を取り出すのが、大変な仕事である。このように
して作つた、輪切り板は、高価な物となつてしま
う。
Traditional round cutting tables are made by cutting the roots of trees diagonally. Tree roots have a complicated grain pattern, so cutting diagonally can prevent them from splitting. It takes time to dig out the roots, and the roots are covered with stones, so removing them is a difficult task. The round plates made in this way end up being expensive.

輪切り板を、乾燥させると割れる、普通の状態
よりも多くの水を吸い込ませるとどうなるか、輪
切り板を水につけて、加熱させて、水を吸わせる
と、輪切り板は心を通つて、周辺部分に向かつて
割れがはいる、その割れ目は、心に近くの方が広
くなつている、そしてその輪切り板を乾燥させる
と、割れ目は、もとにもどり、見えなくなつた後
に、さらに乾燥させると、普通の輪切り板と同じ
様にして割れ目がはいる。
When a round board is dried, it cracks. What happens if you let it absorb more water than normal? If you soak a round board in water, heat it, and make it absorb water, the round board will pass through the heart and the surrounding area. Cracks appear towards the parts, and the cracks are wider near the heart.When the sliced board is dried, the cracks return to their original state and become invisible, and then they are dried further. Then, the cracks appear in the same way as a regular round board.

本考案は、図1の様に樹木を輪切りにした輪切
り板1の心2を通して切れ目3をいれる直径十六
センチメートル程度の輪切り板1ならば、心材部
分に長さ四センチメートル程度の切れ目3をいれ
る。
In this invention, as shown in Figure 1, if the cutting board 1 is about 16 centimeters in diameter and the cut 3 is made through the core 2 of the cutting board 1 which is made by cutting a tree into rings, then the cut 3 is about 4 centimeters long in the heartwood part. Insert.

切れ目3は、心2の近くが広く、両端がせまく
なつている様にあける、これは輪切り板1を乾燥
させると、心2附近の方が、縮まり方が大きいか
らである。
The cuts 3 are made so that they are wide near the core 2 and narrow at both ends.This is because when the round plate 1 is dried, it shrinks more near the core 2.

以上の様に切れ目3をいれた輪切り板1は乾燥
させても割れ目がはいる事がなくなり、切れ目3
をいれた部分も、心2の近くを広くした事でひび
割れ程度にしか見えない様になる、切れ目3を同
一幅にいれた場合には、心2附近が接する時にも
周辺近くの切れ目3は切れ目3が残り、周辺近く
の切れ目3が接する時には、割れ目がはいつてし
まう。
As mentioned above, even when the round plate 1 with the cut 3 is dried, there will be no cracks, and the cut 3
By widening the area near the core 2, the part where the slit 3 is inserted will look like nothing more than a crack.If the slit 3 is made the same width, even when the slit 2 is in contact with the slit 3, the slit 3 near the periphery will be Cuts 3 remain, and when the cuts 3 near the periphery touch, the cracks grow.

特に割れやすい樹木や変形している樹木には図
2の様に、切れ目3を二本入れると小ひびもはい
らない。
For trees that are particularly susceptible to breakage or deformed trees, making two cuts 3 as shown in Figure 2 will eliminate the need for small cracks.

輪切り板1を、水につけて加熱してやると割れ
目がはいりやすい部分に、ひび割れするので、そ
のひび割れ部分に切れ目3をいれると良い。
When the round plate 1 is soaked in water and heated, it will crack in areas where cracks are likely to enter, so it is best to make cuts 3 in those cracked areas.

切れ目3をいれる場合には、輪切り台にする時
の輪切り板1の裏面の切れ目3の方を、表面の切
れ目3よりも広くあけるのが、乾燥させた時に、
輪切り板1に割れをいれないで表面の切れ目3を
密着させるこつである、密着させると、切れ目3
は見えなくなる。
When making cuts 3, it is best to make the cuts 3 on the back side of the round cutting board 1 wider than the cuts 3 on the front side when used as a round cutting table.
The trick is to make the cut 3 on the surface of the round plate 1 stick together without creating any cracks.
becomes invisible.

切れ目3の幅は、周辺部分に近い部分で二ミリ
メートル程度、心2部分近くで七ミリメートル程
度が直径十六センチメートル程度の輪切り板1の
標準である。
The width of the cut 3 is about 2 mm near the periphery and about 7 mm near the center 2, which is the standard width for the cut plate 1 having a diameter of about 16 cm.

【図面の簡単な説明】[Brief explanation of drawings]

1図は、本考案の上面図である。2図は、本考
案の上面図である。3図は、本考案乾燥時の上面
図である。 1は、輪切り板、2は、心、3は、切れ目。
FIG. 1 is a top view of the present invention. FIG. 2 is a top view of the present invention. FIG. 3 is a top view of the present invention during drying. 1 is the round board, 2 is the heart, and 3 is the cut.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 図1の様に、輪切り板1の心材部分に、周辺部
分に向けて、切れ目3をいれる事で、乾燥させて
も、割れ目がはいるのを、防ぐとともに、心2附
近の切れ目3を広くする事で、切れ目3をひび割
れ程度にせばめる様にした輪切り板。
As shown in Figure 1, by making cuts 3 in the core of the round plate 1 toward the periphery, you can prevent cracks from forming even when drying, and make the cuts 3 near the core 2 wider. By doing this, the cut 3 is narrowed to the extent of a crack.
JP5393083U 1983-04-11 1983-04-11 Round cutting board Granted JPS59160207U (en)