Prior art keywords
molding
temperature
double
adhesive
attached
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP8166385U
Other languages
Japanese (ja)
Other versions
JPS61196847U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP8166385U priority Critical patent/JPH0348913Y2/ja
Publication of JPS61196847U publication Critical patent/JPS61196847U/ja
Application granted granted Critical
Publication of JPH0348913Y2 publication Critical patent/JPH0348913Y2/ja
Expired legal-status Critical Current

Links

Landscapes

  • Vehicle Interior And Exterior Ornaments, Soundproofing, And Insulation (AREA)
  • Adhesive Tapes (AREA)

Description

【考案の詳細な説明】 産業上の利用分野 本考案は、両面貼付けテープで車体に貼着固定
するモールデイングの改良に関するものである。
[Detailed Description of the Invention] Industrial Application Field The present invention relates to an improvement in molding that is attached and fixed to a vehicle body using double-sided adhesive tape.

従来の技術 一般に、第4図で示す如く軟質ポリ塩化ビニル
樹脂等を所定横断面形状の長尺材に押出し成形し
たボデイサイドモールデイングm1、ABS樹脂等
で所望の識別記号や模様を外表面に有するようイ
ンジエクシヨン成形したマークm2或いはポリウ
レタン樹脂等のエラストマー樹脂で形成したバン
パーモールデイングm3等(以下、総称して単に
「モールデイングM」という。)はクロロプレン樹
脂等の発泡シートで形成した基材の両面にアクリ
ル酸エステル樹脂等の感圧接着剤或いは粘着剤を
付着した所謂「両面貼付けテープ」を用いて、ド
アパネルや車体パネル、バンパー本体等に貼着固
定することが行われている。その両面貼付けテー
プは片面の接着剤或いは粘着剤でモールデイング
の底面に貼付け、他側面の接着剤または粘着剤を
剥離紙で被覆してモールデイングの貼着固定直前
に引き剥がすことにより露出する接着剤または粘
着剤で被取付体にモールデイングを押圧圧着する
ように備え付けられている。
Conventional technology In general, as shown in Fig. 4, body side molding m 1 is made by extruding soft polyvinyl chloride resin or the like into a long material with a predetermined cross section, and a desired identification symbol or pattern is applied to the outer surface using ABS resin or the like. Bumper molding M2 , etc. (hereinafter collectively referred to simply as ``molding M'') made of elastomer resin such as polyurethane resin or in-die extension molding mark M2 or bumper molding M3 made of elastomer resin such as polyurethane resin, etc., is made of a foamed sheet of chloroprene resin or the like. A so-called "double-sided adhesive tape" in which pressure-sensitive adhesives such as acrylic ester resins or adhesives are attached to both sides of a base material is used to attach and fix products to door panels, car body panels, bumper bodies, etc. . The double-sided adhesive tape is attached to the bottom of the molding with an adhesive or pressure-sensitive adhesive on one side, and the adhesive or adhesive on the other side is covered with release paper, which is peeled off just before the molding is attached and fixed to expose the adhesive. The molding is attached to the object to be attached by pressure using adhesive or adhesive.

考案が解決しようとする問題点 ところで、この両面貼付けテープでモールデイ
ングを被取付体に貼着固定するにあたり、被取付
体に対して最適の取付強度を確保するためには接
着剤または粘着剤を一定温度で加温して軟化させ
ると共に所定の押圧力で圧着することが必要であ
る。そのうち、押圧力については第5図で示す如
く工場内でゴムローラRのような適当な治工具で
モールデイングMを押圧することにより容易に解
決することができる。然し、温度についてはこれ
を所望通りに管理することはなかなか困難で、例
えばクロロプレン発泡基材の両面にアクリル酸エ
ステル樹脂を塗布した両面貼付けテープTを用い
る場合第6図のグラフで示すように押圧力が一定
でも温度変化で接着力が変りまた最も良好な接着
力を得るためには通常で10〜40℃程度にアクリル
酸エステルが加温されていることが必要である。
この温度管理はモールデイングのようにユーザー
の希望に応じて取付けるものでは各地のデイラー
が行わなければならないから必ずしも適確に行わ
れるとは限らず、特にその管理なしに冬期の低温
下で取付けられるものにあつては十分な接着強度
で貼着固定されずに離脱してしまい易いのが実情
である。
Problems that the invention aims to solve By the way, when attaching and fixing the molding to the object to be attached using this double-sided adhesive tape, it is necessary to use an adhesive or adhesive to ensure the optimum attachment strength to the object to be attached. It is necessary to soften the material by heating it at a constant temperature and to press it with a predetermined pressing force. Among them, the pressing force can be easily solved by pressing the molding M with a suitable tool such as a rubber roller R in the factory as shown in FIG. However, it is quite difficult to control the temperature as desired. For example, when using double-sided adhesive tape T in which acrylic ester resin is coated on both sides of a chloroprene foam base material, it is difficult to control the temperature as shown in the graph in Figure 6. Even if the pressure is constant, the adhesive strength changes with temperature changes, and in order to obtain the best adhesive strength, it is usually necessary to heat the acrylic ester to about 10 to 40°C.
This temperature control is not necessarily carried out properly in products that are installed according to the user's wishes, such as molding, because it has to be carried out by dealers in each region, and it is often installed at low temperatures in winter without any particular control. The reality is that when it comes to objects, they tend to fall off because they are not fixed with sufficient adhesive strength.

問題点を解決するための手段 本考案に係るモールデイングにおいては、温度
変化に応じて変色する判別標識を持つ剥離紙で片
面を被覆した両面貼付けテープを備えてなるもの
である。
Means for Solving the Problems The molding according to the present invention includes a double-sided adhesive tape whose one side is covered with a release paper having an identification mark that changes color according to temperature changes.

作 用 このモールデイングでは、温度変化に応じて変
色する判別標識を剥離紙に設けることにより両面
貼付けテープの接着剤または粘着剤を所定温度ま
で加温することを促せるものであり、また、その
温度を判別標識の変色で特定できるから温度管理
を極めて簡単にししかも両面貼付けテープの強固
な接着力で車体の必要個所に取付けられるように
なる。
Function This molding can promote heating of the adhesive or pressure-sensitive adhesive of the double-sided tape to a predetermined temperature by providing an identification mark on the release paper that changes color according to temperature changes. Since the temperature can be identified by the discoloration of the identification mark, temperature control is extremely simple, and the strong adhesive strength of the double-sided adhesive tape allows it to be attached to the required location on the vehicle body.

実施例 以下、第1〜3図を参照して説明すれば、次の
通りである。
Embodiments The following description will be made with reference to FIGS. 1 to 3.

このモールデイングMは軟質のポリ塩化ビニル
樹脂で押出し成形したボデイサイドモールデイン
グで、裏面側には両面貼付けテープ10が備え付
けられている。その両面貼付けテープ10はクロ
ロプレン樹脂の発泡シート11をベースにし、両
側面には接着剤或いは粘着剤の塗層12,13が
形成されている。これら塗層12,13のうち、
片面12はモールデイングMの裏面に両面貼付け
テープ10を貼着するに用いられており、他の片
面13はモールデイングMを被取付体に貼付け固
定するまでにゴミ等が付着するのを防止するべく
紙製の剥離紙(離型紙ともいう。)14で被覆さ
れている。その剥離紙14には、温度変化で変色
する判別標識15,15…が設けられている。こ
の判別標識15,15…は一定温度以下で有色を
呈しまたその一定温度を超えたときには白色の如
き他の色調を呈するものであり、両面貼付けテー
プ10の塗層12,13を例えばアクリル酸エス
テル樹脂で設けるときには10℃以上、好ましくは
20℃以上で有色を呈するよう形成するのが望まし
い。この判別標識15,15…は温度変化に応じ
て変色する塗料を剥離紙14に直接塗布すること
によりコーテイング部(1,2図参照)として形
成でき、または温度変化に応じて変色する塗料を
付着したラベル(第3図参照)を貼付けることに
よつても形成することができる。
This molding M is a body side molding extruded from a soft polyvinyl chloride resin, and a double-sided adhesive tape 10 is attached to the back side. The double-sided adhesive tape 10 is based on a foamed sheet 11 of chloroprene resin, and coating layers 12 and 13 of adhesive or pressure-sensitive adhesive are formed on both sides. Among these coating layers 12 and 13,
One side 12 is used to attach the double-sided adhesive tape 10 to the back side of the molding M, and the other side 13 is used to prevent dust from adhering to the molding M before it is attached and fixed to the object to be attached. It is covered with a release paper (also referred to as release paper) 14 made of paper. The release paper 14 is provided with discrimination marks 15, 15, . . . that change color due to temperature changes. These discrimination marks 15, 15... exhibit color when the temperature is below a certain temperature, and exhibit other colors such as white when the temperature exceeds the certain temperature. When using resin, the temperature should be 10°C or higher, preferably
It is desirable to form the film so that it becomes colored at 20°C or higher. These discrimination marks 15, 15... can be formed as a coating part (see Figures 1 and 2) by directly applying a paint that changes color according to temperature changes to the release paper 14, or by attaching a paint that changes color according to temperature changes. It can also be formed by pasting a labeled label (see Figure 3).

このように構成するモールデイングでは、車体
の所望個所に貼着固定するにあたつて、加熱する
ことにより塗層12,13を軟化させるようにす
る。その加熱に伴つて、判別標識15,15…は
一定温度を超えると変色するようになる。この変
色は塗層12,13が強固な接着力を発揮するに
最適な温度に達したことを示すもので、それを確
認した後に剥離紙14を引き剥がして塗層13を
被取付体に当てがうと共にゴムローラ等の押圧手
段で圧接すれば、塗層12,13でモールデイン
グMは確実にしかも確りと貼着固定できるように
なる。
In the molding constructed in this manner, the coating layers 12 and 13 are softened by heating before being attached and fixed to a desired location on the vehicle body. Along with the heating, the discrimination marks 15, 15, . . . begin to change color when the temperature exceeds a certain temperature. This discoloration indicates that the coating layers 12 and 13 have reached the optimum temperature for exhibiting strong adhesion, and after confirming this, the release paper 14 is peeled off and the coating layer 13 is applied to the object to be attached. If the coating layers 12 and 13 are applied together with pressure using a pressing means such as a rubber roller, the molding M can be reliably and securely adhered and fixed.

なお、上述した判別標識15,15…の変色温
度は加熱時に塗層12,13の帯熱がモールデイ
ングMに伝導して逃げることもあるので、最適温
度よりやや高めに設定するのが望ましい場合もあ
る。また、上述したモールデイングMとしてはボ
デイサイドモールデイングを例示したが、これ以
外にバンパーモールデイングやマークにも適用す
ることができしかも樹脂成形品以外にも金属、そ
の他の材質のモールデイングに適用することがで
きる。更に、両面貼付けテープは発泡シートを基
材にするものの他に、通常のフイルム状のものを
基材にしたものでも用いることができ、その強力
な接着力を発揮する塗層の帯熱温度は使用する接
着剤または粘着剤の種類によつて多少異なるもの
である。また、判別標識は単なる標識に限定され
ず注意書きのような文字をも含むことは言うまで
もない。
It should be noted that the discoloration temperature of the above-mentioned discrimination marks 15, 15... may be desirably set slightly higher than the optimum temperature since the heat of the coating layers 12, 13 may be conducted to the molding M and escape during heating. There is also. In addition, although body side molding is exemplified as the molding M mentioned above, it can also be applied to bumper moldings and marks, and can also be applied to moldings of metals and other materials other than resin molded products. can do. Furthermore, double-sided adhesive tapes can be used not only with foam sheets as the base material, but also with ordinary film-like materials as the base material, and the heating temperature of the coating layer that exhibits strong adhesive strength is It varies somewhat depending on the type of adhesive or adhesive used. Further, it goes without saying that the discrimination mark is not limited to a simple mark, but also includes characters such as cautionary notes.

考案の効果 以上の如く、本考案に係るモールデイングに依
れば、両面貼付けテープで強固な接着力を得る温
度管理を容易にしかも確実に行えるから、取付け
後に脱落等が発生するのを最少限に抑えることが
できるようになる。
Effects of the invention As described above, according to the molding according to the invention, it is possible to easily and reliably control the temperature to obtain strong adhesive force with double-sided adhesive tape, thereby minimizing the occurrence of falling off after installation. It will be possible to suppress the

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は本考案に係るモールデイングの底面側
を示す斜視図、第2図は同モールデイングの底面
側を示す一部拡大斜視図、第3図は別の実施例に
係るモールデイングの底面側を示す一部拡大斜視
図、第4図はモールデイングの取付け個所を示す
車体の斜視図、第5図はモールデイングのローラ
による圧着工程を示す説明図、第6図は両面貼付
けテープの帯熱温度と接着力との関係を示すグラ
フである。 10:両面貼付けテープ、14:剥離紙、1
5,15…:判別標識。
FIG. 1 is a perspective view showing the bottom side of a molding according to the present invention, FIG. 2 is a partially enlarged perspective view showing the bottom side of the same molding, and FIG. 3 is a bottom view of a molding according to another embodiment. FIG. 4 is a perspective view of the vehicle body showing the mounting location of the molding, FIG. 5 is an explanatory diagram showing the process of crimping the molding with rollers, and FIG. 6 is a strip of double-sided adhesive tape. It is a graph showing the relationship between thermal temperature and adhesive strength. 10: Double-sided adhesive tape, 14: Release paper, 1
5, 15...: Discrimination mark.

Claims (1)

【実用新案登録請求の範囲】 (1) 温度変化に応じて変色する判別標識を持つ剥
離紙で片面を被覆した両面貼付けテープを備え
てなることを特徴とするモールデイング。 (2) 上記判別標識が、温度変化に応じて変色する
塗料のコーテイング部で形成されているところ
の実用新案登録請求の範囲第1項記載のモール
デイング。 (3) 上記判別標識が、温度変化に応じて変色する
印刷ラベルを貼着することにより形成されてい
るところの実用新案登録請求の範囲第1項記載
のモールデイング。
[Scope of Claim for Utility Model Registration] (1) A molding characterized by comprising a double-sided adhesive tape covered on one side with a release paper having an identification mark that changes color in response to temperature changes. (2) The molding according to claim 1, wherein the discrimination mark is formed of a coating of paint that changes color according to temperature changes. (3) The molding according to claim 1, wherein the discrimination mark is formed by pasting a printed label that changes color according to temperature changes.
JP8166385U 1985-05-30 1985-05-30 Expired JPH0348913Y2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP8166385U JPH0348913Y2 (en) 1985-05-30 1985-05-30

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP8166385U JPH0348913Y2 (en) 1985-05-30 1985-05-30

Publications (2)

Publication Number Publication Date
JPS61196847U JPS61196847U (en) 1986-12-08
JPH0348913Y2 true JPH0348913Y2 (en) 1991-10-18

Family

ID=30628653

Family Applications (1)

Application Number Title Priority Date Filing Date
JP8166385U Expired JPH0348913Y2 (en) 1985-05-30 1985-05-30

Country Status (1)

Country Link
JP (1) JPH0348913Y2 (en)

Also Published As

Publication number Publication date
JPS61196847U (en) 1986-12-08

Similar Documents

Publication Publication Date Title
CA1091715A (en) Switch-proof pressure sensitive adhesive label
EP0569921B1 (en) Self-adhesive decorative surface covering material
US5737897A (en) Insulation board composite
US5209959A (en) Surface printable polyvinyl chloride laminate with carrier and application tape
JPH07323494A (en) label
US5217773A (en) Image protective film
US20140078236A1 (en) Thick, Printable Labels Suitable for Use in a Thermal Transfer Printer
JP2001234130A (en) Adhesive sheet and method for its manufacture
JPH08333556A (en) Transfer type tacky sheet material
JPH0348913Y2 (en)
CA2173847A1 (en) Self-adhesive wallcoverings
EP0246656B1 (en) Process for producing self adhesive sheet materials
KR100248854B1 (en) Color pattern cork plate for interior decoration of buildings
US4574098A (en) Pattern transposing tape
US3290206A (en) Curl resistant laminate
AU7362691A (en) Film composite having repositionable adhesive by which it can become permanently bonded to a plasticized substrate
JPH0423639Y2 (en)
JPH0725246Y2 (en) Adhesive tape for masking
JPH0613238Y2 (en) Adhesive tape or sheet for marking and masking
JPH06270261A (en) Method for producing high-definition laminated sheet
JPH0790231A (en) Adhesive sheet
JPH02210386A (en) Partial peeling method for sheet-like object
JP2526782Y2 (en) Extruded polystyrene resin laminate
JPS5962684A (en) Thin adhesive sheet
JPH1095073A (en) Film sticking close to smooth surface and its manufacture