WO2009127325A1 - Procédé de fabrication d’un document de sécurité ou de valeur - Google Patents

Procédé de fabrication d’un document de sécurité ou de valeur Download PDF

Info

Publication number
WO2009127325A1
WO2009127325A1 PCT/EP2009/002373 EP2009002373W WO2009127325A1 WO 2009127325 A1 WO2009127325 A1 WO 2009127325A1 EP 2009002373 W EP2009002373 W EP 2009002373W WO 2009127325 A1 WO2009127325 A1 WO 2009127325A1
Authority
WO
WIPO (PCT)
Prior art keywords
laser
paper substrate
marker
marking
film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/EP2009/002373
Other languages
German (de)
English (en)
Inventor
André Gregarek
Manfred Heim
Markus Krombholz
Annett Bähr
Bernhard Wiedner
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Giesecke and Devrient GmbH
Original Assignee
Giesecke and Devrient GmbH
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Giesecke and Devrient GmbH filed Critical Giesecke and Devrient GmbH
Priority to AT09732638T priority Critical patent/ATE546296T1/de
Priority to EP09732638A priority patent/EP2271501B1/fr
Publication of WO2009127325A1 publication Critical patent/WO2009127325A1/fr
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Abstract

L'invention concerne un procédé de fabrication d'un document de sécurité ou de valeur comprenant les étapes suivantes : B) Mise à disposition d'un stratifié (14, 18) composé d'au moins un substrat en papier (14) qui est muni d'une zone de marquage avec une substance de marquage pouvant être modifiée au laser et d'un élément de sécurité (18) présent dans la zone de marquage et pouvant être fragilisé sous l'effet du laser, et L) Exposition du stratifié (14, 18) à un rayonnement laser pour générer simultanément et de manière coïncidente des lignes d'affaiblissement (26) dans l'élément de sécurité (18) et des identifiants (22) dans le substrat en papier (18) par modification de la substance de marquage.
PCT/EP2009/002373 2008-04-16 2009-04-01 Procédé de fabrication d’un document de sécurité ou de valeur Ceased WO2009127325A1 (fr)

Priority Applications (2)

Application Number Priority Date Filing Date Title
AT09732638T ATE546296T1 (de) 2008-04-16 2009-04-01 Verfahren zur herstellung eines sicherheits- oder wertdokuments
EP09732638A EP2271501B1 (fr) 2008-04-16 2009-04-01 Procédé de fabrication d un document de sécurité ou de valeur

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
DE102008019092A DE102008019092A1 (de) 2008-04-16 2008-04-16 Verfahren zur Herstellung eines Sicherheits- oder Wertdokuments
DE102008019092.6 2008-04-16

Publications (1)

Publication Number Publication Date
WO2009127325A1 true WO2009127325A1 (fr) 2009-10-22

Family

ID=41058970

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/EP2009/002373 Ceased WO2009127325A1 (fr) 2008-04-16 2009-04-01 Procédé de fabrication d’un document de sécurité ou de valeur

Country Status (4)

Country Link
EP (1) EP2271501B1 (fr)
AT (1) ATE546296T1 (fr)
DE (1) DE102008019092A1 (fr)
WO (1) WO2009127325A1 (fr)

Cited By (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2011117472A1 (fr) * 2010-03-25 2011-09-29 Upm-Kymmene Corporation Papier de sécurité et procédé pour la fabrication d'un papier de sécurité
US20160108581A1 (en) * 2013-05-10 2016-04-21 Fábrica Nacional De Moneda Y Timbre - Real Case De La Moneda Method of providing a security document with a security feature, and security document
US9321294B2 (en) 2012-01-23 2016-04-26 Leonhard Kurz Stiftung & Co. Kg Security document and method for producing a security document
DE202017103832U1 (de) 2017-06-21 2017-07-20 Ovd Kinegram Ag Transferfolie, Laminierfolie und Folienelement
EP3279004A1 (fr) * 2016-08-04 2018-02-07 Giesecke+Devrient Currency Technology GmbH Élément de sécurité, procédé de fabrication d'un élément de sécurité ainsi que document de valeur pourvu d'un tel élément de sécurité
EP3279006A1 (fr) * 2016-08-03 2018-02-07 Giesecke+Devrient Currency Technology GmbH Procédé de fabrication d'un élément de sécurité
DE102022001403A1 (de) 2021-11-04 2023-05-04 Giesecke+Devrient Currency Technology Gmbh Transfer-Sicherheitselement-Material und Wertdokument mit einem Sicherheitselement
WO2023078582A1 (fr) 2021-11-04 2023-05-11 Giesecke+Devrient Currency Technology Gmbh Matériau d'élément de sécurité de transfert et document de valeur comprenant un élément de sécurité
DE102022001402A1 (de) 2022-04-25 2023-10-26 Giesecke+Devrient Currency Technology Gmbh Verfahren zum Übertragen eines Sicherheitselements auf ein Zielsubstrat

Families Citing this family (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE102008046513A1 (de) 2008-09-10 2010-04-29 Giesecke & Devrient Gmbh Verfahren zur Herstellung eines Sicherheits-oder Wertdokuments
PT2991839T (pt) 2013-06-26 2019-09-19 Fabrica Nac De Moneda Y Timbre Real Casa De La Moneda Método de fornecimento de um documento de segurança com uma funcionalidade de segurança e um documento de segurança
CN103572659B (zh) * 2013-09-24 2016-03-09 广东冠豪高新技术股份有限公司 一种防伪无碳复写纸及制备方法
DE102016002120A1 (de) * 2016-02-24 2017-08-24 Giesecke & Devrient Gmbh Sicherheitsmerkmal und Verfahren zu dessen Herstellung
DE102016006931A1 (de) * 2016-06-06 2017-12-07 Giesecke+Devrient Currency Technology Gmbh Sicherheitsmerkmal und Verfahren zu dessen Herstellung
DE102016006929A1 (de) * 2016-06-06 2017-12-07 Giesecke+Devrient Currency Technology Gmbh Sicherheitsmerkmal und Verfahren zu dessen Herstellung
DE102016015378A1 (de) * 2016-12-22 2018-06-28 Giesecke+Devrient Currency Technology Gmbh Verfahren zur Herstellung eines Wertdokuments
DE102019006255A1 (de) * 2019-09-04 2021-03-04 Giesecke+Devrient Currency Technology Gmbh Gegen Spaltung geschütztes Sicherheitspapier und Wertdokument

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2002003104A2 (fr) * 2000-07-03 2002-01-10 Optaglio Limited Structure optique
US6827283B2 (en) * 2000-09-21 2004-12-07 Orga Kartensysteme Gmbh Product with a security element
WO2005108109A1 (fr) * 2004-05-05 2005-11-17 Giesecke & Devrient Gmbh Document de valeur
US20060127649A1 (en) * 2002-09-19 2006-06-15 Mario Keller Security paper

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4343885A (en) 1978-05-09 1982-08-10 Dynachem Corporation Phototropic photosensitive compositions containing fluoran colorformer
IL85760A (en) 1987-03-19 1991-06-10 Xytronyx Inc Systems for the visualization of exposure to ultraviolet radiation and for the utilization of ultraviolet radiation to effect color changes
GB0114266D0 (en) 2001-06-12 2001-08-01 Ciba Sc Holding Ag Laser marking method

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2002003104A2 (fr) * 2000-07-03 2002-01-10 Optaglio Limited Structure optique
US6827283B2 (en) * 2000-09-21 2004-12-07 Orga Kartensysteme Gmbh Product with a security element
US20060127649A1 (en) * 2002-09-19 2006-06-15 Mario Keller Security paper
WO2005108109A1 (fr) * 2004-05-05 2005-11-17 Giesecke & Devrient Gmbh Document de valeur

Cited By (13)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2011117472A1 (fr) * 2010-03-25 2011-09-29 Upm-Kymmene Corporation Papier de sécurité et procédé pour la fabrication d'un papier de sécurité
US9321294B2 (en) 2012-01-23 2016-04-26 Leonhard Kurz Stiftung & Co. Kg Security document and method for producing a security document
DE102012001121C5 (de) * 2012-01-23 2018-01-04 Leonhard Kurz Stiftung & Co. Kg Sicherheitsdokument, Verfahren zur Herstellung eines Sicherheitsdokuments und Verfahren zur Herstellung eines individualisierten Sicherheitsdokuments
US9938667B2 (en) 2013-05-10 2018-04-10 Fábrica Nacional de Moneda y Timbre-Real Casa de la Moneda Method of providing a security document with a security feature, and security document
US20160108581A1 (en) * 2013-05-10 2016-04-21 Fábrica Nacional De Moneda Y Timbre - Real Case De La Moneda Method of providing a security document with a security feature, and security document
EP3279006A1 (fr) * 2016-08-03 2018-02-07 Giesecke+Devrient Currency Technology GmbH Procédé de fabrication d'un élément de sécurité
EP3279004A1 (fr) * 2016-08-04 2018-02-07 Giesecke+Devrient Currency Technology GmbH Élément de sécurité, procédé de fabrication d'un élément de sécurité ainsi que document de valeur pourvu d'un tel élément de sécurité
DE202017103832U1 (de) 2017-06-21 2017-07-20 Ovd Kinegram Ag Transferfolie, Laminierfolie und Folienelement
DE102017113787A1 (de) 2017-06-21 2018-12-27 Ovd Kinegram Ag Verfahren zur Herstellung einer Transferfolie, Verfahren zur Herstellung eines Folienelements sowie Transferfolie, Laminierfolie und Folienelement
DE102022001403A1 (de) 2021-11-04 2023-05-04 Giesecke+Devrient Currency Technology Gmbh Transfer-Sicherheitselement-Material und Wertdokument mit einem Sicherheitselement
WO2023078582A1 (fr) 2021-11-04 2023-05-11 Giesecke+Devrient Currency Technology Gmbh Matériau d'élément de sécurité de transfert et document de valeur comprenant un élément de sécurité
DE102022001402A1 (de) 2022-04-25 2023-10-26 Giesecke+Devrient Currency Technology Gmbh Verfahren zum Übertragen eines Sicherheitselements auf ein Zielsubstrat
WO2023208416A1 (fr) 2022-04-25 2023-11-02 Giesecke+Devrient Currency Technology Gmbh Procédé de transfert d'un élément de sécurité sur un substrat cible

Also Published As

Publication number Publication date
EP2271501B1 (fr) 2012-02-22
DE102008019092A1 (de) 2009-10-22
EP2271501A1 (fr) 2011-01-12
ATE546296T1 (de) 2012-03-15

Similar Documents

Publication Publication Date Title
EP2271501B1 (fr) Procédé de fabrication d un document de sécurité ou de valeur
EP2646256B1 (fr) Support de données à marquage
EP2454100B1 (fr) Procédé de fabrication d'un corps multicouche et corps multicouche
EP2164707A1 (fr) Signe de sécurité et son procédé de réalisation
EP0866750A1 (fr) Feuille susceptible d'etre inscrite au moyen d'un faisceau laser
EP2379339A1 (fr) Support de données à zone transparente
EP2342084A1 (fr) Procédé de fabrication d'un document de sécurité ou de valeur
EP2199095B1 (fr) Elément de sécurité pour support de données et son procédé de fabrication
EP3215371B1 (fr) Support de données comprenant un élément de sécurité transparent
WO2009065630A1 (fr) Feuille pouvant être imprimée par laser
EP1826728A2 (fr) Elément de sécurité pouvant être marqué au laser
EP2465703B1 (fr) Elément de sécurité à couleur variable structuré
DE10006377A1 (de) Mit einem Laser beschriftetes Etikett sowie Verfahren und Vorrichtung zu seiner Herstellung
DE102008046462A1 (de) Verfahren zur Herstellung einer mehrschichtigen Folie
DE102014115910A1 (de) Etikett zum Beschriften mit einer zunächst verborgenen Innenbeschriftung
EP4041568B1 (fr) Matériau de transfert d'élément de sécurité, son procédé de fabrication et utilisation
DE102015005672A1 (de) Sicherheitsmerkmal und Verfahren zu dessen Herstellung
EP3279003B1 (fr) Élément de sécurité et procédé de fabrication d'un élément de sécurité
EP3243669A2 (fr) Élément de sécurité et son procédé de fabrication
EP1926791A1 (fr) Ruban auto-adhesif
EP3789207B1 (fr) Papier de sécurité et document de sécurité protégés contre la coupure
EP4214063A1 (fr) Matériau de transfert d'éléments de sécurité permettant le transfert, dans un bon registre, d'éléments de sécurité à des documents de valeur
DE102016006931A1 (de) Sicherheitsmerkmal und Verfahren zu dessen Herstellung
DE202004004040U1 (de) Sicherheitsaufkleber

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 09732638

Country of ref document: EP

Kind code of ref document: A1

DPE1 Request for preliminary examination filed after expiration of 19th month from priority date (pct application filed from 20040101)
NENP Non-entry into the national phase

Ref country code: DE

WWE Wipo information: entry into national phase

Ref document number: 2009732638

Country of ref document: EP