ATE462523T1 - Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen,fehlerreduzierten schweissnaht - Google Patents

Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen,fehlerreduzierten schweissnaht

Info

Publication number
ATE462523T1
ATE462523T1 AT02737228T AT02737228T ATE462523T1 AT E462523 T1 ATE462523 T1 AT E462523T1 AT 02737228 T AT02737228 T AT 02737228T AT 02737228 T AT02737228 T AT 02737228T AT E462523 T1 ATE462523 T1 AT E462523T1
Authority
AT
Austria
Prior art keywords
weld
welds
ductile
ductile iron
welding
Prior art date
Application number
AT02737228T
Other languages
English (en)
Inventor
Daniel Copeland
David Farr
James Wren
Original Assignee
Us Pipe And Foundry Company Ll
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Us Pipe And Foundry Company Ll filed Critical Us Pipe And Foundry Company Ll
Application granted granted Critical
Publication of ATE462523T1 publication Critical patent/ATE462523T1/de

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B23MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
    • B23KSOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
    • B23K9/00Arc welding or cutting
    • B23K9/23Arc welding or cutting taking account of the properties of the materials to be welded
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B23MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
    • B23KSOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
    • B23K35/00Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
    • B23K35/22Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
    • B23K35/24Selection of soldering or welding materials proper
    • B23K35/30Selection of soldering or welding materials proper with the principal constituent melting at less than 1550°C
    • B23K35/3033Ni as the principal constituent
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B23MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
    • B23KSOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
    • B23K35/00Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
    • B23K35/22Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
    • B23K35/38Selection of media, e.g. special atmospheres for surrounding the working area
    • B23K35/383Selection of media, e.g. special atmospheres for surrounding the working area mainly containing noble gases or nitrogen

Landscapes

  • Engineering & Computer Science (AREA)
  • Mechanical Engineering (AREA)
  • Chemical & Material Sciences (AREA)
  • Materials Engineering (AREA)
  • Physics & Mathematics (AREA)
  • Plasma & Fusion (AREA)
  • Arc Welding In General (AREA)
AT02737228T 2001-05-29 2002-05-29 Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen,fehlerreduzierten schweissnaht ATE462523T1 (de)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
US09/866,258 US6730876B2 (en) 2001-05-29 2001-05-29 Highly ductile reduced imperfection weld for ductile iron and method for producing same
PCT/US2002/016813 WO2002096590A1 (en) 2001-05-29 2002-05-29 Highly ductile reduced imperfection weld for ductile iron and method for producing same

Publications (1)

Publication Number Publication Date
ATE462523T1 true ATE462523T1 (de) 2010-04-15

Family

ID=25347240

Family Applications (1)

Application Number Title Priority Date Filing Date
AT02737228T ATE462523T1 (de) 2001-05-29 2002-05-29 Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen,fehlerreduzierten schweissnaht

Country Status (6)

Country Link
US (1) US6730876B2 (de)
EP (1) EP1390173B1 (de)
JP (1) JP2004527381A (de)
AT (1) ATE462523T1 (de)
DE (1) DE60235804D1 (de)
WO (1) WO2002096590A1 (de)

Families Citing this family (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4551082B2 (ja) * 2003-11-21 2010-09-22 三菱重工業株式会社 溶接方法
FR2886314B1 (fr) 2005-05-26 2007-07-20 Industeel France Acier pour coques de sous-marins a soudabilite renforcee
DE102005035585B3 (de) * 2005-07-29 2006-08-10 Areva Np Gmbh Verfahren zur Herstellung einer Schweißverbindung sowie Verfahren zur Reparatur einer derartigen Schweißverbindung
US20080216989A1 (en) * 2007-03-07 2008-09-11 Behr America Inc. Weld bead reinforcement of charge air cooler headers and method of making same
EP2387481B1 (de) * 2008-12-10 2018-03-14 Boston Scientific Scimed, Inc. Verfahren zum verbinden von titanlegierung und stahllegierung und medizinisches bauteil mit einer solchen verbindung
DE102010031890B3 (de) * 2010-07-21 2011-11-10 Benteler Automobiltechnik Gmbh Verfahren zum Herstellen einer stoffschlüssigen Verbindung und Hohlprofilverbindung
US10974349B2 (en) * 2010-12-17 2021-04-13 Magna Powertrain, Inc. Method for gas metal arc welding (GMAW) of nitrided steel components using cored welding wire
US9126287B2 (en) * 2012-03-12 2015-09-08 Siemens Energy, Inc. Advanced pass progression for build-up welding
ITMI20131271A1 (it) * 2013-07-29 2015-01-30 D G Weld S R L Metodo per il rivestimento in materiale metallico di corpi in ghisa sferoidale e piani per stampi per macchine della pressofusione di alluminio realizzato con tale metodo
US12240199B2 (en) * 2021-11-12 2025-03-04 Nippon Steel Corporation Welded member
CN114669839A (zh) * 2022-03-29 2022-06-28 岭澳核电有限公司 焊缝修补方法

Family Cites Families (25)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US1589017A (en) 1918-10-11 1926-06-15 John C Lincoln Method and means for electric-arc welding
US2547872A (en) 1948-01-31 1951-04-03 Stacey Brothers Gas Constructi Welding torch
US2900490A (en) 1958-06-24 1959-08-18 Int Nickel Co Coated electrode for welding cast iron
US2995815A (en) * 1959-03-13 1961-08-15 Int Nickel Co Welding rod and method of making and welding with same
US3253950A (en) * 1962-05-01 1966-05-31 Eutectic Welding Alloys Flux-coated welding electrode
US3328557A (en) * 1964-01-09 1967-06-27 Eutectic Welding Alloys Nickel arc welding electrode
US3301997A (en) 1965-02-15 1967-01-31 Canada Iron Foundries Ltd Method of welding ductile iron
US3555239A (en) 1966-11-16 1971-01-12 William J Kerth Welding machine with digital pulse control
US3581053A (en) 1967-12-05 1971-05-25 Union Carbide Corp Synchro-arc metal transfer
US3803381A (en) 1971-12-22 1974-04-09 Dover Corp Arc welding gun
US3851143A (en) 1972-03-29 1974-11-26 Int Nickel Co Weld rod
US3778588A (en) 1972-03-29 1973-12-11 Int Nickel Co Self-shielding cored wire to weld cast iron
US3851142A (en) 1972-03-29 1974-11-26 Int Nickel Co Weld rod containing manganese
SU492394A1 (ru) 1973-07-19 1975-11-25 Ордена Ленина И Ордена Трудового Красного Знамени Институт Электросварки Им.Е.О.Патона Сварочна проволока
FR2251399B1 (de) * 1973-11-20 1978-12-01 Pont A Mousson
US4087673A (en) 1976-06-11 1978-05-02 Weld Mold Company Method of welding and electrode therefore
DE2700720C2 (de) * 1976-08-27 1982-06-24 Mitsubishi Denki K.K., Tokyo Verfahren zum Lichtbogen-Verbindungsschweißen
US4534793A (en) 1979-09-19 1985-08-13 Research Corporation Cast iron welding materials and method
US4624706A (en) * 1985-07-02 1986-11-25 Inco Alloys International, Inc. Weld wire from extruded nickel containing powder
US5242759A (en) * 1991-05-21 1993-09-07 Cook Incorporated Joint, a laminate, and a method of preparing a nickel-titanium alloy member surface for bonding to another layer of metal
FR2742368B1 (fr) * 1995-12-18 1998-03-06 Framatome Sa Procede de raccordement par soudage heterogene bout a bout de deux pieces de natures differentes et utilisations
FR2742369B1 (fr) * 1995-12-18 1998-03-06 Framatome Sa Procede de raccordement par soudage heterogene de deux pieces et utilisation
US5915743A (en) 1997-06-30 1999-06-29 The Boeing Company Metal spray tool repair system
US6335512B1 (en) * 1999-07-13 2002-01-01 General Electric Company X-ray device comprising a crack resistant weld
US6308882B1 (en) * 1999-09-13 2001-10-30 Dana Corporation Method for joining ductile iron and steel

Also Published As

Publication number Publication date
US6730876B2 (en) 2004-05-04
WO2002096590A1 (en) 2002-12-05
EP1390173A1 (de) 2004-02-25
EP1390173B1 (de) 2010-03-31
EP1390173A4 (de) 2008-02-27
JP2004527381A (ja) 2004-09-09
US20020179583A1 (en) 2002-12-05
DE60235804D1 (de) 2010-05-12

Similar Documents

Publication Publication Date Title
CA2823235C (en) High toughness weld metals with superior ductile tearing resistance
Durgutlu Experimental investigation of the effect of hydrogen in argon as a shielding gas on TIG welding of austenitic stainless steel
EP2911825B1 (de) Zusammengesetzter schweissdraht und verfahren zur herstellung
CN102985215B (zh) 用γ化元素以及含小于10%的氮气或氧气的气体对镀铝钢件的电弧/激光混合焊接方法
Costanza et al. Weldability of austenitic stainless steel by metal arc welding with different shielding gas
Kumar et al. Experimental investigation and optimization of TIG welding parameters on aluminum 6061 alloy using firefly algorithm
US20070221643A1 (en) Gas-less process and system for girth welding in high strength applications including liquefied natural gas storage tanks
CN111448029A (zh) 气体保护电弧焊焊丝和气体保护电弧焊方法
CN112171016A (zh) 一种奥氏体不锈钢nbg焊接工艺
ATE462523T1 (de) Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen,fehlerreduzierten schweissnaht
US9333580B2 (en) Gas-less process and system for girth welding in high strength applications
CN103476538B (zh) 用于焊接具有高镍含量的钢的药芯焊丝
US6570127B2 (en) Shielding gas mixture for MIG brazing
Torbati et al. Optimization procedures for GMAW of bimetal pipes
Costa et al. Inconel 625 weld claddings obtained by the GMAW-RE with rotating electrode
Torbati et al. Welding bimetal pipes in duplex stainless steel
US7217905B2 (en) Weld filler metal that reduces residual stress and distortion
JP2008000808A (ja) 低温靭性、耐低温割れ性、および全姿勢溶接時のビード形状が良好な高強度溶接金属
Kumar et al. Optimization of Process Parameters on Tig Welding to Enhance Mechanical Properties of AA-6351 T6 Alloy
JP2006026651A (ja) ステンレス鋼溶接用シールドガス
Patel et al. Experimental study of the effect of heat input on mechanical properties of TIG welded joints of SA516 grade 70 material
Muniraju et al. Litrature survey on on gas metal arc welding process
Houldcroft Welding process developments and future trends
Giudice et al. A Review on Fusion Welding of Dissimilar Ferritic/Austenitic Steels: Processing and Weld Metallurgy
Kumar et al. Shielding Gas Compositions

Legal Events

Date Code Title Description
RER Ceased as to paragraph 5 lit. 3 law introducing patent treaties