CN101805437A - 一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法 - Google Patents

一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法 Download PDF

Info

Publication number
CN101805437A
CN101805437A CN 201010151482 CN201010151482A CN101805437A CN 101805437 A CN101805437 A CN 101805437A CN 201010151482 CN201010151482 CN 201010151482 CN 201010151482 A CN201010151482 A CN 201010151482A CN 101805437 A CN101805437 A CN 101805437A
Authority
CN
China
Prior art keywords
printing ink
alcohol ester
molten
pure ester
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010151482
Other languages
English (en)
Inventor
张伟公
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 201010151482 priority Critical patent/CN101805437A/zh
Publication of CN101805437A publication Critical patent/CN101805437A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法。采用了分子量1500-3500的聚酯多元醇和聚醚多元醇脱水后与多异氰酸酯反应聚合而成。其合成工艺简单,生产出的油墨粘结性、润湿分散性、附着力等性能佳,色泽鲜艳,干燥速度快,印刷品无残留。使用范围广,可用于PET、PVC、BOPP、OPP等塑料薄膜上。

Description

一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法
一、技术领域
纯酯溶聚氨酯树脂以及纯酯溶油墨,具体的说就是一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法。
二、背景技术
溶剂型聚氨酯树脂(简称PU),在印刷行业已广泛应用。由于它本身有甲苯、丁酮溶剂存在,它就会污染环境、危害人们身体健康。特别是食品包装国家已强令禁止不让用甲苯、丁酮等有害溶剂。目前,印刷界还有一些醇溶树脂,因为它本身干燥慢,易残留,影响工作效率。
三、发明内容
为了解决上述不足,一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法,采用了分子量1500-3500的聚酯多元醇和聚醚多元醇脱水后与多异氰酸酯反应聚合而成。其固含量为30%。所用的溶剂为酯类溶剂。将合成的纯酯溶聚氨酯树脂再按比例用酯类溶剂和有机颜料配比后分散、研磨、包装成纯酯溶油墨。
采用本发明技术,提高了产品合格率、提高了生产效率,降低了成本,得到了客户的好评,具备了市场竞争力。
四、具体实施方式
下面结合实施例对本发明作进一步详细说明。
用了分子量1500-3500的聚酯多元醇10-50和聚醚多元醇30-80脱水后与多异氰酸酯20-60反应聚合而成,反应后加入酯类溶剂60-90,生成固含量为30%的纯酯溶聚氨酯树脂。再用纯酯溶聚氨酯树脂20-50加入酯类溶剂50-90加入有机颜料10-30分散后,研磨包装而成纯酯溶油墨。

Claims (3)

1.一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法,其特征是:采用了分子量1500-3500的聚酯多元醇和聚醚多元醇脱水后与多异氰酸酯反应聚合而成。其固含量为30%。
2.一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法,其特征是:合成纯酯溶聚氨酯树脂所有的溶剂为酯类溶剂。
3.一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法,其特征是:将合成纯酯溶聚氨酯树脂再按比例用酯类溶剂和有机颜料配比后分散、研磨、包装成纯酯溶油墨。
CN 201010151482 2010-04-13 2010-04-13 一种纯酯溶聚氨酯树脂以及纯酯溶油墨的制备方法 Pending CN101805437A (zh)