CS210309B1 - Polyvinylchloride-based mixtures with increased heroin resistance - Google Patents
Polyvinylchloride-based mixtures with increased heroin resistance Download PDFInfo
- Publication number
- CS210309B1 CS210309B1 CS579680A CS579680A CS210309B1 CS 210309 B1 CS210309 B1 CS 210309B1 CS 579680 A CS579680 A CS 579680A CS 579680 A CS579680 A CS 579680A CS 210309 B1 CS210309 B1 CS 210309B1
- Authority
- CS
- Czechoslovakia
- Prior art keywords
- parts
- antimony
- resistance
- weight
- phosphate
- Prior art date
Abstract
Predmetom vynálezu sú zmesi na báze chlorobsahujúcich polymérov so zvýšenou odolnosťou proti horeniu, odolnosťou proti tepelnému namáhaniu obsahujúce triarylfosfáty v kombinácii s organickými antimonitými zlúčeninami s vazbou Sb-S a dalšími běžnými přísadami používanými pri zpracovaní týchto polymérov.The subject of the invention are mixtures based on chlorine-containing polymers with increased resistance to fire, resistance to thermal stress, containing triaryl phosphates in combination with organic antimony compounds with a Sb-S bond and other common additives used in the processing of these polymers.
Description
210309 '1
Predmetom vynálezu sú zmesí na báze polyvinylchloridu so zvýšenou odolnostou voči ho-reniu a vysokou tepelnou stabilitou, v kterých sa tieto vlastnosti dosahujú použitím organic-kých esterov kyseliny fosforecnej v kombinácii s antimonitými estermi merkaptokarboxy1ovýchkyselin.
Polyméry vinylchloridu majú v dosledku vysokého obsahu chloru dostatocnú odolnost vocihoreniu. Prídavkom róznych typov zmakčovadiel /napr. organických esterov kyseliny ftalovej,adipovej, sebakovej/ v množstvách 20 až 150 dielov na 100 hmotnostných dielov polymeru sa do-sahuje modifikácia fyzikálne-mechanických a spracovatelských vlastností, ale v dosledku celko-vého poklesu obsahu chloru v zmesí výrazné stupa ich hořlavost. Toto zvýšenie hořlavostije nutné eliminovat najma u tých výrobkoch z polyvinyIchloridu, v ktorých sa vyžadujezvýšená odolnost voči horeniu, ako sú napr. banské dopravné pásy s krycou vrstvou z PVC,podlahoviny, klínové řemene, koženky a folie používané v dopravných prostriedkoch, nábytkár-skom priemysle a pod.
Možným riešením je použitie roznych typov halogénobsahujúcich organických zlúčehín /chlo-rované parafíny, deriváty hexachlorcyklopentadienu, hromované aromatické zlúčeniny/ samotnýchalebo ich kombinácii s anorganickými zlúceninamí /Sb2O^, O, boritany zinku/ ako přísad do zmesí polymérov vinylchloridu a běžných typov zmakčovadiel.
Známe sú tíež organické zlúčeniny antimonu, ktoré znižujú hořlavost polymérov, napr.antimonité deriváty alfa-hydroxykarboxy1ových kyselin /US pat. 3 657 179, US pat. 3 801 527/,alkalické soli antiraon-glýkolesterov /US pat. 3 944 586/.
Použitím týchto zlúčenin pre zníženie hořlavosti zmesí polymérov vinylchloridu sa ne-priaznivo ovplyvňujú mechanické vlastnosti zmesí, dochadza k poklesu mákčíacej účinnosti,k zhoršovaniu tepelnej a svetelnej stability, znášanlivosti zložíek zmesí a pod.
Známým sposobom zníženia hořlavosti polymérov vinylchloridu je použitie zmakčovadiel,ktoré zvyŠujú odolnost voči horeniu. K takým typom zmakčovadiel patria napr. trikrezy1fos fát,trixylenylfosfát, krezyldifenylfosfát, trioktylfosfát, tris/2-chlorety1/fosfát, tris/2,3-di-chlorpropyl/fosfát, brómovaný trikrezylfosfát a dalšie. Pomocou týchto fosforobsahujícichzmakčovadiel sa pri ich vyššom dávkovaní do polymérov vinylchloridu dosahuje zvýšenie odolnos-ti voči horeniu. Ich nevýhodou je, že v porovnaní so základnými typroi zmakčovadiel majú nižšiumákčiacu účinnost a zhoršujú tepelnú stabilitu zmesí. Preto pri ich použití je potřebné přidá-vat vačšie množstva tepelných stabilizátorov alebo použit účinnejšie typy kov-obsahujúcich/napr. Sn, Ba-Cd/ tepelných stabilizátorov. Výrazné zlepšenie odolnosti voči horeniu a súčasne zvýšenie tepelnej stability sa podlávynálezu dosiahne tým, že ako systém zmakčovadlo-retardér hořeníe-tepelný stabilizátor saku 100 hmotnostným dielom polyvinylchloridu přidá 10 až 100 hmotnostných dielov triarylfosfátuobecného vzorce /1/
v ktorom R představuje lineárny alebo rozvětvený alkyl s 1 až 4 atomami uhlíka alebo vodík a0,2 až 5 hmotnostných dielov organickej antimonitej zlúčeniny obecného vzorca /11/
Sb/SR^COOR1/3 /11/ v ktorom představuje alkyl s 1 až 12 atomami uhlíka alebo cykloalkyl s 5 až 7 atomami xihlí-2 ka a R alkylén s 1 až 4 atomami uhlíka, pričom v uvedenej kombinácii organická antimonitá zlú-čenina posobí súčasne ako vysokoúčinný tepelný stabilizátor a súčasne ako retardér horenia. 210309 2 K zvýšeniu odolnosti voči horeniu v měkčených polyraeroch vinylchloridu podlá vynálezudochádza v doeledku využitia efektu kombinácie retardačně účinných prvkov> ako je fosforv zraákčovadle, antimon v tepelnom stabilizátore a halogénom v polymere*
Typickým prikladom tepelných stabilizátorov na báze antimonu sú antimon-tris/ízooktyl-merkaptoacetát/, antimon-tris/butyl-3-merkaptopropionát/, antimon-tris/cyklohexylmerkaptoacetát/a zmesi uvedených zlúčenin. Žiadny z ostatných bežne používaných tepelných stabilizátorov nezvyšuje odolnost polymérov vinylchloridu voči horeniu so súčasným výrazným stabilizačhým účinkom, ako uvedené typyorganických zlúčenin antimonu.
Prikladom organických zlúčenin fosforu sú trikrezylfosfát, krezyldifenylfosfát, tris/t--butylfeny1/fosfát, tris/dodecylfeny1/fosfát, třis/izopropylfenyl/fosfát» izopropyldif enyl-fosfát» terč.butylfenyldifenylfosfát.
Zmesi na báze polymérov vinylchloridu s navrhovaným systémorn přísad podlá vynálezumdžu obsahovat rfalšie běžné přísady» ako sú plnívá, mazadlá» pigmenty, antístatiká,rfalšie typy zmákčovadiel» Světelné stabilizátory, antioxidanty, modifikátory a iné pomocnélátky používané při spracovatelskom procese. Výhodou navrhovaného systému přísad je možnost zniženia dávkovania zložiek v doeledkuich sýnergického pdsobenia, čo sa prejaví v ekonomických úsporách. Vysoká tepelná stabilitazaručuje bezpečné zpracovánie aj v náročných Zpracovatelských postupoch.
Kompozícia podlá vynálezu je univerzálně použitelná v najrožnejδích aplikáciach měkče-ných polymerav vinylchloridu a plastisolov na ich báze. Systém podlá vynálezu sa vyznačujedobrou znášanlivostou s polymérom a ostatnými běžnými přísadami. Vo finálnych výrobkochnedochádza k migrácii přísad a k vzniku zákalu.
Jednotlivé zložky systému sú obtiažne extrahovatelné, hydrolyticky a tepelne stabilněa počas životnosti výrobkov nedochádza k úbytkom účinných zložiek.
Vzhladom na vysokú tepelnú stabilitu pri použití navrhovaného systému nevznikajú prispracovaní prchavé produkty a látky negativné ovplyvhujúce životné prostredie. Jednotlivézložky systému sú technicky lahko dostupné a ekonomicky výhodné.
Spdsob rěalizácie vynálezu a výhody vyplývajúce z jeho použitia ozrejmujú následovněpříklady: Příklad 1 Připravili sa zmesi obsahujúce 100 hmotnostných dielov suspenzného polyviňylchlotidu, 70 hmotnostných dielov zmesného triacylfosfátu na báze izopropylfenolov, 0,5 hmotriosthéhodiela mazadla a 1,5 hmotnostného diela tepelného stabilizátore. Ako tepelný stabilizátor sapoužil antimon-tris/izooktylmerkaptoacetát/, ktorého účinok sa porovnal s dibuťylcinizooktylmerkaptoacetátora. Válcováním pri 150 °C po dobu 5 min sa s predzmesí připravili fólie k sta-noveniu tepelne-atabilizačnej účinnosti v stabilmetri a k stanoveniu transparentnosti napřístroji Leukometer. Lisováním pri 160 °C sa připravili vzorky na vyhodnotenie hořlavostistanovenej metodou limitného kyslíkového čísla podlá ČSN 64 0756. Výsledky su uvedenév nasledujúcej tabulke.
210309 '1
SUMMARY OF THE INVENTION The present invention provides polyvinyl chloride-based compositions with enhanced flame resistance and high thermal stability in which these properties are achieved using organic phosphoric acid esters in combination with antimony mercaptocarboxylic acid esters.
Polymers of vinyl chloride have a high resistance to burning due to their high chlorine content. By adding various types of softeners (e.g. organic phthalic acid, adipic acid, sebacic acid esters (in amounts of 20 to 150 parts per 100 parts by weight of polymer) have a modification of the physical-mechanical and processing properties, but their flammability is significantly increased due to the overall decrease in chlorine content. This increase in flammability needs to be eliminated in particular for those polyvinylchloride products in which increased flame resistance is required, such as mining conveyor belts with a PVC covering, flooring, V-belts, artificial leather and foils used in vehicles, furniture industry and so on.
A possible solution is the use of various types of halogen-containing organic compounds / chlorinated paraffins, derivatives of hexachlorocyclopentadiene, accumulated aromatic compounds (alone or in combination with inorganic compounds / Sb 2 O 3, 0, zinc borates) as additives to mixtures of vinyl chloride polymers and conventional types of wetters.
Also known are antimony organic compounds that reduce the flammability of polymers, e.g., antimonon derivatives of alpha-hydroxycarboxylic acids (US Pat. No. 3,657,179, U.S. Pat. No. 3,801,527), alkali salts of anti-clone glycols / US Pat. 3,944,586].
By using these compounds to reduce the flammability of the vinyl chloride polymer blends, the mechanical properties of the blends are adversely affected, the shrinkage efficiency decreases, the thermal and light stability deteriorates, the compatibility of the blend components, and the like.
A well-known method of reducing the flammability of vinyl chloride polymers is the use of softeners that increase flame resistance. Such types of softeners include, for example, tricrylphosphate, trixylenylphosphate, crezyldiphenylphosphate, trioctylphosphate, tris / 2-chloroethylphosphate, tris / 2,3-dichloropropyl / phosphate, brominated tricresylphosphate and others. By using these phosphor-containing lubricants, the higher the fire resistance of the vinyl chloride polymers is achieved by their higher dosage. Their disadvantage is that, compared to the basic types of softeners, they have lower absorption efficiency and impair the thermal stability of the compositions. Therefore, in their use, it is necessary to add more heat stabilizers or to use more efficient types of metal-containing (e.g. Sn, Ba-Cd / thermal stabilizers. Significant improvements in flame resistance and, at the same time, increased thermal stability are achieved by adding 10 to 100 parts by weight of the triarylphosphate of the formula (1) as a softener-flame retardant-thermal jacket stabilizer system of 100 parts by weight of polyvinyl chloride.
wherein R represents a linear or branched alkyl of 1 to 4 carbon atoms or hydrogen and 0.2 to 5 parts by weight of an organic antimony compound of the general formula (11)
In which the alkyl of 1 to 12 carbon atoms or cycloalkyl of 5 to 7 carbon atoms is present and R is an alkylene of 1 to 4 carbon atoms, wherein said organic antimony compound is simultaneously acts as a high-efficiency heat stabilizer and at the same time as a flame retardant. 210309 2 In order to increase the resistance to flame retardation in plasticized vinyl chloride polymers, the present invention makes use of the effect of combining retarding elements such as phosphorus in the cracker, antimony in the thermal stabilizer and halogen in the polymer.
Typical examples of antimony-based thermal stabilizers are antimony-tris (isooctyl) mercaptoacetate, antimony-tris / butyl-3-mercaptopropionate, antimony-tris / cyclohexylmercaptoacetate, and mixtures thereof. None of the other commonly used thermal stabilizers increases the flame resistance of vinyl chloride polymers with simultaneous significant stabilizing effect, such as said types of organic antimony compounds.
Examples of organic phosphorus compounds are tricresylphosphate, cresyl diphenylphosphate, tris / t-butylphenyl / phosphate, tris / dodecylphenyl / phosphate, tris / isopropylphenyl / phosphate, isopropyldiphenyl phosphate, tert-butylphenyldiphenyl phosphate.
Vinyl chloride based polymer blends with the proposed additive system may incorporate more conventional additives such as fillers, lubricants, pigments, antistatic agents, finer types of softeners, and light stabilizers, antioxidants, modifiers, and other auxiliaries used in the processing process. The advantage of the proposed additive system is the possibility of reducing the dosage of the ingredients in the most effective synergies, which will result in economic savings. High thermal stability guarantees safe processing even in demanding processing processes.
The composition of the invention is universally applicable in the most severe applications of softened vinyl chloride and plastisol polymers based thereon. The system according to the invention is characterized by a good compatibility with the polymer and other conventional additives. There is no migration of additives and haze in the final products.
The components of the system are difficult to extract, hydrolytically and thermally stable during the lifetime of the products there is no loss of active ingredients.
Because of the high thermal stability of the proposed system, volatile products and substances that do not affect the environment are not processed. The components of the system are technically easy to access and economically advantageous.
The following examples illustrate the invention and the advantages of its use: EXAMPLE 1 Mixtures of 100 parts by weight of suspension polyvinyl chloride, 70 parts by weight of isopropylphenol-based mixed triacylphosphate, 0.5 parts by weight of lubricant and 1.5 parts by weight of thermal stabilizer were prepared. The heat stabilizer used was antimony-tris / isooctylmercaptoacetate, the effect of which was compared with the dibutylcinococtylmercaptoacetator. By rolling at 150 ° C for 5 min, foils were prepared with the masterbatch to determine the thermal stabilization efficiency in the stabilizer and the transparency determined by the Leukometer. By pressing at 160 ° C, samples were prepared for evaluation of flammability determined by the limit oxygen number method according to ČSN 64 0756. The results are given in the following table.
Claims (2)