CS272518B1 - Thermo-oxidation stabilized dian - Google Patents
Thermo-oxidation stabilized dian Download PDFInfo
- Publication number
- CS272518B1 CS272518B1 CS832088A CS832088A CS272518B1 CS 272518 B1 CS272518 B1 CS 272518B1 CS 832088 A CS832088 A CS 832088A CS 832088 A CS832088 A CS 832088A CS 272518 B1 CS272518 B1 CS 272518B1
- Authority
- CS
- Czechoslovakia
- Prior art keywords
- dian
- thermo
- boric acid
- phosphates
- mixture
- Prior art date
Abstract
Řešení představuje formulaci termooxidačně stabilizovaného dianu, stabilizace je provedena přídavkem 0,01 až 1,0 % hmot. směsi kyseliny borité s její alkalickou solí, alkalickými fosforečnany, fosfornany, fosforitany, hexametafosforečnany, alkalickými cínatany, trifenylfosfinem nebo směsi uvedených látek, přičemž hmotnostní poměr kyseliny borité ve směsi s bazickými sloučeninami je 1 : 0,1 až 10.The solution represents a formulation of thermo-oxidatively stabilized diane, stabilization is carried out by adding 0.01 to 1.0% by weight of a mixture of boric acid with its alkaline salt, alkaline phosphates, phosphates, phosphites, hexametaphosphates, alkaline stannates, triphenylphosphine or a mixture of the above substances, with the weight ratio of boric acid in the mixture with basic compounds being 1:0.1 to 10.
Description
Vynález se týká termooxidačně stabilizovaného dianu vůči průběhu tepelného a oxidačního štěpení.The invention relates to a thermo-oxidatively stabilized dian against the course of thermal and oxidative cleavage.
Dian je důležitou surovinou především pro přípravu epoxidových pryskyřic a polykarbonátů. Podmínkou získání vysoce kvalitních epoxidových pryskyřic a polykarbonátů je především vysoká kvalita dianu, především ve vysokém obsahu ρ,ρ'-izoméru a nízkém obsahu monofenolů. I vysoce čistý dian je relativně labilní sloučeninou podléhající poměrně snadno působení tepla, kyslíku či stop kyselin. Schéma degradačních reakcí je velmi složité, přičemž se dian nejprve štěpí na izopropenylfenol, který přechází zčásti na izopropylřenol a zčásti na polymerní izopropenylfenoly. Reakce provází vznik fenolu a chinonů. Uvedené látky jsou při výrobě kvalitních epoxidových pryskyřic a polykarbonátů nežádoucí, usilovně se proto hledají cesty vedoucí ke zvýšení tepelné i oxidační stability dianu, zejména při teplotách nad teplotou tání. Podle stávajícího stavu techniky se dosahuje zvýšení termooxidační stability dianu přídavkem některých aditiv, jako je kyselina boritá, alkyltitanáty, ftalanhydrid, cínaté sole, epoxidovaný sojový olej a bis-/glycidyleter/dianu. Vůči účinkům stop kyselin je známo použití sekundárního fosforečnanu sodného, případně sec. a terč, fosforečnanů alkalických zemin. Uvedená aditiva, podle stávajícího stavu techniky, dovolují podstatně omezit štěpení dianu účinkem tepla, kyslíku či stop kyselosti, ale degradační reakce nejsou v potřebné míře retardovány. V současné době není takový způsob termooxidační stabilizace dianu, který by v plné míře uspokojoval potřeby výroby kvalitních epoxidových pryskyřic a polykarbonátů.Dian is an important raw material especially for the preparation of epoxy resins and polycarbonates. The condition for obtaining high-quality epoxy resins and polycarbonates is above all the high quality of dian, especially in the high content of ρ, ρ'-isomer and the low content of monophenols. Even highly pure dian is a relatively labile compound that is relatively easily exposed to heat, oxygen or trace acids. The scheme of degradation reactions is very complex, with dian first cleaving to isopropenylphenol, which is converted in part to isopropylrenol and in part to polymeric isopropenylphenols. The reaction is accompanied by the formation of phenol and quinones. These substances are undesirable in the production of high-quality epoxy resins and polycarbonates, so ways are being sought to increase the thermal and oxidative stability of dian, especially at temperatures above the melting point. According to the prior art, an increase in the thermo-oxidative stability of dian is achieved by the addition of certain additives such as boric acid, alkyl titanates, phthalic anhydride, tin salts, epoxidized soybean oil and bis- / glycidyl ether / dian. Due to the effects of trace acids, it is known to use secondary sodium phosphate, or sec. and a target of alkaline earth phosphates. Said additives, according to the prior art, make it possible to substantially reduce the cleavage of dian by the action of heat, oxygen or traces of acidity, but the degradation reactions are not retarded to the necessary extent. At present, there is no such method of thermo-oxidative stabilization of dian that would fully satisfy the needs of the production of high-quality epoxy resins and polycarbonates.
Rozsáhlými a náročnými výzkumnými pracemi bylo nyní nalezeno, že lze dosáhnout výborné termooxidační stability dianu, jestliže obsahuje 0,01 až 1 % hmot, směsi kyseliny borité s její alkalickou solí, nebo alkalickými fosforečnany, fosfornany, fosforitany, hexametafosforečnany, alkalickými cínatany, trifenylfosfinem nebo směsí uvedených bazických sloučenin, přičemž hmotnostní poměr směsi kyseliny borité s bazickými sloučeninami je 1 : 0,1 až 10.Extensive and demanding research has now found that excellent thermo-oxidative stability of dian can be achieved if it contains 0.01 to 1% by weight of a mixture of boric acid with its alkali salt or alkaline phosphates, phosphates, phosphates, hexametaphosphates, alkaline tinates, triphenylphosphine or mixtures of said basic compounds, the weight ratio of the mixture of boric acid to the basic compounds being 1: 0.1 to 10.
Z alkalických solí se používají s výhodou sodné a draselné soli, lze však použít ve zvláštních případech i lithné soli. Samotná kyselina boritá má sama o sobě jistý stabilizační efekt, ale způsobuje výrazný rozklad dianu, zejména vlivem silné acidity svých přechodových komplexů. Alkalické soli, trifenylfosfin, cínatany a směsi těchto bazických látek se projevují jako málo účinné termooxidační stabilizátory dianu. Je však pozoruhodné, že směsi kyseliny borité s uvedenými bazcickými látkami ve vyznačeném hmotnostním poměru, se projevují výrazným termooxidačním stabilizujícím efektem tavenin dianu. Je to dosud neznámý synergismus účinku. Stabilizační efekt směsi podle vynálezu se sleduje změnou optické propustnosti 40 % etanolického roztoku dianu při 360 nm, dále pak stanoveném obsahu volného fenolu a p-izopropylfenolu. Aditiva pro termooxidační stabilizaci dianu se neprojevují nežádoucími efekty na technologii výroby a vlastnosti epoxidových pryskyřic.Of the alkali metal salts, sodium and potassium salts are preferably used, but lithium salts can also be used in special cases. Boric acid itself has a certain stabilizing effect, but it causes a significant decomposition of dian, especially due to the strong acidity of its transition complexes. Alkali salts, triphenylphosphine, tinates and mixtures of these basic substances prove to be ineffective thermo-oxidative stabilizers of dian. It is noteworthy, however, that mixtures of boric acid with said basic substances in the indicated weight ratio have a marked thermo-oxidative stabilizing effect of dianium melts. It is a hitherto unknown synergism of the effect. The stabilizing effect of the mixture according to the invention is monitored by changing the optical transmittance of a 40% ethanolic solution of diane at 360 nm, followed by the determined content of free phenol and p-isopropylphenol. Additives for thermo-oxidative stabilization of dian do not have adverse effects on the production technology and properties of epoxy resins.
Příklad .Example.
Dian byl připraven vakuovou destilací technického dianu o teplotě tání 154 až 155 °C (korig.) a krystalizací z vroucího xylen-vodného systému. Podle analýzy kapal, chromatografii měl tento dian složení:Dian was prepared by vacuum distillation of technical dian, m.p. 154-155 ° C (corrected), and crystallization from a boiling xylene-aqueous system. According to the analysis of liquids, chromatography, this dian had the composition:
p,p' - izomér 99,95 % .p, p '- isomer 99.95%.
o,p - izomér 0,04 % monofenoly 0,01 % (celkem) teplota tání 156,8 až 157,1 °C (korrig,), optická propustnost při 360 nm 87,7 %.o, p - isomer 0.04% monophenols 0.01% (total) melting point 156.8-157.1 ° C (corrected), optical transmittance at 360 nm 87.7%.
Postup zkoušky termooxidační stabilizace: do kuželové zábrusové baňky objemu 250 ml bylo předloženo 100 g dianu a zvolené množství aditiva. Dian s aditivem byl pod. vzdušnou atmosférou roztaven při 160 °C, promísen a vložen do horkovzdušného sterilizátoru a temperován na teplotu 160± °c, promísen a vložen do κThermo-oxidative stabilization test procedure: 100 g of dian and the selected amount of additive were introduced into a 250 ml conical ground glass flask. Dian with the additive was under. melted at 160 ° C with an air atmosphere, mixed and placed in a hot air sterilizer and tempered to a temperature of 160 ± ° C, mixed and placed in κ
CS 272 518 Bl 2 horkovzdušného sterilizátoru a temperován na teplotu 160Í 0,5 °C, po dobu 24 hodin. Po temperaci měl vzorek v jednotlivých provedeních tyto vlastnosti.CS 272 518 B1 2 hot air sterilizer and tempered to a temperature of 160 ° C 0.5 ° C, for 24 hours. After tempering, the sample had the following properties in the individual embodiments.
PŘEDMĚT VYNÁLEZUOBJECT OF THE INVENTION
Claims (1)