CS360588A1 - Preparation of sodium carbonate for catching admixtures of gaseous compounds,e.g. sulphur oxide - Google Patents

Preparation of sodium carbonate for catching admixtures of gaseous compounds,e.g. sulphur oxide

Info

Publication number
CS360588A1
CS360588A1 CS883605A CS360588A CS360588A1 CS 360588 A1 CS360588 A1 CS 360588A1 CS 883605 A CS883605 A CS 883605A CS 360588 A CS360588 A CS 360588A CS 360588 A1 CS360588 A1 CS 360588A1
Authority
CS
Czechoslovakia
Prior art keywords
upto
na2co3
dried
admixtures
catching
Prior art date
Application number
CS883605A
Other languages
Czech (cs)
Other versions
CS270337B1 (en
Inventor
Antonin Akademik Vlcek
Lubomir Doc Ing Csc Neuzil
Vaclav Ing Csc Bejcek
Karel Ing Csc Mocek
Jiri Ing Wald
Original Assignee
Antonin Akademik Vlcek
Neuzil Lubomir
Vaclav Ing Csc Bejcek
Mocek Karel
Wald Jiri
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Antonin Akademik Vlcek, Neuzil Lubomir, Vaclav Ing Csc Bejcek, Mocek Karel, Wald Jiri filed Critical Antonin Akademik Vlcek
Priority to CS883605A priority Critical patent/CS270337B1/en
Priority to DE1989610881 priority patent/DE68910881T2/en
Priority to AT89109475T priority patent/ATE97638T1/en
Priority to EP19890109475 priority patent/EP0343673B1/en
Publication of CS360588A1 publication Critical patent/CS360588A1/en
Publication of CS270337B1 publication Critical patent/CS270337B1/en

Abstract

Na2CO3.XH2O where x is 7.5-10.5 or its mixt. with aq. Na2CO3 soln. is (i) thermally decomposed or subjected to microwave radiation at 32-35.3 deg . C or dried at upto 32 deg. C to lower the value of x to below 7.5. (ii) hydrate obtd. from (i) is then dried at upto 35.3 deg. C to lower the value of x to less than 4 and (iii) further dried at upto 450 deg. C to produce soda (Na2CO3) with an H2O content (x) of equal to or below 1.05 Starting material in (i) is obtd. conventionally from NaHCO3, sodium sesquicarbonate, Wegscheiders salt etc. - Soda prod. (I) is used to remove SO2 and nitrogen oxides from gas mixts. and is highly porous and reactive. (I) has a desulphurising efficiency of above 95%. (I) can also be used as an additive forsolid detergents and is easily transported with low dust content. Energy and time demands are lower than in prior art prepn.(0/0)
CS883605A 1988-05-27 1988-05-27 Method of sodium carbonate preparation for gaseous mixtures' admixtures trapping especially of sulphur dioxide CS270337B1 (en)

Priority Applications (4)

Application Number Priority Date Filing Date Title
CS883605A CS270337B1 (en) 1988-05-27 1988-05-27 Method of sodium carbonate preparation for gaseous mixtures' admixtures trapping especially of sulphur dioxide
DE1989610881 DE68910881T2 (en) 1988-05-27 1989-05-26 Process for the production of extra light sodium carbonate.
AT89109475T ATE97638T1 (en) 1988-05-27 1989-05-26 PROCESS FOR PRODUCTION OF EXTRA-LIGHT SODIUM CARBONATE.
EP19890109475 EP0343673B1 (en) 1988-05-27 1989-05-26 Method of production of extra light soda

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CS883605A CS270337B1 (en) 1988-05-27 1988-05-27 Method of sodium carbonate preparation for gaseous mixtures' admixtures trapping especially of sulphur dioxide

Publications (2)

Publication Number Publication Date
CS360588A1 true CS360588A1 (en) 1989-11-14
CS270337B1 CS270337B1 (en) 1990-06-13

Family

ID=5376596

Family Applications (1)

Application Number Title Priority Date Filing Date
CS883605A CS270337B1 (en) 1988-05-27 1988-05-27 Method of sodium carbonate preparation for gaseous mixtures' admixtures trapping especially of sulphur dioxide

Country Status (1)

Country Link
CS (1) CS270337B1 (en)

Also Published As

Publication number Publication date
CS270337B1 (en) 1990-06-13

Similar Documents

Publication Publication Date Title
ES480399A1 (en) Process for the removal of sulphur oxides from high-chloride flue gases.
JPS5510461A (en) Treating method for bayer circulating solution
TW326404B (en) An exhaust desulfurization method
TW377305B (en) Method for removing sulfur dioxide and nitrogen oxides from combustion gases a method for removing air-polluted substance from combustion gases
GB1078596A (en) Process for the treatment of sulfur oxide-containing gases
CS360588A1 (en) Preparation of sodium carbonate for catching admixtures of gaseous compounds,e.g. sulphur oxide
JPS5522319A (en) High temperature waste gas cleaning
JPS5719078A (en) Disposal of fly ash
JPS5227068A (en) Exhaust gas desulfurization process
JPS56160312A (en) Manufacture of granular activated carbon
JPS57111237A (en) Production of alumina sol
GB2169887B (en) A process for removing gaseous sulphur compounds, such as sulphur dioxide, from the flue gases of a furnace
JPS551843A (en) Hydrogen sulfide removing agent
JPS565318A (en) Preparing hard type dense ash
JPS56113328A (en) Improvement in desulfurization process for exhaust gas
ES8603348A1 (en) PROCEDURE FOR THE PROCESSING OF THE IMPURE SODIUM OXALATE, WHICH IS FORMED DURING THE DIGESTION OF THE BAUXITE
JPS52130473A (en) Decomposition of nitrogen oxides
JPS54101762A (en) Removing method for nitrogen oxides contained in exhaust gas
JPS53118202A (en) Method of minimizing formation of nitrogen oxides in sintering system
JPH0359309A (en) In-furnace desulfurization method
JPS53128592A (en) Process for removing hydrogen sulfide
JPS55114333A (en) Method for decreasing nitrogen oxide in waste gas
JPS54142176A (en) Waste gas treatment
JPS5295578A (en) Wet process desulfurization of exhaust gas by slag
JPS5562809A (en) Purifying method of sodium aluminate solution

Legal Events

Date Code Title Description
IF00 In force as of 2000-06-30 in czech republic
MM4A Patent lapsed due to non-payment of fee

Effective date: 20010527