CU34670A - METHOD FOR THE TREATMENT OF FERRUGINOUS NICKEL AND COBALT LATERAL MINERALS - Google Patents

METHOD FOR THE TREATMENT OF FERRUGINOUS NICKEL AND COBALT LATERAL MINERALS

Info

Publication number
CU34670A
CU34670A CU34670A CU34670A CU34670A CU 34670 A CU34670 A CU 34670A CU 34670 A CU34670 A CU 34670A CU 34670 A CU34670 A CU 34670A CU 34670 A CU34670 A CU 34670A
Authority
CU
Cuba
Prior art keywords
solution
nickel
tails
washing
ferruginous
Prior art date
Application number
CU34670A
Other languages
Spanish (es)
Other versions
CU20877L (en
Inventor
Toirac Ildefonso Lopez
Javier Otero
Catasus Juan Mendez
Anzorandia Severino Sifontes
Ravil A Gafarov
Salomon Izrailevich Sobol
Original Assignee
Mini Ind Basica
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mini Ind Basica filed Critical Mini Ind Basica
Priority to CU34670A priority Critical patent/CU34670A/en
Publication of CU20877L publication Critical patent/CU20877L/en
Publication of CU34670A publication Critical patent/CU34670A/en

Abstract

La invención se refiere a la Rama de la hidrometalúrgia de los metales no ferrosos, en particular al tratamiento del mineral laterítico ferruginoso de Ni y Co con la utilización de los procesos de autoclave de la lixiviación de los procesos de autoclave de la lixiviación ácida de Ni y Co, separación de la solución y la cola, precipitación de sulfuro de Ni y Co de la solución. El método consiste en el lavado de las colas con la solución que contiene el reductor - hierro bivalente a Ph de 1,5 - 3,0 y la temperatura menor de 100 grado C, lo que permite hacer pasar por segunda vez a la solución Ni y Co, cooprecipitados con alunita que forma en el proceso de la lixiviación del mineral. Utilizando para el lavado de las colas las soluciones residuales después de la precipitación de sulfuros, - Fe2+, H2+ y el ácido sulfúrico, y también los sulfatos de una serie de metales aluminio, magnesio, cromo etc, se aumenta la concentración total de sulfato en la solución niquelífera, lo que aumenta la extracción en forma de sulfuros de Ni y Co en el curso de su realización. Además, el método permite eliminar la contaminación del medio ambiental, suspendiendo el consumo del agua potable para el lavado de las colas. La invención puede utilizarse en la industria cobalto-niquelíferaThe invention relates to the branch of hydrometallurgy of non-ferrous metals, in particular to the treatment of Ni and Co ferruginous lateritic ore with the use of autoclave processes of leaching of autoclave processes of Ni acid leaching. and Co, separation of the solution and the tail, precipitation of Ni and Co sulfide from the solution. The method consists of washing the tails with the solution containing the reducer - bivalent iron at Ph of 1.5 - 3.0 and the temperature less than 100 degree C, which allows to pass the Ni solution a second time and Co, co-precipitated with alunite that forms in the mineral leaching process. By using the residual solutions after precipitation of sulfides, - Fe2 +, H2 + and sulfuric acid, and also the sulfates of a series of metals, aluminum, magnesium, chromium, etc., for washing the tails, the total concentration of sulfate in the nickel-containing solution, which increases the extraction in the form of Ni and Co sulfides in the course of its realization. In addition, the method allows the contamination of the environment to be eliminated, suspending the consumption of drinking water for washing the tails. The invention can be used in the cobalt-nickel industry

CU34670A 1977-02-15 1977-02-15 METHOD FOR THE TREATMENT OF FERRUGINOUS NICKEL AND COBALT LATERAL MINERALS CU34670A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CU34670A CU34670A (en) 1977-02-15 1977-02-15 METHOD FOR THE TREATMENT OF FERRUGINOUS NICKEL AND COBALT LATERAL MINERALS

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CU34670A CU34670A (en) 1977-02-15 1977-02-15 METHOD FOR THE TREATMENT OF FERRUGINOUS NICKEL AND COBALT LATERAL MINERALS

Publications (2)

Publication Number Publication Date
CU20877L CU20877L (en) 1980-07-08
CU34670A true CU34670A (en) 1982-08-24

Family

ID=41087311

Family Applications (1)

Application Number Title Priority Date Filing Date
CU34670A CU34670A (en) 1977-02-15 1977-02-15 METHOD FOR THE TREATMENT OF FERRUGINOUS NICKEL AND COBALT LATERAL MINERALS

Country Status (1)

Country Link
CU (1) CU34670A (en)

Also Published As

Publication number Publication date
CU20877L (en) 1980-07-08

Similar Documents

Publication Publication Date Title
DOP2000000087A (en) METHOD TO REMOVE THE MINERAL OF LATERITA DEL FERRONIQUEL
FI128350B (en) Processing process to recover and separate substances from solution
CA2597440A1 (en) Process for enhanced acid leaching of laterite ores
RU95122127A (en) METHOD FOR ISOLATING ZINC AND IRON FROM ZINC AND IRON-CONTAINING SULPHIDE MATERIAL
BRPI0513652A (en) process for leaching laterite ores containing limonite and saprolite
GB1283588A (en) Process for the recovery of metals and sulphur form metal sulphides
AU2009225947A1 (en) A process for atmospheric leaching of laterite ores using hypersaline leach solution
CU34670A (en) METHOD FOR THE TREATMENT OF FERRUGINOUS NICKEL AND COBALT LATERAL MINERALS
US2588265A (en) Isolation of nickel sulfide
BRPI1100327A2 (en) Nickel and cobalt recovery method
GB1396470A (en) Process for separating oxidic ores containing nickel and or copper and or cobalt
FI56701C (en) SUR EXTRAHERINGSPROCESS FOR BEHANDLING AV NICKEL-KOPPAR-METALLSTEN
Korkmaz Comparative study of high pressure and atmospheric acid leaching for the extraction of nickel and cobalt from refractory nickel laterite ores
SU389158A1 (en) METHOD OF PROCESSING ANODE PLATINUM-CONTAINING SLUDES
SU704231A1 (en) Method of processing ferrous nickel-cobalt laterite ores
GB1314213A (en) Process for the concentration of non-ferrous minerals
BR0313497A (en) Process for Recovering Valuable Metals from Laterite Ore and Concentrates Contaminated with Iron
Yazici et al. Recovery of cobalt from sulphate solutions by precipitation via persulphate oxidation
Saha et al. Recovery of Cobalt From Lateritic Nickel--Cobalt Ores With Special Reference to Sukinda Ultramafic Fields
ES8100815A1 (en) Recuperation of cyanides from rinsing solutions of cyanidric processes for electrodeposition of metals.
US2111951A (en) Hydro-metallurgy
GB543887A (en) Process for the purification of manganous sulphate solutions
WO2017197417A1 (en) Method of recovering a target metal
AU2006212723B2 (en) Process for enhanced acid leaching of laterite ores
RU2006115017A (en) METHOD OF NICKEL, COBALT AND COPPER DEPOSITION IS SELECTIVE FROM ZINC FROM SULPHATE SOLUTIONS IN THE FORM OF SULPHIDES