ES2001615A6 - Metodo para colada continua de metales - Google Patents
Metodo para colada continua de metalesInfo
- Publication number
- ES2001615A6 ES2001615A6 ES8601468A ES8601468A ES2001615A6 ES 2001615 A6 ES2001615 A6 ES 2001615A6 ES 8601468 A ES8601468 A ES 8601468A ES 8601468 A ES8601468 A ES 8601468A ES 2001615 A6 ES2001615 A6 ES 2001615A6
- Authority
- ES
- Spain
- Prior art keywords
- temperature
- corresponds
- bar
- solid phase
- metal casting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
METODO PARA COLADA CONTINUA DE METALES. EN EL METODO DE COLADA EL ESPESOR DE LA BARRA SE REDUCE DE MANERA CONTINUA A LA VELOCIDAD DE 0,5 MM/MIN HASTA MENOR DE 2,2 MM/MIN ENTRE EL MOMENTO EN QUE EL CENTRO DE LA BARRA TIENE UNA TEMPERATURA QUE CORRESPONDE A UNA PROPORCION DE FASE SOLIDA ENTRE 0,1 Y 0,3 Y EL MOMENTO EN QUE DICHA TEMPERATURA HA DESCENDIDO A NIVEL QUE CORRESPONDE A LA PROPORCION DE FASE SOLIDA DE LIMITE DE FLUIDIZACION, SIN REDUCCION SUSTANCIAL EN EL ESPESOR ENTRE EL MOMENTO EN QUE EL CENTRO DE LA BARRA TIENE LA TEMPERATURA QUE CORRESPONDE A LA PROPORCION DE FASE SOLIDA DE LIMITE DE FLUIDIZACION Y EL MOMENTO EN EL QUE DICHA TEMPERATURA HA DESCENDIDO AL LIMITE DE SOLIDO.
Applications Claiming Priority (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60171314A JPS6233048A (ja) | 1985-08-03 | 1985-08-03 | 連続鋳造法 |
| JP17131585 | 1985-08-03 | ||
| JP29877485A JPS62158555A (ja) | 1985-12-30 | 1985-12-30 | 連続鋳造方法 |
| JP29877385A JPS62158554A (ja) | 1985-12-30 | 1985-12-30 | 連続鋳造方法 |
| JP13627686A JPS62275556A (ja) | 1985-08-03 | 1986-06-13 | 連続鋳造方法 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| ES2001615A6 true ES2001615A6 (es) | 1988-06-01 |
Family
ID=27527452
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| ES8601468A Expired ES2001615A6 (es) | 1985-08-03 | 1986-08-01 | Metodo para colada continua de metales |
Country Status (6)
| Country | Link |
|---|---|
| US (1) | US4687047A (es) |
| EP (1) | EP0211422B2 (es) |
| AU (1) | AU571787B2 (es) |
| CA (1) | CA1279462C (es) |
| DE (1) | DE3676753D1 (es) |
| ES (1) | ES2001615A6 (es) |
Families Citing this family (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6363561A (ja) * | 1986-09-04 | 1988-03-19 | Nippon Steel Corp | 連続鋳造法 |
| CA1298061C (en) * | 1986-09-04 | 1992-03-31 | Takuo Imai | Method and apparatus for continuous compression forging of continuously cast steel |
| DE3800865A1 (de) * | 1987-04-01 | 1988-10-20 | Bosch Gmbh Robert | Stossdaempfer i |
| JP3257224B2 (ja) * | 1994-01-14 | 2002-02-18 | 大同特殊鋼株式会社 | 連続鋳造方法 |
| JP2814958B2 (ja) * | 1994-09-09 | 1998-10-27 | 株式会社神戸製鋼所 | 連続鋳造方法 |
| JP2809186B2 (ja) * | 1996-02-19 | 1998-10-08 | 株式会社神戸製鋼所 | 連続鋳造方法 |
| EP2209574B1 (en) * | 2007-11-19 | 2019-03-06 | Posco | Continuous cast slab and method for manufacturing the same |
| CN107000045B (zh) * | 2014-12-24 | 2019-04-26 | 杰富意钢铁株式会社 | 钢的连续铸造方法 |
| CN109142144B (zh) * | 2018-07-20 | 2020-12-22 | 中冶连铸技术工程有限责任公司 | 铸坯均质化程度分析方法 |
| WO2023228796A1 (ja) * | 2022-05-26 | 2023-11-30 | Jfeスチール株式会社 | 鋼の連続鋳造方法及び連続鋳造機 |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CH530831A (de) * | 1970-09-04 | 1972-11-30 | Concast Ag | Verfahren und Vorrichtung zum Kühlen mittels Sprühdüsen und Führen eines Stranges in der Sekundärkühlzone einer Stranggiessanlage |
| JPS5916862B2 (ja) * | 1973-03-26 | 1984-04-18 | 日本鋼管株式会社 | 連続鋳造法 |
| JPS5160633A (en) * | 1974-11-25 | 1976-05-26 | Nippon Kokan Kk | Haganeno renzokuchuzoho |
| US4519439A (en) * | 1977-07-26 | 1985-05-28 | Jernjontoret | Method of preventing formation of segregations during continuous casting |
| GB1596395A (en) * | 1977-12-14 | 1981-08-26 | Jernkontoret Forskningsavdelni | Method of continuous casting of steels or metal alloys with segregation tendancy and apparatus for carrying out the method |
| JPS5970444A (ja) * | 1982-10-12 | 1984-04-20 | Nippon Kokan Kk <Nkk> | セミマクロ偏析のない連続鋳造鋳片の製造方法 |
| JP4651133B2 (ja) * | 1997-04-18 | 2011-03-16 | 三井化学株式会社 | 架橋ポリアスパラギン酸系樹脂の製造方法 |
-
1986
- 1986-08-01 CA CA000515167A patent/CA1279462C/en not_active Expired - Lifetime
- 1986-08-01 DE DE8686110690T patent/DE3676753D1/de not_active Expired - Lifetime
- 1986-08-01 ES ES8601468A patent/ES2001615A6/es not_active Expired
- 1986-08-01 AU AU60791/86A patent/AU571787B2/en not_active Expired
- 1986-08-01 EP EP86110690A patent/EP0211422B2/en not_active Expired - Lifetime
- 1986-08-01 US US06/892,075 patent/US4687047A/en not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| CA1279462C (en) | 1991-01-29 |
| EP0211422A1 (en) | 1987-02-25 |
| US4687047A (en) | 1987-08-18 |
| AU6079186A (en) | 1987-02-05 |
| EP0211422B2 (en) | 1995-11-08 |
| EP0211422B1 (en) | 1991-01-09 |
| AU571787B2 (en) | 1988-04-21 |
| DE3676753D1 (de) | 1991-02-14 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| BE826071A (fr) | Procede et dispositif pour modifier le refroidissement secondaire dans la coulee continue d'acier | |
| NZ184495A (en) | Casting steel ingots and slabs thin cast sheets pressure welded together | |
| GB1386061A (en) | Metal casting using mould fluxes | |
| GB2166432B (en) | Refractory wear part for use in the pouring of molten metal | |
| ZA818652B (en) | Method of cooling castings in the continuous casting of steel | |
| IT8722148A0 (it) | Procedimento di colata di metallo fuso, in particolare di leghe di alluminio e leghe di magnesio e dispositivo per la sua esecuzione. | |
| FI800869A7 (fi) | Menetelmä seegrauksen vähentämiseksi teräksen jatkuvan valun yhteydessä. | |
| MX161908A (es) | Mejoras en recipiente de manejo de metal fundido | |
| GB1528928A (en) | Methods of and chill moulds for casting metal ingots billets and the like | |
| JPS5213418A (en) | Cast steel for welding | |
| IT1150605B (it) | Procedimento per la colata d'acciaio,in particolare di lingotti d'acciaio | |
| SU458594A1 (ru) | Способ внепечного рафинировани жидкой стали | |
| ES8703315A1 (es) | Procedimiento para fabricar piezas moldeadas de hierro fundido con grafico esferoidal o vermicular. | |
| SU670629A1 (ru) | Модификатор чугуна | |
| FR2352063A1 (fr) | Procede d'introduction d'une addition solide dans un bain de metal liquide | |
| JPS55154520A (en) | Particulate slagging composition for extended optimum continuous casting of steel | |
| JPS5431013A (en) | Method of adding calcium metal or calcium alloy into molten steel within continuous casting tandish | |
| ES267396Y (es) | Placa de revestimiento de mazarotas refractarias. | |
| IT1088903B (it) | Procedimento di introduzione di una addizione solida in un bagno di metallo liquido | |
| Nikulin | Inoculation of R 6 M 5 High-Speed Steel With Rare Earth Compounds | |
| PL273826A2 (en) | Method of heat treating the castings made of cr-mo cast steel and intended to operate at high temperatures | |
| JPS5288223A (en) | Method of casting steel ingot with few surface defects and granular stratification molten flux for embodying the method | |
| Shimada | REFRACTORY MATERIALS FOR CASTING HIGH MANGANESE STEEL,(DEVELOPMENT OF TECHNOLOGY OF HIGH MANGANESE STEEL MAKING--II) | |
| GB1550493A (en) | Method of casting molten metal to form ingots or castings | |
| FR2290975A1 (fr) | Procede et dispositif pour fixer une piece rapportee a la plaque de base d'une lingotiere |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FD1A | Patent lapsed |
Effective date: 20060802 |