Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mond Nickel Co Ltd
Original Assignee
Mond Nickel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mond Nickel Co LtdfiledCriticalMond Nickel Co Ltd
Priority claimed from GB2133059Aexternal-prioritypatent/GB913293A/en
Publication of ES259105A1publicationCriticalpatent/ES259105A1/es
Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces
(AREA)
Abstract
Un procedimiento de producir hierro calado, que contiene grafito esferoridal, por medio de magnesio, caracterizado porque incluye la operación de mantener hierro fundido que contiene magnesio en un recipiente en el cual la superficie del baño está cubierta sustancialmente por completo por una placa de grafito o de un material refractario en contacto con el metal.
ES0259105A1960-06-221960-06-21Un procedimiento de producir hierro colado