ES431626A1 - Un procedimiento para colar continuamente lingotes de aceroen especial llantones. - Google Patents
Un procedimiento para colar continuamente lingotes de aceroen especial llantones.Info
- Publication number
- ES431626A1 ES431626A1 ES431626A ES431626A ES431626A1 ES 431626 A1 ES431626 A1 ES 431626A1 ES 431626 A ES431626 A ES 431626A ES 431626 A ES431626 A ES 431626A ES 431626 A1 ES431626 A1 ES 431626A1
- Authority
- ES
- Spain
- Prior art keywords
- ingot
- slag
- cooling zone
- secondary cooling
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B22—CASTING; POWDER METALLURGY
- B22D—CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
- B22D11/00—Continuous casting of metals, i.e. casting in indefinite lengths
- B22D11/10—Supplying or treating molten metal
- B22D11/11—Treating the molten metal
- B22D11/111—Treating the molten metal by using protecting powders
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B22—CASTING; POWDER METALLURGY
- B22D—CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
- B22D11/00—Continuous casting of metals, i.e. casting in indefinite lengths
- B22D11/12—Accessories for subsequent treating or working cast stock in situ
- B22D11/124—Accessories for subsequent treating or working cast stock in situ for cooling
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Continuous Casting (AREA)
- Treatment Of Steel In Its Molten State (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| AT938873A AT330389B (de) | 1973-11-08 | 1973-11-08 | Verfahren zum kontinuierlichen giessen von stahlstrangen, insbesondere brammen, in einer stranggiessanlage |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| ES431626A1 true ES431626A1 (es) | 1976-11-01 |
Family
ID=3613723
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| ES431626A Expired ES431626A1 (es) | 1973-11-08 | 1974-11-04 | Un procedimiento para colar continuamente lingotes de aceroen especial llantones. |
Country Status (13)
| Country | Link |
|---|---|
| JP (1) | JPS5075525A (fr) |
| AT (1) | AT330389B (fr) |
| BE (1) | BE821823A (fr) |
| BR (1) | BR7409351A (fr) |
| CA (1) | CA1046731A (fr) |
| CH (1) | CH574782A5 (fr) |
| DE (1) | DE2449812A1 (fr) |
| ES (1) | ES431626A1 (fr) |
| FR (1) | FR2250595B1 (fr) |
| GB (1) | GB1479745A (fr) |
| IT (1) | IT1021764B (fr) |
| SE (1) | SE396707B (fr) |
| SU (1) | SU534175A3 (fr) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5680367A (en) | 1979-12-06 | 1981-07-01 | Nippon Steel Corp | Restraining method of cracking in b-containing steel continuous casting ingot |
| AT399463B (de) * | 1987-03-03 | 1995-05-26 | Inteco Int Techn Beratung | Verfahren zum elektroschlacke-stranggiessen von stählen und legierungen |
| RU2196187C1 (ru) * | 2001-04-24 | 2003-01-10 | Дорофеев Генрих Алексеевич | Способ получения сплава со свободным и связанным углеродом |
| CN108393456B (zh) * | 2017-02-05 | 2019-10-29 | 鞍钢股份有限公司 | 一种q345b厚板铸坯组织控制方法 |
| CN113857448B (zh) * | 2021-11-29 | 2022-02-22 | 东北大学 | 一种低碱度免涂层热成形钢连铸用保护渣 |
-
1973
- 1973-11-08 AT AT938873A patent/AT330389B/de not_active IP Right Cessation
-
1974
- 1974-10-03 SE SE7412443A patent/SE396707B/xx unknown
- 1974-10-09 JP JP49115697A patent/JPS5075525A/ja active Pending
- 1974-10-11 IT IT53475/74A patent/IT1021764B/it active
- 1974-10-15 CH CH1383174A patent/CH574782A5/xx not_active IP Right Cessation
- 1974-10-17 CA CA211,591A patent/CA1046731A/fr not_active Expired
- 1974-10-19 DE DE19742449812 patent/DE2449812A1/de not_active Withdrawn
- 1974-10-29 FR FR7436102A patent/FR2250595B1/fr not_active Expired
- 1974-11-04 BE BE150185A patent/BE821823A/fr unknown
- 1974-11-04 ES ES431626A patent/ES431626A1/es not_active Expired
- 1974-11-06 SU SU2078666A patent/SU534175A3/ru active
- 1974-11-07 BR BR9351/74A patent/BR7409351A/pt unknown
- 1974-11-07 GB GB48308/74A patent/GB1479745A/en not_active Expired
Also Published As
| Publication number | Publication date |
|---|---|
| DE2449812A1 (de) | 1975-05-15 |
| SE396707B (sv) | 1977-10-03 |
| BR7409351A (pt) | 1976-05-18 |
| FR2250595B1 (fr) | 1980-08-08 |
| GB1479745A (en) | 1977-07-13 |
| SU534175A3 (ru) | 1976-10-30 |
| SE7412443L (fr) | 1975-05-09 |
| CH574782A5 (fr) | 1976-04-30 |
| FR2250595A1 (fr) | 1975-06-06 |
| IT1021764B (it) | 1978-02-20 |
| ATA938873A (de) | 1975-09-15 |
| CA1046731A (fr) | 1979-01-23 |
| AT330389B (de) | 1976-06-25 |
| BE821823A (fr) | 1975-03-03 |
| JPS5075525A (fr) | 1975-06-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ES418646A1 (es) | Procedimiento y dispositivo para el gobierno del enfria- miento de una barra colada que sale de una lingotera abier- ta. | |
| ES431626A1 (es) | Un procedimiento para colar continuamente lingotes de aceroen especial llantones. | |
| ES427157A1 (es) | Procedimiento y dispositivo para el enfriamiento de la ba- rra colada que se forma en una lingotera oscilante durante la colada continua de acero. | |
| GB1087026A (en) | Improvements in or relating to the continous casting of metals and metal alloys | |
| GB1091790A (en) | Continuous casting mold having ribs | |
| GB1201451A (en) | A method of and apparatus for making granulate | |
| GB2003064A (en) | Horizontal continuous casting plant for copper and copper alloys | |
| ES471183A1 (es) | Procedimiento y aparato para la colada continua de un mate- rial fundido | |
| GB512953A (en) | Process and apparatus for casting bodies of indefinite length | |
| JPS5242412A (en) | Process for refining molten metal infine particles | |
| ES368343A1 (es) | Procedimiento para la fabricacion de ramales segun el procedimiento de colada continua. | |
| ES433372A1 (es) | Un procedimiento para colar continuamente lingotes de ace- ro. | |
| GB1205008A (en) | Improvements in or relating to electro-slag remelting | |
| JPS5268018A (en) | Roller conveying steel plate | |
| JPS5788952A (en) | Sealing method for hot-water feed nozzle in endless track type horizontal continuous casting machine | |
| SU725786A1 (ru) | Установка дл разливки металла | |
| JPS5325210A (en) | Steel refining method | |
| SU452606A1 (ru) | Способ получени стандартных образцов ферросплавов | |
| FR2112118A1 (en) | Slag - for lubricating continuous casting of steel | |
| JPS55147465A (en) | Rotary ring type continuous casting machine | |
| SU407636A1 (fr) | ||
| JPS5377813A (en) | Converter slag separating method | |
| SU676380A2 (ru) | Способ получени чугунных отливок в кокиле | |
| ES421235A1 (es) | Metodo para la fabricacion de piezas fundidas con dos meta-les diferentes, como, por ejemplo, los cilindros para lami- nadoras de uso siderurgico y extrasiderurgico. | |
| JPS5620117A (en) | Manufacture of billet by continuous casting |