ES482429A1 - Procedimiento para la fabricacion de un acero inoxidable de elevada resistencia. - Google Patents

Procedimiento para la fabricacion de un acero inoxidable de elevada resistencia.

Info

Publication number
ES482429A1
ES482429A1 ES482429A ES482429A ES482429A1 ES 482429 A1 ES482429 A1 ES 482429A1 ES 482429 A ES482429 A ES 482429A ES 482429 A ES482429 A ES 482429A ES 482429 A1 ES482429 A1 ES 482429A1
Authority
ES
Spain
Prior art keywords
weight
translation
manufacture
machine
stainless steel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
ES482429A
Other languages
English (en)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CIFLO HENRIK
Original Assignee
CIFLO HENRIK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CIFLO HENRIK filed Critical CIFLO HENRIK
Priority to ES482429A priority Critical patent/ES482429A1/es
Publication of ES482429A1 publication Critical patent/ES482429A1/es
Expired legal-status Critical Current

Abstract

Procedimiento para la fabricación de un acero inoxidable de elevada resistencia, apropiado para el pulido y resistente a los ácidos, caracterizado por comprender la aleación, además del hierro y de los elementos residuales habituales, de un máximo de 2,00% (en peso) de C, un máximo de 1,00% (en peso) de Si, un máximo de 5,00% (en peso) de Mn; un mínimo de 5,00% (en peso) de Cr, un máximo de 12% (en peso) de Ni, un máximo de 4,00% (en peso) de Cu, un máximo de 3,00% (en peso) de Mo, un mínimo de 0,005% (en peso) de N, 0,02 a 0,25% (en peso) de Zr, y/o de Be, 0,001 a 0,20% (en peso) de Al, 0,04 a 1,50% (en peso) de Nb y/o de V, un mínimo de 0,001% (en peso) de Ca y un mínimo de 0,01% (en peso) de B y/o de Ce.
ES482429A 1979-06-28 1979-06-28 Procedimiento para la fabricacion de un acero inoxidable de elevada resistencia. Expired ES482429A1 (es)

Priority Applications (1)

Application Number Priority Date Filing Date Title
ES482429A ES482429A1 (es) 1979-06-28 1979-06-28 Procedimiento para la fabricacion de un acero inoxidable de elevada resistencia.

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
ES482429A ES482429A1 (es) 1979-06-28 1979-06-28 Procedimiento para la fabricacion de un acero inoxidable de elevada resistencia.

Publications (1)

Publication Number Publication Date
ES482429A1 true ES482429A1 (es) 1980-02-16

Family

ID=8478634

Family Applications (1)

Application Number Title Priority Date Filing Date
ES482429A Expired ES482429A1 (es) 1979-06-28 1979-06-28 Procedimiento para la fabricacion de un acero inoxidable de elevada resistencia.

Country Status (1)

Country Link
ES (1) ES482429A1 (es)

Similar Documents

Publication Publication Date Title
GB2000188A (en) Cobalt-chronium-nitrogen alloys for surgical implants
JPS53108022A (en) Iron-nickel-chromium-molybdenum alloy of high ductility
JPS5681661A (en) Heat resistant cast alloy
GB1063374A (en) Chromium-nickel-aluminium steel and method
JPS5723050A (en) Heat resistant steel with excellent high temp. strength
ES8206655A1 (es) Procedimiento de convertir acero austenitico.
DE2967326D1 (en) High-strength stainless steel, well suited for polishing and resistant to acids
ES482429A1 (es) Procedimiento para la fabricacion de un acero inoxidable de elevada resistencia.
ES543202A0 (es) Procedimiento de obtencion de acero inoxidable
ES426814A2 (es) Un procedimiento para producir una aleacion ferrea sinteri- zada.
GB923844A (en) Austenitic steel generator rings and steel therefor
JPS5582739A (en) Alloy for hearth member with improved thermal impact resistance and high temperature compressive strength
GB1343735A (en) Refractory iron-base alloy and articles or parts made therefrom
JPS54118323A (en) Heat crack resistant steel for use as metal mold
JPS5270924A (en) Heat-resisting austenite casting alloy
GB872052A (en) Stainless steel resistant to nitric acid corrosion
JPS5413414A (en) Medium cr low ni stainless cast steel of high corrosion resistance and high strength
GB833240A (en) Improvements relating to ferritic alloy steels
JPS5635756A (en) Precipitation hardening type hot working tool steel
JPS57134536A (en) Heat resistant alloy
JPS5413412A (en) Highly corrosion resistant austenitic stainless steel of superior crevice corrosion resistant characteristics
JPS5378914A (en) Low alloy steel for large-sized forged product
GB883359A (en) Improvements in or relating to the cladding of metals
JPS5528307A (en) Heat resistant alloy with superior weld crack resistance
JPS52155127A (en) Heat treatment of ni-cr-w alloy cold worked material

Legal Events

Date Code Title Description
MM4A Patent lapsed

Effective date: 19960401