ES8401875A1 - Un metodo para soldar completamente por fusion dos posiciones de metal base. - Google Patents
Un metodo para soldar completamente por fusion dos posiciones de metal base.Info
- Publication number
- ES8401875A1 ES8401875A1 ES519102A ES519102A ES8401875A1 ES 8401875 A1 ES8401875 A1 ES 8401875A1 ES 519102 A ES519102 A ES 519102A ES 519102 A ES519102 A ES 519102A ES 8401875 A1 ES8401875 A1 ES 8401875A1
- Authority
- ES
- Spain
- Prior art keywords
- relating
- fusion welding
- welding methods
- metal
- parent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
METODO PARA SOLDAR CONJUNTAMENTE POR FUSION DOS PORCIONES DE METAL DE BASE.CARACTERIZADO PORQUE SE APLICA A CADA PORCION DE METAL DE BASE, UN RECUBRIMIENTO FORMADO POR UN METAL QUE TIENE UN POTENCIAL ELECTROMECANICO INFERIOR AL DE DICHO METAL DE BASE, PORQUE EL RECUBRIMIENTO SE DISPONE DE MODO QUE RECUBRA POR LO MENOS LA ZONA DE SUPERFICIE DE CONTACTO MUTUO INTERFACIAL Y LAS ZONAS DE SOLDADURA PREVISTAS, PORQUE LA ZONA DE CONTACTO INTERFACIAL Y LAS ZONAS DE SOLDADURA PREVISTAS, SE AMOLAN PARA HACER SUS SUPERFICIES RUGOSAS ANTES DE LA APLICACION DEL RECUBRIMIENTO, Y PORQUE EL RECUBRIMIENTOSE APLICA MEDIANTE UN PROCESO DE ROCIADO POR ARCO O MEDIANTE UN PROCESO DE ROCIADO POR LLAM
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| GB8201573 | 1982-01-20 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| ES519102A0 ES519102A0 (es) | 1984-01-01 |
| ES8401875A1 true ES8401875A1 (es) | 1984-01-01 |
Family
ID=10527741
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| ES519102A Expired ES8401875A1 (es) | 1982-01-20 | 1983-01-19 | Un metodo para soldar completamente por fusion dos posiciones de metal base. |
Country Status (10)
| Country | Link |
|---|---|
| US (1) | US4564743A (es) |
| EP (1) | EP0098852B1 (es) |
| JP (1) | JPS59500090A (es) |
| AU (1) | AU556191B2 (es) |
| CA (1) | CA1205873A (es) |
| DE (1) | DE3365923D1 (es) |
| ES (1) | ES8401875A1 (es) |
| GB (1) | GB2115331B (es) |
| IT (1) | IT1197544B (es) |
| WO (1) | WO1983002415A1 (es) |
Families Citing this family (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB8623160D0 (en) * | 1986-09-26 | 1986-10-29 | Alcan Int Ltd | Welding aluminium alloys |
| CA1326808C (en) * | 1986-10-24 | 1994-02-08 | Koichi Yasuda | Blowhole_pit preventing agent and arc-welding method using the same |
| GB8704251D0 (en) * | 1987-02-24 | 1987-04-01 | Alcan Int Ltd | Welding aluminium alloys |
| US5965278A (en) * | 1993-04-02 | 1999-10-12 | Ppg Industries Ohio, Inc. | Method of making cathode targets comprising silicon |
| US6026577A (en) * | 1993-10-15 | 2000-02-22 | Warner-Lambert Company | Disposable razor with removable razor head |
| KR0141337B1 (ko) * | 1994-09-05 | 1998-07-15 | 김수광 | 소우블레이드용 세그먼트 |
| US6528763B1 (en) * | 2001-04-30 | 2003-03-04 | Lsp Technologies, Inc. | Laser search peening for exfoliation corrosion detection |
| US7121806B2 (en) * | 2003-12-19 | 2006-10-17 | Dresser-Rand Company | Welding method and an assembly formed thereby |
| DE102009040083A1 (de) * | 2009-09-04 | 2011-03-10 | Stadtmüller, Uwe | Verfahren und Vorrichtung zum Verschweißen von im Fügebereich eine Punkt- oder kurze Linienberührung aufweisenden Teilen sowie Fügeeinrichtung |
| WO2017142435A1 (ru) * | 2016-02-19 | 2017-08-24 | Общество С Ограниченной Ответственностью "Ромет" | Способ сварки изделия из коррозионностоиких многослойных металлических материалов |
| CN105953954B (zh) * | 2016-04-29 | 2018-09-04 | 河海大学 | 一种组合钢桥面板界面母材焊趾疲劳热点应力测试方法 |
| CN119566539B (zh) * | 2024-11-26 | 2025-09-23 | 华中科技大学 | 一种压铸AlSi10MnMg与6005A-T6铝型材的无穿孔密封焊接方法 |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB470323A (en) * | 1936-02-04 | 1937-08-12 | Kodak Ltd | Method of welding and weld rods therefor |
| GB568918A (en) * | 1943-05-28 | 1945-04-26 | British Aluminium Co Ltd | Improvements in and relating to soldering methods |
| FR1520979A (fr) * | 1966-04-27 | 1968-04-12 | Procédé de soudure d'alliages trempants | |
| US4157923A (en) * | 1976-09-13 | 1979-06-12 | Ford Motor Company | Surface alloying and heat treating processes |
| JPS547603A (en) * | 1977-06-20 | 1979-01-20 | Mueszeripari Muevek Lab | Nonnpulsation distribution pump |
| JPS5586684A (en) * | 1978-12-22 | 1980-06-30 | Hitachi Ltd | Bonding method of metal |
| US4269867A (en) * | 1979-09-04 | 1981-05-26 | Texasgulf Inc. | Metallizing of a corrodible metal with a protective metal |
-
1983
- 1983-01-07 DE DE8383900352T patent/DE3365923D1/de not_active Expired
- 1983-01-07 AU AU11052/83A patent/AU556191B2/en not_active Ceased
- 1983-01-07 JP JP83500400A patent/JPS59500090A/ja active Pending
- 1983-01-07 WO PCT/GB1983/000001 patent/WO1983002415A1/en not_active Ceased
- 1983-01-07 EP EP83900352A patent/EP0098852B1/en not_active Expired
- 1983-01-07 US US06/531,895 patent/US4564743A/en not_active Expired - Fee Related
- 1983-01-17 GB GB08301217A patent/GB2115331B/en not_active Expired
- 1983-01-19 IT IT47577/83A patent/IT1197544B/it active
- 1983-01-19 ES ES519102A patent/ES8401875A1/es not_active Expired
- 1983-01-19 CA CA000419786A patent/CA1205873A/en not_active Expired
Also Published As
| Publication number | Publication date |
|---|---|
| EP0098852B1 (en) | 1986-09-10 |
| IT1197544B (it) | 1988-12-06 |
| AU1105283A (en) | 1983-07-28 |
| GB2115331A (en) | 1983-09-07 |
| IT8347577A0 (it) | 1983-01-19 |
| US4564743A (en) | 1986-01-14 |
| WO1983002415A1 (en) | 1983-07-21 |
| EP0098852A1 (en) | 1984-01-25 |
| ES519102A0 (es) | 1984-01-01 |
| AU556191B2 (en) | 1986-10-23 |
| DE3365923D1 (en) | 1986-10-16 |
| CA1205873A (en) | 1986-06-10 |
| JPS59500090A (ja) | 1984-01-19 |
| GB8301217D0 (en) | 1983-02-16 |
| GB2115331B (en) | 1986-01-22 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ES8401875A1 (es) | Un metodo para soldar completamente por fusion dos posiciones de metal base. | |
| ES8600100A1 (es) | Procedimiento e instalacion de soldadura de puntos, por rayo laser | |
| ES543055A0 (es) | Metodo para mejorar la resistencia la ductilidad y la resistencia a la corrosion de una soldadura de aleacion que contiene nitrogeno. | |
| ZA823118B (en) | A method for joining aluminum to titanium by welding,and a thereby produced welded joint | |
| JPS57199574A (en) | Arc welder mounting welding stud to metallic member in water | |
| ATE18729T1 (de) | Verfahren zur herstellung einer schweissverbindung sowie zwischenteil zu dessen durchfuehrung. | |
| Mandzhgaladze et al. | Properties of Welded Joints of the Alloy 06 KhN 28 MDT and the Steel 03 Kh 18 N 20 M 3 D 3 S 3 B | |
| SE8300997L (sv) | Forfarande och flussmedel for elektroslaggsvetsning | |
| Chernyshova | Increasing the Corrosion Resistance of Welded Joints in 09 GN 1 B Low Alloy Steel by Adding Deoxidizing Agents Into Weld Metal | |
| JPS53140245A (en) | Improving method for fatiuge strength of fillet welded joint | |
| JPS5399049A (en) | Welding method of pipe and flange | |
| JPS57134289A (en) | Metallic parts for laser beam welding | |
| JPS57181775A (en) | Welding method for titanium alloy | |
| Nomura et al. | Further improvement of narrow gap welding techniques | |
| Sobotka et al. | Evaluation of the Long-Term Creep Strength Properties of Welded Joints in Pipes of the 17 341 Steel(16% Cr--12% Ni--2% Mo). III.--Microstructural Aspects of Creep of the Weld Metal of Electrode E-B 422 | |
| Sixt | Coating of Ferrous Materials by Weld and Hard Facing Materials of Non-Ferrous Metals to Austrian Standard M 7825 | |
| Ranke | The Selection of the Shielding Gases for Gas-Shielded Metal-Arc Welding | |
| Godai et al. | Newly Developed Vertical-Down Low Hydrogen Welding Electrodes for Field Joints of Pipelines | |
| Volchenko et al. | The Corrosion Resistance of Welded Joints in the Clad Layer of a Bimetal | |
| Orlova | The Corrosion Resistance of 15 Kh 25 T Steel Welds in Concentrated NaOH Solutions | |
| Janota | Positioning Adaptability of Resistance Spot Welding Robots | |
| Paton et al. | Laminated Steel for Welded Structures | |
| Mantel | Where Do the Greatest Difficulties for the Welder Lie in Passing from Steel to Copper Based Materials? | |
| Xie | Weld Quality Disturbance in GMA Welding | |
| Davis | Introduction to Welding Fluxes for Mild and Low Alloy Steels[Pamphlet] |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FD1A | Patent lapsed |
Effective date: 20000601 |