FR2411242A1 - Poudre a base de molybdene riche en oxygene pour pulverisation par plasma, son procede de fabrication et le revetement obtenu a l'aide d'une telle poudre - Google Patents
Poudre a base de molybdene riche en oxygene pour pulverisation par plasma, son procede de fabrication et le revetement obtenu a l'aide d'une telle poudreInfo
- Publication number
- FR2411242A1 FR2411242A1 FR7834551A FR7834551A FR2411242A1 FR 2411242 A1 FR2411242 A1 FR 2411242A1 FR 7834551 A FR7834551 A FR 7834551A FR 7834551 A FR7834551 A FR 7834551A FR 2411242 A1 FR2411242 A1 FR 2411242A1
- Authority
- FR
- France
- Prior art keywords
- oxygen
- molybdene
- powder
- plasma
- rich
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
LA DURETE ET, PAR SUITE, LA RESISTANCE A L'USURE DES REVETEMENTS APPLIQUES PAR PULVERISATION A LA FLAMME DE MOLYBDENE, PEUVENT ETRE AMELIORES SENSIBLEMENT EN INCORPORANT AU MOINS 0,5 EN POIDS D'OXYGENE DANS LA POUDRE A PULVERISER PAR PLASMA A BASE DE MOLYBDENE, SOIT PAR DISSOLUTION D'OXYGENE OU D'OXYDE, SOIT DANS UNE SECONDE PHASE PAR ADJONCTION D'OXYGENE OU D'UN OXYDE, SOIT PAR OXYDATION SUPERFICIELLE, SOIT PAR COMBINAISON DE CES DIFFERENTES SOLUTIONS, AVANT LA PULVERISATION DU PLASMA. LES REVETEMENTS OBTENUS A L'AIDE D'UN TEL MOYEN PRESENTENT UNE DURETE ACCRUE PAR RAPPORT AUX REVETEMENTS OBTENUS PAR PULVERISATION DE PLASMA DE MOLYBDENE "PUR" CONTENANT GENERALEMENT ENTRE 1 ET 2 D'OXYGENE. APPLICATION: REVETEMENT POUR SEGMENTS DE PISTON DANS LES MOTEURS A COMBUSTION INTERNE.
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US05/858,777 US4146388A (en) | 1977-12-08 | 1977-12-08 | Molybdenum plasma spray powder, process for producing said powder, and coatings made therefrom |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| FR2411242A1 true FR2411242A1 (fr) | 1979-07-06 |
Family
ID=25329147
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| FR7834551A Withdrawn FR2411242A1 (fr) | 1977-12-08 | 1978-12-08 | Poudre a base de molybdene riche en oxygene pour pulverisation par plasma, son procede de fabrication et le revetement obtenu a l'aide d'une telle poudre |
Country Status (8)
| Country | Link |
|---|---|
| US (1) | US4146388A (fr) |
| JP (1) | JPS5490027A (fr) |
| AT (1) | AT357390B (fr) |
| CA (1) | CA1159282A (fr) |
| DE (1) | DE2852534A1 (fr) |
| FR (1) | FR2411242A1 (fr) |
| GB (1) | GB2010336B (fr) |
| NL (1) | NL7811935A (fr) |
Families Citing this family (23)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6227533A (ja) * | 1985-07-26 | 1987-02-05 | Japan Synthetic Rubber Co Ltd | 内部酸化型合金およびその成形物の製造方法 |
| DE3785775T2 (de) * | 1986-02-12 | 1993-08-12 | Gte Prod Corp | Verfahren zur ueberwachung des sauerstoffgehaltes in einem agglomerierten molybdaenpulver. |
| US4624700A (en) * | 1986-02-20 | 1986-11-25 | Gte Products Corporation | Method for controlling the oxygen content in agglomerated molybdenum powders |
| US4684400A (en) * | 1986-02-20 | 1987-08-04 | Gte Products Corporation | Method for controlling the oxygen content in agglomerated molybdenum powders |
| US5000785A (en) * | 1986-02-12 | 1991-03-19 | Gte Products Corporation | Method for controlling the oxygen content in agglomerated molybdenum powders |
| US4854980A (en) * | 1987-12-17 | 1989-08-08 | Gte Laboratories Incorporated | Refractory transition metal glassy alloys containing molybdenum |
| DE3837782A1 (de) * | 1988-11-08 | 1990-05-10 | Starck Hermann C Fa | Sauerstoffhaltiges molybdaenmetallpulver sowie verfahren zu dessen herstellung |
| DE3842263C1 (fr) * | 1988-12-15 | 1990-06-13 | Linde Ag, 6200 Wiesbaden, De | |
| US5173108A (en) * | 1989-03-21 | 1992-12-22 | Gte Products Corporation | Method for controlling the oxygen content in agglomerated molybdenum powders |
| US5330557A (en) * | 1990-02-12 | 1994-07-19 | Amax Inc. | Fluid bed reduction to produce flowable molybdenum metal |
| US5290507A (en) * | 1991-02-19 | 1994-03-01 | Runkle Joseph C | Method for making tool steel with high thermal fatigue resistance |
| DE4317350C2 (de) * | 1993-05-25 | 1995-04-20 | Ptg Plasma Oberflaechentech | Verfahren zum Beschichten von Tassenstösseln |
| DK16494A (da) * | 1994-02-08 | 1995-08-09 | Man B & W Diesel Gmbh | Fremgangsmåde til fremstilling af en cylinderforing samt en sådan foring |
| US5766693A (en) * | 1995-10-06 | 1998-06-16 | Ford Global Technologies, Inc. | Method of depositing composite metal coatings containing low friction oxides |
| US7276102B2 (en) * | 2004-10-21 | 2007-10-02 | Climax Engineered Materials, Llc | Molybdenum metal powder and production thereof |
| US7524353B2 (en) * | 2004-10-21 | 2009-04-28 | Climax Engineered Materials, Llc | Densified molybdenum metal powder and method for producing same |
| US7470307B2 (en) * | 2005-03-29 | 2008-12-30 | Climax Engineered Materials, Llc | Metal powders and methods for producing the same |
| GB2468054B (en) * | 2006-03-24 | 2011-11-09 | Climax Engineered Mat Llc | Metal powders and methods for producing the same |
| CN100506438C (zh) * | 2006-11-29 | 2009-07-01 | 金堆城钼业股份有限公司 | 一种制取喷涂钼粉的方法 |
| US20090181179A1 (en) * | 2008-01-11 | 2009-07-16 | Climax Engineered Materials, Llc | Sodium/Molybdenum Composite Metal Powders, Products Thereof, and Methods for Producing Photovoltaic Cells |
| US8197885B2 (en) * | 2008-01-11 | 2012-06-12 | Climax Engineered Materials, Llc | Methods for producing sodium/molybdenum power compacts |
| US10287177B1 (en) * | 2018-05-08 | 2019-05-14 | Robert Ten | Method and apparatus for extracting high-purity molybdenum oxide powders and nanopowders from low-grade concentrates |
| US10612111B2 (en) | 2018-08-21 | 2020-04-07 | Robert Ten | Method and apparatus for extracting high-purity gold from ore |
Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB1102845A (en) * | 1965-10-23 | 1968-02-14 | American Metal Climax Inc | Improvements relating to coating compositions containing molybdenum |
| FR2221526A1 (fr) * | 1973-03-15 | 1974-10-11 | Goetzewerke | |
| FR2234382A1 (en) * | 1973-06-22 | 1975-01-17 | Metallisation Ste Nouvelle | Partially oxidised molybdenum coatings - deposited using plasma torch to give a surface of increased coefft of friction |
| US3960545A (en) * | 1975-03-24 | 1976-06-01 | Gte Sylvania Incorporated | Cermet plasma flame spray powder, method for producing same and articles produced therefrom |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3973948A (en) * | 1973-11-12 | 1976-08-10 | Gte Sylvania Incorporated | Free flowing powder and process for producing it |
| US3909241A (en) * | 1973-12-17 | 1975-09-30 | Gte Sylvania Inc | Process for producing free flowing powder and product |
| US4011073A (en) * | 1975-07-02 | 1977-03-08 | Gte Sylvania Incorporated | Flame spray powder of cobalt-molybdenum mixed metal agglomerates using a molybdenum salt binder and process for producing same |
-
1977
- 1977-12-08 US US05/858,777 patent/US4146388A/en not_active Expired - Lifetime
-
1978
- 1978-09-08 CA CA000310939A patent/CA1159282A/fr not_active Expired
- 1978-12-05 DE DE19782852534 patent/DE2852534A1/de not_active Withdrawn
- 1978-12-07 NL NL7811935A patent/NL7811935A/xx not_active Application Discontinuation
- 1978-12-07 GB GB7847639A patent/GB2010336B/en not_active Expired
- 1978-12-07 AT AT877478A patent/AT357390B/de not_active IP Right Cessation
- 1978-12-07 JP JP15059878A patent/JPS5490027A/ja active Pending
- 1978-12-08 FR FR7834551A patent/FR2411242A1/fr not_active Withdrawn
Patent Citations (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB1102845A (en) * | 1965-10-23 | 1968-02-14 | American Metal Climax Inc | Improvements relating to coating compositions containing molybdenum |
| FR2221526A1 (fr) * | 1973-03-15 | 1974-10-11 | Goetzewerke | |
| US3890137A (en) * | 1973-03-15 | 1975-06-17 | Goetzewerke | Welding powder for producing wear-resistant layers by build-up welding |
| FR2234382A1 (en) * | 1973-06-22 | 1975-01-17 | Metallisation Ste Nouvelle | Partially oxidised molybdenum coatings - deposited using plasma torch to give a surface of increased coefft of friction |
| US3960545A (en) * | 1975-03-24 | 1976-06-01 | Gte Sylvania Incorporated | Cermet plasma flame spray powder, method for producing same and articles produced therefrom |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5490027A (en) | 1979-07-17 |
| ATA877478A (de) | 1979-11-15 |
| GB2010336A (en) | 1979-06-27 |
| CA1159282A (fr) | 1983-12-27 |
| US4146388A (en) | 1979-03-27 |
| NL7811935A (nl) | 1979-06-12 |
| AT357390B (de) | 1980-07-10 |
| DE2852534A1 (de) | 1979-07-05 |
| GB2010336B (en) | 1983-01-06 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| FR2411242A1 (fr) | Poudre a base de molybdene riche en oxygene pour pulverisation par plasma, son procede de fabrication et le revetement obtenu a l'aide d'une telle poudre | |
| US4570946A (en) | Nitrided piston ring with outer layer on surface | |
| JPS55154565A (en) | Surface-covered sintered hard alloy member | |
| ATE192784T1 (de) | Verfahren zum herstellen einer gleitfläche auf einem metallischen werkstück | |
| GB1459495A (en) | Application of refractory coatings to sealing elements | |
| ZA847449B (en) | Improved molding tool and method | |
| FR2376021A1 (fr) | Pignon de chaine pour une bicyclette | |
| GB1300034A (en) | Improvements in or relating to piston rings | |
| FR2428677A1 (fr) | Melanges de poudres a pulverisation dans une flamme et procede de production de revetements a liaison adherente sur un substrat metallique a l'aide de ces melanges de poudres | |
| FR2442279A1 (fr) | Melanges de poudres a pulverisation dans une flamme, pour la production de revetements sur des substrats metalliques | |
| GB2155588A (en) | Corrosion resistant piston ring | |
| GB1389812A (en) | Oxide coated metal sliding members | |
| ITMI922948A1 (it) | Processo per rivestire la superficie interna di contenitori metallici con materiali poliolefinici | |
| JPS54126854A (en) | Piston ring | |
| ES8203104A1 (es) | Procedimiento para la fabricacion de un cuerpo de metal duro | |
| US3947269A (en) | Boron-hardened tungsten facing alloy | |
| JPS5920859B2 (ja) | ピストンリングの組合せ | |
| JPS565969A (en) | Sliding member | |
| JPS55164070A (en) | Sliding parts for internal combustion engine | |
| EP0331279A3 (fr) | Composés et leur utilisation | |
| JPS5696066A (en) | Treatment of sliding member to provide wear resistance | |
| JPS57134013A (en) | Spalling-resisting and wear-resisting roll | |
| JPS5744435A (en) | Can lid winding and fastening tool | |
| GB1509559A (en) | Method of protecting molten metal containers against corrosion | |
| JPS57157547A (en) | Manufacture of semiconductor device |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| CD | Change of name or company name | ||
| ST | Notification of lapse |