FR2415500A1 - Procede de coulee continue ou semi-continue d'un metal - Google Patents
Procede de coulee continue ou semi-continue d'un metalInfo
- Publication number
- FR2415500A1 FR2415500A1 FR7802575A FR7802575A FR2415500A1 FR 2415500 A1 FR2415500 A1 FR 2415500A1 FR 7802575 A FR7802575 A FR 7802575A FR 7802575 A FR7802575 A FR 7802575A FR 2415500 A1 FR2415500 A1 FR 2415500A1
- Authority
- FR
- France
- Prior art keywords
- ingot
- inductor
- fier
- continuous metal
- metal casting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
L'invention concerne la métallurgie Le procédé faisant l'objet de l'invention est caractérisé en ce que les ceintures de refroidissement 3, 6, 7, 8 sont mises successivement hors d'action, en commençant par la ceinture supérieure 3, au fur et à mesure que le pied du lingot 2 arrive au niveau de chacune des ceintures de re roidissement suivantes au cours de son déplacement de haut en bas, et que jusqu'à l'achèvement du processus de coulée du lingot on fait arriver le fluide de refroidissement par celle des ceintures de refroidissement qui permet à la frontière liquide-solide sur la surface latérale du lingot d'être maintenue sensiblement à mi-hauteur de l'inducteur 4. L'invention s'applique notamment à l'élaboration de lingots, notamment de 500 à 1 100 mm de diamètre, en alliages caractérisés par de faibles vitesses de solidification.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| FR7802575A FR2415500A1 (fr) | 1978-01-30 | 1978-01-30 | Procede de coulee continue ou semi-continue d'un metal |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| FR7802575A FR2415500A1 (fr) | 1978-01-30 | 1978-01-30 | Procede de coulee continue ou semi-continue d'un metal |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| FR2415500A1 true FR2415500A1 (fr) | 1979-08-24 |
| FR2415500B1 FR2415500B1 (fr) | 1980-07-25 |
Family
ID=9203984
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| FR7802575A Granted FR2415500A1 (fr) | 1978-01-30 | 1978-01-30 | Procede de coulee continue ou semi-continue d'un metal |
Country Status (1)
| Country | Link |
|---|---|
| FR (1) | FR2415500A1 (fr) |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR1509962A (fr) * | 1966-10-04 | 1968-01-19 | Metall Zd Im V I | Procédé de coulée continue et semi-continue de métaux et installation pour sa mise en oeuvre |
| FR2047894A1 (fr) * | 1969-06-24 | 1971-03-19 | Kuibyshevsky Metallurg | |
| FR2106545A1 (fr) * | 1970-09-16 | 1972-05-05 | Krasnog |
-
1978
- 1978-01-30 FR FR7802575A patent/FR2415500A1/fr active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR1509962A (fr) * | 1966-10-04 | 1968-01-19 | Metall Zd Im V I | Procédé de coulée continue et semi-continue de métaux et installation pour sa mise en oeuvre |
| FR2047894A1 (fr) * | 1969-06-24 | 1971-03-19 | Kuibyshevsky Metallurg | |
| FR2106545A1 (fr) * | 1970-09-16 | 1972-05-05 | Krasnog |
Also Published As
| Publication number | Publication date |
|---|---|
| FR2415500B1 (fr) | 1980-07-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE3273900D1 (en) | Process and apparatus having improved efficiency for producing a semi-solid slurry | |
| US4156451A (en) | Continuous or semi-continuous metal casting method | |
| DE3366204D1 (en) | Use of mould nozzles | |
| NL7714089A (en) | Continuous metal casting using inductor mould - with cooling arrangement allowing variation in ingot pulling velocity | |
| JPS54131533A (en) | Flow rate controller for molten metal | |
| JPS5732862A (en) | Secondary cooling method in continuous casting of ni steel | |
| GB1499038A (en) | Electromagnetic mould for continuous or semicontinuous casting | |
| JPS56154267A (en) | Method for suppressing vortex of molten steel in tundish in continuous casting | |
| SU1576226A1 (ru) | Способ непрерывного лить заготовок | |
| JPS57142761A (en) | Casting method for steel ingot | |
| JPS57127548A (en) | Production of hollow billet utilizing vibration | |
| JPS53118261A (en) | Die for use in hot extrusion of non-symmetrical shape steel | |
| JPS5373758A (en) | Method of controlling oil temperature for hydraulic elevator | |
| JPS5419135A (en) | Centralized controller for distribution line connected equipment | |
| JPS57161087A (en) | Base plate for tin electroplated steel plate | |
| JPS52142607A (en) | Automatic fluid discharge apparatus | |
| JPS56109149A (en) | Continuous casting method of less surface cracking | |
| UA5901A1 (uk) | Спосіб подавлення пилоутворення при наповненні ковша рідким металом | |
| JPS53114734A (en) | Controlling method for molten zing bath in molten zing plating method | |
| Takeuchi et al. | Twin-Drum Continuous Casting of Stainless Steel | |
| JPS5237208A (en) | Tempeature control system for molten metals in an electromagnetic pump | |
| JPS536204A (en) | Scum removing apparatus | |
| JPS52123993A (en) | Method and apparatus for cooling molten slag | |
| JPS56102358A (en) | Surface defect preventing method of ingot in continuous casting | |
| JPS5286588A (en) | Punching method and die for heavy metal boards with low melting points |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| ST | Notification of lapse |