JPH0160745U - - Google Patents
Info
- Publication number
- JPH0160745U JPH0160745U JP15468687U JP15468687U JPH0160745U JP H0160745 U JPH0160745 U JP H0160745U JP 15468687 U JP15468687 U JP 15468687U JP 15468687 U JP15468687 U JP 15468687U JP H0160745 U JPH0160745 U JP H0160745U
- Authority
- JP
- Japan
- Prior art keywords
- mold
- copper plate
- plate cylinder
- thin copper
- fitted
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図は本考案の連続鋳造用鋳型の実施例を示
す水平断面図、第2図は連続鋳造用鋳型の従来例
を示す水平断面図、第3図は連続鋳造用鋳型の他
の従来例を示す水平断面図である。
1…銅板、2…冷却溝、3…冷却箱。
Fig. 1 is a horizontal sectional view showing an embodiment of the continuous casting mold of the present invention, Fig. 2 is a horizontal sectional view showing a conventional example of the continuous casting mold, and Fig. 3 is another conventional example of the continuous casting mold. FIG. 1...Copper plate, 2...Cooling groove, 3...Cooling box.
Claims (1)
当該薄銅板円筒の背面にはめ込む冷却箱の内面に
周方向に亘つて等間隔に深さよりも幅の大きい偏
平形状の溝を上下方向に向けて配設し、上記薄銅
板円筒の背面に上記冷却箱をはめ込むことによつ
て偏平形状の冷却水通路を形成してなることを特
徴とする円形断面鋳片の連続鋳造用鋳型。 The inner wall of the mold in contact with the slab is formed from a thin copper plate cylinder,
On the inner surface of the cooling box that is fitted into the back of the thin copper plate cylinder, flat grooves having a width larger than the depth are vertically arranged at equal intervals along the circumference, and the cooling box is fitted into the back of the thin copper plate cylinder. A mold for continuous casting of circular cross-section slabs, characterized in that a flat cooling water passage is formed by fitting a box into the mold.