JPH0162351U - - Google Patents
Info
- Publication number
- JPH0162351U JPH0162351U JP15802487U JP15802487U JPH0162351U JP H0162351 U JPH0162351 U JP H0162351U JP 15802487 U JP15802487 U JP 15802487U JP 15802487 U JP15802487 U JP 15802487U JP H0162351 U JPH0162351 U JP H0162351U
- Authority
- JP
- Japan
- Prior art keywords
- roll
- steel strip
- sealing device
- annealing furnace
- side tension
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図は本考案の一実施例を示す模式図、第2
図は第1図の要部拡大を示す模式図、第3図は本
考案のシール装置を備えた連続焼鈍炉の概要図、
第4図は本考案のシール装置を使用して焼鈍した
鋼帯のすり疵発生状態を示す図、第5図は従来の
シール装置を示す図である。 21…シール装置、22,23…シールロール
、24…駆動装置、25…Crめつき層、26…
ダル仕上げ部分。
図は第1図の要部拡大を示す模式図、第3図は本
考案のシール装置を備えた連続焼鈍炉の概要図、
第4図は本考案のシール装置を使用して焼鈍した
鋼帯のすり疵発生状態を示す図、第5図は従来の
シール装置を示す図である。 21…シール装置、22,23…シールロール
、24…駆動装置、25…Crめつき層、26…
ダル仕上げ部分。
Claims (1)
- 【実用新案登録請求の範囲】 鋼帯を焼鈍する連続焼鈍炉の入り側及び出側に
設けられた駆動装置を備えたシール装置において
、表面をRz=5μm〜20mμのダル仕上げし
、その上にクロムめつき処理してなる一対のロー
ルを、その構成ロールが上下にオフセツトするよ
うに配設するとともに、そのロール表面間隔が前
記鋼帯の(板厚+0.1〜2.0mm)とし、鋼帯
とロールとの巻き掛け角を下記の条件を満足せし
めるようにしたことを特徴とする連続焼鈍炉のシ
ール装置。 T1≦T2eμθ・・・(1) ここにおいて、T1:ロールに働くトルクによ
るロール表面の接線方向の力、 T2:各ロールの各々の入り側張力と出側張
力のうちの小さい方の張力、 e:自然対数、 μ:摩擦係数、 θ:巻き掛け角。