JPH0360903B2 - - Google Patents
Info
- Publication number
- JPH0360903B2 JPH0360903B2 JP58141285A JP14128583A JPH0360903B2 JP H0360903 B2 JPH0360903 B2 JP H0360903B2 JP 58141285 A JP58141285 A JP 58141285A JP 14128583 A JP14128583 A JP 14128583A JP H0360903 B2 JPH0360903 B2 JP H0360903B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- less
- steels
- hardenability
- wear resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Earth Drilling (AREA)
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14128583A JPS6033339A (ja) | 1983-08-01 | 1983-08-01 | 耐摩耗合金鋼 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14128583A JPS6033339A (ja) | 1983-08-01 | 1983-08-01 | 耐摩耗合金鋼 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6033339A JPS6033339A (ja) | 1985-02-20 |
| JPH0360903B2 true JPH0360903B2 (pl) | 1991-09-18 |
Family
ID=15288332
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14128583A Granted JPS6033339A (ja) | 1983-08-01 | 1983-08-01 | 耐摩耗合金鋼 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6033339A (pl) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN103290329A (zh) * | 2012-02-22 | 2013-09-11 | 北京辰极国泰科技有限公司 | 一种高强韧合金铸钢挖掘机斗齿及其生产工艺 |
| JP6055577B1 (ja) * | 2015-04-21 | 2016-12-27 | 株式会社小松製作所 | チゼル用鋼およびチゼル |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS52138428A (en) * | 1976-05-17 | 1977-11-18 | Nippon Steel Corp | Production of rail having excellent wear resistance and damage resistance as rolled |
| JPS5380318A (en) * | 1976-12-27 | 1978-07-15 | Daido Steel Co Ltd | Hot tool steel with excellent high temperature strength |
| JPS5831066A (ja) * | 1981-07-28 | 1983-02-23 | Toyota Motor Corp | 冷間加工用金型 |
-
1983
- 1983-08-01 JP JP14128583A patent/JPS6033339A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6033339A (ja) | 1985-02-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2003027181A (ja) | 高靭性耐摩耗用鋼 | |
| JP2011074427A (ja) | 掘削用中空鋼ロッド | |
| SE528454C2 (sv) | Utskiljningshärdbart martensitiskt rostfritt stål innefattande titansulfid | |
| KR100415626B1 (ko) | 경화능이 우수한 고강도 내마모강 | |
| JPH0578781A (ja) | 高強度高靱性耐摩耗用鋼 | |
| JPH0360903B2 (pl) | ||
| JP3297500B2 (ja) | 被削性の優れた高強度棒鋼 | |
| JP2002235144A (ja) | 耐摩耗強靭鋼、カッティングエッジ、バケットツースおよびバケットリップ | |
| JPH031370B2 (pl) | ||
| JPH07116550B2 (ja) | 低合金高速度工具鋼およびその製造方法 | |
| JP2927694B2 (ja) | 耐折損性に優れた強靭耐摩耗鋼 | |
| JP4125423B2 (ja) | 土砂摩耗特性に優れた工具鋼の製造方法 | |
| JP7176877B2 (ja) | 耐衝撃性に優れた機械構造用合金鋼 | |
| JPS5925027B2 (ja) | 耐摩耐衝撃強靭工具綱 | |
| JP4159010B2 (ja) | 草刈刃用基板 | |
| JP3962143B2 (ja) | 草刈刃用基板 | |
| JPS6112851A (ja) | 高靭性耐摩耗鋼 | |
| JPH07179988A (ja) | 高温強度の優れた熱間工具鋼 | |
| KR100206355B1 (ko) | 고인성. 고내마모성 치즐소재 및 그 제조방법 | |
| JPS60215743A (ja) | 耐摩耗鋼 | |
| JP3227730B2 (ja) | 掘削用大型シャンク用鋼 | |
| JP2548067B2 (ja) | 高靭性低合金鋼 | |
| JPS60165356A (ja) | 耐摩耗合金鋼 | |
| JP2000328182A (ja) | 熱間加工性に優れる機械構造用快削鋼 | |
| JPS6123258B2 (pl) |