JPH0442009Y2 - - Google Patents

Info

Publication number
JPH0442009Y2
JPH0442009Y2 JP7188886U JP7188886U JPH0442009Y2 JP H0442009 Y2 JPH0442009 Y2 JP H0442009Y2 JP 7188886 U JP7188886 U JP 7188886U JP 7188886 U JP7188886 U JP 7188886U JP H0442009 Y2 JPH0442009 Y2 JP H0442009Y2
Authority
JP
Japan
Prior art keywords
workpiece
die
hole
punch
tip
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP7188886U
Other languages
Japanese (ja)
Other versions
JPS62183917U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP7188886U priority Critical patent/JPH0442009Y2/ja
Publication of JPS62183917U publication Critical patent/JPS62183917U/ja
Application granted granted Critical
Publication of JPH0442009Y2 publication Critical patent/JPH0442009Y2/ja
Expired legal-status Critical Current

Description

【考案の詳細な説明】 (産業上の利用分野) この考案は、絞り加工用金型に係り、さらに詳
細には、例えば波形状のワークにおける山部の稜
線部に孔加工を行なう前工程に使用する絞り加工
用金型に関する。
[Detailed description of the invention] (Industrial application field) This invention relates to a drawing mold, and more specifically, to a pre-process of drilling a hole in the ridgeline of a crest in a corrugated workpiece, for example. Regarding the drawing die to be used.

(従来の技術) 従来、第4図に示すごとき波形状のワークWの
山部の稜線部を押圧変形せしめて平面部WPを形
成し、この平面部に孔WHを加工するような場
合、先ず平面部WPを形成すべく絞り加工を行な
つた後に、孔WHの加工を行なつている。
(Prior art) Conventionally, when pressing and deforming the ridgeline of the peak of a corrugated workpiece W as shown in FIG. 4 to form a flat part WP, and drilling a hole WH in this flat part, first, After performing the drawing process to form the flat portion WP, the hole WH is processed.

(考案が解決しようとする問題点) しかし従来は、波形状のワークWの稜線部を単
に押圧変形せしめて平面部WPを形成するもので
あるから、種々の問題点があつた。すなわち、平
面部WPを形成するときには、ワークWの稜線部
の両側の傾斜面を押圧変形して平面部WPを形成
するものである。したがつて、上記平面部WPに
形成される前の両側の押圧変形される部分の総面
積よりも平面部WPの面積の方が小さいために、
平面部WPの周囲にしわを生じ易いものであつ
た。
(Problems to be Solved by the Invention) However, in the past, the ridgeline portion of the corrugated workpiece W was simply pressed and deformed to form the flat portion WP, which caused various problems. That is, when forming the flat portion WP, the inclined surfaces on both sides of the ridgeline portion of the workpiece W are pressed and deformed to form the flat portion WP. Therefore, since the area of the plane part WP is smaller than the total area of the parts to be pressed and deformed on both sides before being formed on the plane part WP,
Wrinkles were likely to form around the flat part WP.

(問題を解決するための手段) 上記のごとき問題に鑑みて、本考案は、波形状
に形成されたワークの山部または谷部を形成する
傾斜面に係合する傾斜した係合支持面を形成した
ダイの稜線部に水平な底面を有する矩形状の切欠
部を形成して設けると共に、この底面部に穴部を
形成して設け、前記ワークの稜線部分を前記ダイ
の切欠部の底面部へ押圧するパンチの先端部をテ
ーパ状に形成すると共に、このパンチの先端面
に、前記ワークの1部を前記穴部内へ押圧する半
球状部を形成してなるものである。
(Means for solving the problem) In view of the above problems, the present invention provides an inclined engagement support surface that engages with an inclined surface forming a peak or valley of a workpiece formed in a wave shape. A rectangular notch having a horizontal bottom surface is formed on the ridgeline portion of the formed die, and a hole portion is formed on the bottom surface portion, and the ridgeline portion of the workpiece is connected to the bottom surface of the notch portion of the die. The tip of the punch that presses the hole is formed into a tapered shape, and the tip of the punch has a hemispherical portion that presses a portion of the workpiece into the hole.

(実施例) 第1図〜第3図を参照するに、本実施例に係る
絞り加工用金型はパンチ1とダイ3よりなるもの
である。上記ダイ3には、波形上に形成された前
記ワークWの山部Mまたは谷部VAを形成する傾
斜面SPに係合する傾斜した係合支持面5A,5
Bが形成してあり、上記係合支持面5A,5Bが
合わさつた稜線部7には、水平な底面部9を有す
る矩形状の切欠部11が形成してある。そして上
記底面部9の中央部には穴部13が形成してあ
る。
(Example) Referring to FIGS. 1 to 3, the drawing die according to this example includes a punch 1 and a die 3. The die 3 has inclined engagement support surfaces 5A, 5 that engage with the inclined surfaces SP forming the peaks M or valleys VA of the workpiece W formed on the waveform.
A rectangular cutout 11 having a horizontal bottom surface 9 is formed in the ridgeline 7 where the engagement support surfaces 5A and 5B meet. A hole 13 is formed in the center of the bottom portion 9.

前記パンチ1は、前記ワークWの稜線部分WL
を前記ダイ3の切欠部11の底面部9へ押圧して
前記平面部WPを形成する作用をなすものであつ
て、このパンチ1の先端部にはテーパ状部15が
形成してある。そして、このパンチ1の先端面1
7には、前記ワークWの1部を前記穴部13内へ
押圧する半球状部19が突出形成してある。
The punch 1 punches the ridgeline portion WL of the workpiece W.
The punch 1 has a tapered portion 15 formed at its tip. Then, the tip surface 1 of this punch 1
7 has a hemispherical portion 19 protrudingly formed to press a portion of the workpiece W into the hole portion 13.

以上のごとき構成において、ワークWの山部M
をダイ3に支持せしめると、ワークWの傾斜面
SPがダイ3の傾斜した係合支持面5A,5Bに
面接触して支持される。上述のごとくワークWが
ダイ3に支持された状態にあるときに、ワークW
の稜線部WLに平面部WPを形成すべく、パンチ
1の先端部をダイ3の切欠部11に係合すると、
ワークWの稜線部WLが押し潰されて、平面部
WPが形成されることとなる。
In the above configuration, the peak M of the work W
When supported by the die 3, the inclined surface of the work W
The SP is supported in surface contact with the inclined engagement support surfaces 5A and 5B of the die 3. When the work W is supported by the die 3 as described above, the work W
When the tip of the punch 1 is engaged with the notch 11 of the die 3 in order to form the flat part WP on the ridgeline WL of
The ridgeline WL of the workpiece W is crushed and the flat part
WP will be formed.

上述のごとく、パンチ1の先端部とダイ3の切
欠部11との係合によつて平面部WPを形成する
とき、ワークWの1部分がパンチ1の先端部の半
球状部分19によつて押し潰されてダイ3の穴部
13内へ挿入される。この際、パンチ1のテーパ
状部15とダイ3の切欠部11の垂直な側面9S
との間にワークWを挾圧することがないので、ワ
ークWの肉厚を薄くするようなことがないもので
ある。
As described above, when the flat part WP is formed by the engagement between the tip of the punch 1 and the notch 11 of the die 3, a portion of the work W is caused by the hemispherical portion 19 of the tip of the punch 1. It is crushed and inserted into the hole 13 of the die 3. At this time, the vertical side surface 9S of the tapered part 15 of the punch 1 and the notch part 11 of the die 3
Since the work W is not clamped between the two, the thickness of the work W will not be reduced.

既に理解されるように、ワークWの稜線部分
WLを平面部WPに形成するとき、ワークWの1
部分がダイ3の穴部13内へ押圧されるものであ
るから、ワークWの平面部WPに形成される部分
の総面積が上記平面部WPより大きくしわを生じ
易い余分な部分が前記穴部13内へ引き込まれる
態様となつて、しわの発生が抑制されるものであ
る。
As already understood, the ridgeline part of the work W
When forming WL on the plane part WP, 1 of the workpiece W
Since the part is pressed into the hole 13 of the die 3, the total area of the part formed in the flat part WP of the workpiece W is larger than the flat part WP, and the extra part that tends to wrinkle is the hole part. 13, thereby suppressing the formation of wrinkles.

前述のごとく、ワークWに平面部WPを形成し
た後に、ダイ3の穴部13内へ押圧されたワーク
Wの1部分である半球状部分WBを次工程で打抜
くことにより、平面部WPに孔WHが形成される
ものである。
As mentioned above, after forming the flat part WP on the workpiece W, the hemispherical part WB, which is a part of the workpiece W pressed into the hole 13 of the die 3, is punched in the next step to form the flat part WP. This is where the hole WH is formed.

(考案の効果) 以上のごとき実施例の説明より理解されるよう
に、本考案によれば、波形状のワークWの山部ま
たは谷部に平面部WPを形成すると共に孔WHを
形成する場合、ワークWの余分な部分をダイ3に
形成した穴部13内へ押圧する構成であるから、
上記平面部WPを形成する際に生じ易いしわの発
生を抑制することができるものである。
(Effects of the invention) As can be understood from the explanation of the embodiments above, according to the invention, when a flat part WP is formed at the peak or trough of a corrugated workpiece W and a hole WH is formed. , since the configuration is such that the excess portion of the workpiece W is pressed into the hole 13 formed in the die 3,
This makes it possible to suppress the generation of wrinkles that are likely to occur when forming the flat portion WP.

【図面の簡単な説明】[Brief explanation of the drawing]

図面は本考案の1実施例を示すもので、第1図
は第3図における−線に沿つた断面図に相当
する断面説明図、第2図は第3図における−
線に沿つた断面図に相当する断面説明図であ
る。第3図は斜視説明図である。第4図は加工例
を示す説明図、第5図は第4図の−線に沿つ
た断面説明図である。 1……パンチ、3……ダイ、5A,5B……係
合支持面、7……稜線部、9……底面部、11…
…切欠部、13……穴部、15……テーパ状部、
17……先端面、19……半球上部。
The drawings show one embodiment of the present invention, and FIG. 1 is an explanatory sectional view corresponding to the sectional view taken along the line - in FIG. 3, and FIG.
FIG. 3 is an explanatory cross-sectional view corresponding to a cross-sectional view taken along a line. FIG. 3 is a perspective explanatory view. FIG. 4 is an explanatory view showing a processing example, and FIG. 5 is an explanatory cross-sectional view taken along the - line in FIG. 4. DESCRIPTION OF SYMBOLS 1... Punch, 3... Die, 5A, 5B... Engagement support surface, 7... Ridge line part, 9... Bottom part, 11...
...Notch, 13... Hole, 15... Tapered part,
17... Tip surface, 19... Upper hemisphere.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 波形状に形成されたワークWの山部Mまたは谷
部VAを形成する傾斜面SPに係合する傾斜した係
合支持面5A,5Bを形成したダイ3の稜線部7
に水平な底面9を有する矩形状の切欠部11を形
成して設けると共に、この底面部9に穴部13を
形成して設け、前記ワークWの稜線部分WLを前
記ダイ3の切欠部11の底面部9へ押圧するパン
チ1の先端部をテーパ状15に形成すると共に、
このパンチ1の先端面17に、前記ワークWの1
部を前記穴部13内へ押圧する半球状部19を形
成してなることを特徴とする絞り加工用金型。
The ridgeline portion 7 of the die 3 is formed with inclined engagement support surfaces 5A and 5B that engage with the inclined surface SP forming the peaks M or valleys VA of the workpiece W formed in a wave shape.
A rectangular notch 11 having a horizontal bottom surface 9 is formed and provided, and a hole 13 is formed and provided in the bottom surface 9, so that the ridgeline portion WL of the workpiece W is aligned with the notch 11 of the die 3. The tip of the punch 1 that presses against the bottom part 9 is formed into a tapered shape 15, and
1 of the workpiece W on the tip surface 17 of this punch 1.
A drawing mold characterized in that a hemispherical part 19 is formed to press a part into the hole part 13.
JP7188886U 1986-05-15 1986-05-15 Expired JPH0442009Y2 (en)