JPH05112709A5 - - Google Patents
Info
- Publication number
- JPH05112709A5 JPH05112709A5 JP3-252210A JP25221091A JPH05112709A5 JP H05112709 A5 JPH05112709 A5 JP H05112709A5 JP 25221091 A JP25221091 A JP 25221091A JP H05112709 A5 JPH05112709 A5 JP H05112709A5
- Authority
- JP
- Japan
- Prior art keywords
- crystalline polymer
- liquid crystalline
- melting point
- matrix resin
- document
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP03252210A JP3119508B2 (ja) | 1991-09-30 | 1991-09-30 | 液晶ポリマーを含有する再成形品の製造方法 |
| EP19920116771 EP0535650A3 (en) | 1991-09-30 | 1992-09-30 | Molding resin composition |
| KR1019920017834A KR960006785B1 (ko) | 1991-09-30 | 1992-09-30 | 성형용 수지조성물 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP03252210A JP3119508B2 (ja) | 1991-09-30 | 1991-09-30 | 液晶ポリマーを含有する再成形品の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH05112709A JPH05112709A (ja) | 1993-05-07 |
| JPH05112709A5 true JPH05112709A5 (cs) | 1999-08-24 |
| JP3119508B2 JP3119508B2 (ja) | 2000-12-25 |
Family
ID=17234037
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP03252210A Expired - Fee Related JP3119508B2 (ja) | 1991-09-30 | 1991-09-30 | 液晶ポリマーを含有する再成形品の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3119508B2 (cs) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3983301B2 (ja) * | 1996-11-29 | 2007-09-26 | ポリプラスチックス株式会社 | 射出成形体 |
| JP3664915B2 (ja) | 1999-07-16 | 2005-06-29 | ポリプラスチックス株式会社 | 熱可塑性樹脂組成物およびその成形体 |
| JP7373964B2 (ja) * | 2019-10-03 | 2023-11-06 | 三菱瓦斯化学株式会社 | フィルム、セキュリティカード、パスポート、および、フィルムの製造方法 |
-
1991
- 1991-09-30 JP JP03252210A patent/JP3119508B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR101820247B1 (ko) | 투명성 및 내열성이 우수한 폴리유산 스테레오 콤플렉스 수지 조성물 | |
| Williams | Applications for thermotropic liquid crystal polymer blends | |
| US4349504A (en) | Injection moulding process using polymer blends containing high molecular polyethylene of high density | |
| CN103732690A (zh) | 生物可降解树脂组合物以及由此生产的排水板芯材料及排水板 | |
| US4315887A (en) | Injection moulding of high molecular polyethylene using elevated mould temperature | |
| JPH0586257A5 (cs) | ||
| KR960006785B1 (ko) | 성형용 수지조성물 | |
| JPH0586273A5 (cs) | ||
| JPH0586258A5 (cs) | ||
| JPH0586234A5 (cs) | ||
| JPH0586282A5 (cs) | ||
| MY113231A (en) | Composite particulate material for resin reinforcement, production thereof, and reinforced resin composition incorporated therewith | |
| JP3119508B2 (ja) | 液晶ポリマーを含有する再成形品の製造方法 | |
| JPH0586268A5 (cs) | ||
| JP3217091B2 (ja) | 液晶ポリマーを含有する再成形品 | |
| JP3186858B2 (ja) | 液晶樹脂複合体の成形方法 | |
| JP3159741B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JPH0586288A5 (cs) | ||
| JPH0586286A5 (cs) | ||
| JP3224136B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3115655B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| EP0524655B1 (en) | Method for reforming a liquid crystal resin composite | |
| JP3124587B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3224137B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3162124B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 |