JPH0590192A - Method for manufacturing semiconductor device - Google Patents

Method for manufacturing semiconductor device

Info

Publication number
JPH0590192A
JPH0590192A JP24743391A JP24743391A JPH0590192A JP H0590192 A JPH0590192 A JP H0590192A JP 24743391 A JP24743391 A JP 24743391A JP 24743391 A JP24743391 A JP 24743391A JP H0590192 A JPH0590192 A JP H0590192A
Authority
JP
Japan
Prior art keywords
film
insulating film
contact hole
semiconductor device
diffusion layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP24743391A
Other languages
Japanese (ja)
Other versions
JPH0590192A5 (en
Inventor
Yusuke Harada
裕介 原田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Oki Electric Industry Co Ltd
Original Assignee
Oki Electric Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Oki Electric Industry Co Ltd filed Critical Oki Electric Industry Co Ltd
Priority to JP24743391A priority Critical patent/JPH0590192A/en
Publication of JPH0590192A publication Critical patent/JPH0590192A/en
Publication of JPH0590192A5 publication Critical patent/JPH0590192A5/ja
Pending legal-status Critical Current

Abstract

(57)【要約】 【目的】 本発明は、コンタクト孔埋込み配線でパーテ
ィクルの発生がなく、かつ、良好なコンタクト抵抗が得
られる半導体装置の製造方法を提供することを目的とす
る。 【構成】 Si基板上1上にSiO2 膜2及び拡散層3
を形成し、これらの上にBPSG膜4を形成し、拡散層
3上のコンタクト孔5を形成する。次に、Si基板1を
加熱し、さらに加熱によって形成されるSiO2 膜2表
面の活性領域を除去し、それからコンタクト孔5内にW
膜7を埋込むようにした。
(57) [Summary] [Object] It is an object of the present invention to provide a method of manufacturing a semiconductor device in which particles are not generated in a contact hole buried wiring and a good contact resistance is obtained. [Structure] SiO 2 film 2 and diffusion layer 3 on Si substrate 1
Are formed, a BPSG film 4 is formed thereon, and a contact hole 5 on the diffusion layer 3 is formed. Next, the Si substrate 1 is heated, and further, the active region on the surface of the SiO 2 film 2 formed by heating is removed, and then the W in the contact hole 5 is removed.
The membrane 7 was embedded.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【産業上の利用分野】本発明は、半導体装置の製造方
法、特にコンタクト孔埋込み配線の形成方法に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method of manufacturing a semiconductor device, and more particularly to a method of forming a contact hole buried wiring.

【0002】[0002]

【従来の技術】従来、コンタクト孔埋込み配線の形成方
法として、選択CVD(Chemical vapou
r deposition)を用いて行う方法がある。
図2を用いて、この形成方法について、説明をします。
2. Description of the Related Art Conventionally, a selective CVD (Chemical vapor) method has been used as a method of forming a contact hole buried wiring.
rdeposition).
This forming method will be explained using Fig. 2.

【0003】半導体基板11上に素子分離絶縁膜12と
拡散層13を順次形成する。
An element isolation insulating film 12 and a diffusion layer 13 are sequentially formed on a semiconductor substrate 11.

【0004】次に、この素子分離絶縁膜12と拡散層1
3上に絶縁膜14を形成する。そして、拡散層13上の
絶縁膜14を除去することによってコンタクト孔15を
形成する。
Next, the element isolation insulating film 12 and the diffusion layer 1 are formed.
An insulating film 14 is formed on the surface 3. Then, the contact hole 15 is formed by removing the insulating film 14 on the diffusion layer 13.

【0005】次に、選択CVD法により、W(タングス
テン)膜16をコンタクト孔15内に絶縁膜14の表面
と段差が生じない程度に形成する。
Next, a W (tungsten) film 16 is formed in the contact hole 15 by the selective CVD method to such an extent that no step is formed with the surface of the insulating film 14.

【0006】その後、Al−Si系合金膜17をスパッ
タリング法で絶縁膜14とW膜16上に形成する。
After that, an Al--Si alloy film 17 is formed on the insulating film 14 and the W film 16 by the sputtering method.

【0007】[0007]

【発明が解決しようとする課題】しかしながら、上述し
たコンタクト孔埋込み配線の形成方法では、以下のよう
な問題がある。
However, the above-mentioned method of forming the contact hole buried wiring has the following problems.

【0008】半導体装置の製造工程中で形成される絶縁
膜14には、形成時から含まれている塵や、洗浄中や大
気から含まれる水分が存在する。
The insulating film 14 formed during the manufacturing process of the semiconductor device contains dust contained during its formation and water contained during cleaning and from the atmosphere.

【0009】選択CVD法は、半導体基板11を加熱し
てWF6 とSiH4 ガスの熱反応によって、W膜を拡散
層13上にのみ選択的に形成するものである。
The selective CVD method is to selectively form a W film only on the diffusion layer 13 by heating the semiconductor substrate 11 and thermally reacting WF 6 and SiH 4 gas.

【0010】この選択CVD法での半導体基板11の加
熱時に、絶縁膜14中に含まれている水分が放出され
る。特に、絶縁膜表面付近では、絶縁膜の組成物につな
がっているOH基が加熱されることによって、H2 Oと
なり脱離することによって、絶縁膜表面は、ダングリン
グボンド等の活性な部分をもつために、絶縁膜14上で
もWF6 ,SiH4 がその活性領域で反応を起す。その
結果、W核がパーティクルとして多数発生し、その後の
配線工程で、層内ショートを引き起こすという問題があ
る。
When the semiconductor substrate 11 is heated by this selective CVD method, the moisture contained in the insulating film 14 is released. In particular, in the vicinity of the surface of the insulating film, the OH groups connected to the composition of the insulating film are heated to become H 2 O and are released, so that the surface of the insulating film has active parts such as dangling bonds. Therefore, WF 6 and SiH 4 also react on the insulating film 14 in its active region. As a result, a large number of W nuclei are generated as particles, which causes a short circuit within the layer in the subsequent wiring process.

【0011】本発明は、以上述べた選択CVD時、半導
体基板加熱によるH2 O脱離によって絶縁膜表面に活性
な領域が存在し、W核が形成されるという問題点を除去
できる半導体装置の製造方法を提供することを目的とす
る。
The present invention is directed to a semiconductor device which can eliminate the above-mentioned problem that W nuclei are formed due to the existence of an active region on the surface of the insulating film due to H 2 O desorption during heating of the semiconductor substrate during selective CVD. It is intended to provide a manufacturing method.

【0012】[0012]

【課題を解決するための手段】本発明の半導体装置の製
造方法は、半導体基板上に絶縁膜を形成し、この絶縁膜
の一部を半導体基板表面が露出するまで除去することに
よってコンタクト孔を形成し、次に半導体基板を加熱す
ることによって絶縁膜の表面に形成される活性化領域を
除去し、さらにコンタクト孔を金属で埋込んで形成する
ようにした。
According to a method of manufacturing a semiconductor device of the present invention, an insulating film is formed on a semiconductor substrate, and a part of the insulating film is removed until the surface of the semiconductor substrate is exposed to form a contact hole. After the formation, the semiconductor substrate is heated to remove the activation region formed on the surface of the insulating film, and the contact hole is filled with metal.

【0013】[0013]

【作用】本発明の半導体装置の製造方法は、半導体基板
を加熱するので、絶縁膜中に含まれている水分が放出
し、さらに、絶縁膜表面に形成される活性化領域は除去
することによりパーティクルは発生しない。
According to the method of manufacturing a semiconductor device of the present invention, since the semiconductor substrate is heated, the moisture contained in the insulating film is released, and further, the activated region formed on the surface of the insulating film is removed. No particles are generated.

【0014】[0014]

【実施例】本発明の半導体装置の製造方法につき、図1
(a)〜(c)を用いて説明する。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS A semiconductor device manufacturing method according to the present invention will be described with reference to FIG.
A description will be given using (a) to (c).

【0015】先ず、図1(a)に示すようにSi基板1
上に素子分離のための絶縁膜として例えばSiO2 膜2
と、拡散層3を形成する。
First, as shown in FIG. 1A, the Si substrate 1
As an insulating film for element isolation, for example, a SiO 2 film 2
Then, the diffusion layer 3 is formed.

【0016】次に、これらの上に層間絶縁膜として例え
ばBPSG膜4をCVD法にて10000Å形成する。
Next, a BPSG film 4 as an interlayer insulating film, for example, is formed on the above by a CVD method of 10000Å.

【0017】次に、N2 零囲気で950℃×15分行
う。これによって、BPSG膜4表面は平坦化される。
Next, it is performed at 950 ° C. for 15 minutes in a N 2 zero atmosphere. As a result, the surface of the BPSG film 4 is flattened.

【0018】次に、ホトリソエッチングにより、拡散層
3上にコンタクト孔5を形成する。このコンタクト孔5
のエッチングは、RIE(Reactive ion
etching)を用い、条件としては、C2 F6 流
量;15〔sccm〕,CHF3 流量;20〔scc
m〕,ガス圧力;80〔pa〕,RFパワー;400
〔W〕である。
Next, a contact hole 5 is formed on the diffusion layer 3 by photolithography etching. This contact hole 5
RIE (Reactive ion)
Etching), the conditions are C 2 F 6 flow rate; 15 [sccm], CHF 3 flow rate; 20 [scc
m], gas pressure; 80 [pa], RF power; 400
[W].

【0019】次に、図1(b)に示すように、真空中も
しくは不活性ガス中でSi基板1を300〜500℃に
加熱し、BPSG膜4から水分を脱離させる。その際、
BPSG膜4表面は活性領域6となる。
Next, as shown in FIG. 1B, the Si substrate 1 is heated to 300 to 500 ° C. in vacuum or in an inert gas to desorb water from the BPSG film 4. that time,
The surface of the BPSG film 4 becomes the active region 6.

【0020】次に、図1(c)に示すように、真空を破
らずにプラズマエッチングによって活性領域6を除去す
る。プラズマエッチングの条件としては、RFパワー;
20〜100〔W〕,ガス圧力;30〜500〔mto
r〕,エッチング時間;3〜30〔sec〕である。使
用するエッチングガスは、F系のガスとして例えばCF
4 ,NF4 ,SF6 を用い、Ar,He,もしくはH2
で希釈したものを用いる。このプラズマエッチングでコ
ンタクト孔5の底部の拡散層3上の自然酸化膜も除去さ
れることになる。
Next, as shown in FIG. 1C, the active region 6 is removed by plasma etching without breaking the vacuum. The conditions for plasma etching are RF power;
20 to 100 [W], gas pressure; 30 to 500 [mto
r], etching time; 3 to 30 [sec]. The etching gas used is, for example, CF as an F-based gas.
4 , NF 4 , SF 6 and Ar, He, or H 2
Use the one diluted with. This plasma etching also removes the natural oxide film on the diffusion layer 3 at the bottom of the contact hole 5.

【0021】次に、図1(d)に示すように、真空を破
らずに選択CVD法でW膜7をBPSG膜4と段差が生
じない程度に形成する。選択CVDの条件は、WF6 と
SiH4 の流量比SiH4 /WF6;0.2〜1.0,
エッチング温度;235〜280〔℃〕,ガス圧力;5
〜300〔mtorr〕である。
Next, as shown in FIG. 1D, the W film 7 is formed by the selective CVD method without breaking the vacuum, to the extent that no step is formed with the BPSG film 4. The conditions of the selective CVD are as follows: Flow rate ratio of WF 6 and SiH 4 SiH 4 / WF 6 ; 0.2 to 1.0,
Etching temperature: 235-280 [° C.], gas pressure: 5
˜300 [mtorr].

【0022】その後、配線層となるAl−Si系合金膜
8をスパッタリング法にて6000Å形成し、ホトリソ
エッチングにより配線パターンを得る。
Thereafter, an Al--Si alloy film 8 serving as a wiring layer is formed by sputtering to a thickness of 6000Å, and a wiring pattern is obtained by photolithographic etching.

【0023】Si基板加熱による水分の脱離からW膜の
形成工程までは、マルチチャンバを用いた真空系の装置
で行う方が効果的である。
It is more effective to perform the steps from the desorption of water by heating the Si substrate to the step of forming the W film in a vacuum system apparatus using a multi-chamber.

【0024】このマルチチャンバは例えば図3に示すよ
うなものであり、21は、ロードロックチャンバ,22
は、水分脱離用加熱チャンバ,23は、プラズマエッチ
ングチャンバ,24は、WCVDチャンバ,25は真空
搬送用チャンバである。
This multi-chamber is, for example, as shown in FIG. 3, in which 21 is a load lock chamber and 22 is a load lock chamber.
Is a heating chamber for desorption of water, 23 is a plasma etching chamber, 24 is a WCVD chamber, and 25 is a vacuum transfer chamber.

【0025】[0025]

【発明の効果】上述の説明から明らかなように本発明の
半導体装置の製造方法は、開孔部に金属を埋込む工程の
前に半導体基板を加熱することによって、絶縁膜から水
分を放出させ、その時に生成する絶縁膜表面の活性領域
を除去するようにしたので、良好なコンタクト抵抗を得
られかつ、活性領域の除去によりパーティクルの発生も
ない、優れた半導体装置を得ることができる。
As is apparent from the above description, in the method of manufacturing a semiconductor device of the present invention, moisture is released from the insulating film by heating the semiconductor substrate before the step of burying the metal in the opening. Since the active region on the surface of the insulating film generated at that time is removed, it is possible to obtain an excellent semiconductor device in which good contact resistance can be obtained and particles are not generated due to the removal of the active region.

【図面の簡単な説明】[Brief description of drawings]

【図1】本発明の半導体装置の製造工程を説明するため
の図。
FIG. 1 is a diagram for explaining a manufacturing process of a semiconductor device of the present invention.

【図2】従来の半導体装置の製造工程を説明するための
図。
FIG. 2 is a diagram for explaining a conventional manufacturing process of a semiconductor device.

【図3】マルチチャンバの主要部構成図。FIG. 3 is a configuration diagram of main parts of a multi-chamber.

【符号の説明】[Explanation of symbols]

1 Si基板 2 SiO2 膜 3 拡散層 4 BPSG膜 5 コンタクト孔 6 活性領域 7 W膜 8 Al−Si系合金膜1 Si substrate 2 SiO 2 film 3 diffusion layer 4 BPSG film 5 contact hole 6 active region 7 W film 8 Al-Si alloy film

Claims (1)

【特許請求の範囲】[Claims] 【請求項1】 半導体基板上に絶縁膜を形成する工程
と、 前記絶縁膜の一部を前記半導体基板表面が露出するまで
除去することによってコンタクト孔を形成する工程と、 前記半導体基板を加熱する工程と、 前記加熱によって前記絶縁膜の表面に形成される活性領
域を除去する工程と、 前記コンタクト孔を金属で埋込む工程とを含むことを特
徴とする半導体装置の製造方法。
1. A step of forming an insulating film on a semiconductor substrate, a step of forming a contact hole by removing a part of the insulating film until the surface of the semiconductor substrate is exposed, and heating the semiconductor substrate. A method of manufacturing a semiconductor device, comprising: a step, a step of removing an active region formed on the surface of the insulating film by the heating, and a step of filling the contact hole with a metal.
JP24743391A 1991-09-26 1991-09-26 Method for manufacturing semiconductor device Pending JPH0590192A (en)