JPH06200054A5 - - Google Patents
Info
- Publication number
- JPH06200054A5 JPH06200054A5 JP5-902A JP90293A JPH06200054A5 JP H06200054 A5 JPH06200054 A5 JP H06200054A5 JP 90293 A JP90293 A JP 90293A JP H06200054 A5 JPH06200054 A5 JP H06200054A5
- Authority
- JP
- Japan
- Prior art keywords
- resin composition
- present
- temperature
- weight
- polyphenylene ether
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Description
【手続補正書】[Procedural Amendment Document]
【提出日】平成11年11月25日(1999.11.
25)[Submission Date] November 25, 1999 (Heisei 11)
25)
【手続補正1】[Procedural Amendment 1]
【補正対象書類名】明細書[Document to be amended] Statement
【補正対象項目名】0006[Item name to be corrected] 0006
【補正方法】変更[Correction Method] Change
【補正内容】[Correction Details]
【0006】[0006]
【課題を解決するための手段】本発明者らは上述のよう
な課題を解決するため鋭意検討を重ねた結果、特定の温
度以上で溶解することにより本発明の目的に沿った製造
方法を見出し本発明を完成するに到った。すなわち、本
発明はポリフェニレンエーテル系樹脂組成物をトルエン
に溶解して基材に含浸するプリプレグの製造方法におい
て、上記樹脂組成物を下式(I)で表される温度(T
℃)以上で溶解することを特徴とするプリプレグの製造
方法である。
T=149.5G+42.0 ・・・・・・・・・・(I)
[式中、Tは溶解する温度(℃)であり、GはG=(樹
脂組成物中のポリフェニレンエーテルの重量)/(トル
エンの重量+樹脂組成物中のポリフェニレンエーテルの
重量)で表される比率である。]
以下に本発明を詳しく述べる。[Means for Solving the Problems] The present inventors have conducted extensive research to solve the above-mentioned problems and have found a manufacturing method that is in line with the objectives of the present invention by dissolving the resin composition at a temperature above a specific temperature, thereby completing the present invention. That is, the present invention is a method for producing a prepreg in which a polyphenylene ether resin composition is dissolved in toluene and impregnated into a substrate, wherein the resin composition is dissolved at a temperature (T) represented by the following formula (I).
This is a method for producing a prepreg characterized by dissolution at temperatures of 149.5°C or higher. T = 149.5G + 42.0 ・・・・・・・・・・(I) [wherein T is the dissolution temperature (°C), and G is the ratio expressed as G = (weight of polyphenylene ether in the resin composition) / (weight of toluene + weight of polyphenylene ether in the resin composition).] The present invention will be described in detail below.