JPH0644448Y2 - Metal bat - Google Patents
Metal batInfo
- Publication number
- JPH0644448Y2 JPH0644448Y2 JP1989066596U JP6659689U JPH0644448Y2 JP H0644448 Y2 JPH0644448 Y2 JP H0644448Y2 JP 1989066596 U JP1989066596 U JP 1989066596U JP 6659689 U JP6659689 U JP 6659689U JP H0644448 Y2 JPH0644448 Y2 JP H0644448Y2
- Authority
- JP
- Japan
- Prior art keywords
- bat
- sound
- aluminum foil
- aluminum
- main body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
【考案の詳細な説明】 〔産業上の利用分野〕 本考案は、野球で使用する金属製バットに関する。DETAILED DESCRIPTION OF THE INVENTION [Industrial Application Field] The present invention relates to a metal bat used in baseball.
金属製バットはアルミニウム材で構成する場合、第5図
に示すように中空アルミニウム材で本体部1を形成し、
これに同じくアルミニウム材によるグリップエンド2を
溶接により取付けることが多い。When the metal bat is made of an aluminum material, the main body 1 is made of a hollow aluminum material as shown in FIG.
Similarly, the grip end 2 made of an aluminum material is often attached by welding.
前記本体部1は先端をヘッド部3として閉塞し、その近
傍はほぼ同径の打撃部4となり、テーパー部5を介して
細径のグリップ部6がある。The main body 1 is closed at its tip as a head 3, and a hitting portion 4 having substantially the same diameter is provided in the vicinity thereof, and a small-diameter grip portion 6 is provided via a taper portion 5.
かかる金属製バットは、木製バットに比べて打撃音が高
く、特に硬式野球ボールを打った時の聴音としては、木
製バットの「カッ」という明るい音に対して、アルミニ
ウムの金属製バットでは「カン」「カアァーン」と長く
尾を引く、極めて大きな音となる。Such a metal bat has a higher hitting sound than a wooden bat, and as a sound heard when a hardball is hit, a bat has a bright sound, whereas an aluminum metal bat has a The sound is very loud and has a long tail.
金属製バットの打撃音は一般に、打撃直後に発生した音
(第1音)と暫くして発生する音(第2音)の2種類の
音からなり、このうち第1音は衝撃とそれによって引き
起こされた振動によるものと考えられる。The hitting sound of a metal bat generally consists of two kinds of sounds, a sound (first sound) generated immediately after hitting and a sound (second sound) generated for a while, of which the first sound is caused by impact and It is thought to be due to the induced vibration.
また、第2音は打撃によって生じた振動の波がバット内
で拡散し、ヘッド部3とグリップエンド2との両端で反
射してバット内部を移動する間に位相が合致して大きな
振動となって音を発するものである。In addition, the second sound is a large vibration because the wave of the vibration generated by the impact diffuses inside the bat and is reflected at both ends of the head portion 3 and the grip end 2 to be in phase while moving inside the bat. It makes a sound.
なお、打者近傍の聴音は騒音計の計測によれば、木製バ
ットは90〜91bBであるが、アルミニウムの金属製バット
では109〜111dBとなる。The sound level near the batter is 90-91bB for the wooden bat, but 109-111dB for the aluminum metal bat, as measured by a sound level meter.
このようにアルミニウムの金属製バットでの高いレベル
の打撃音を連続して聴音すると、選手及び審判が聴力障
害を生じるおそれがある。また、周辺環境に対しても騒
音公害を生じかねない。If the high-level impact sound of the aluminum metal bat is continuously heard in this manner, the athlete and the referee may have a hearing impairment. In addition, noise pollution may occur in the surrounding environment.
本考案の目的は前記従来例の不都合を解消し、簡単かつ
安価に打撃音を小音化できる金属製バットを提供するこ
とにある。It is an object of the present invention to provide a metal bat which eliminates the inconveniences of the above-mentioned conventional example and can reduce the impact sound easily and inexpensively.
本考案は前記目的を達成するため、中空アルミニウム材
で形成したバットにおいて、該バットの長手方向の中間
部からヘッド部間の面上に接着剤を介してアルミニウム
箔を貼設したことを要旨とするものである。In order to achieve the above-mentioned object, the present invention provides a bat made of a hollow aluminum material, in which an aluminum foil is pasted on the surface between the intermediate portion in the longitudinal direction of the bat and the head portion via an adhesive. To do.
本考案によれば、バットの面上に接着剤を介してアルミ
ニウム箔が貼設されるので、この接着剤とアルミニウム
箔との作用で打撃によって生じた振動の波がバット内で
拡散するのを抑えることで第1音としての打撃音そのも
のを小音化し、また、打撃直後に発生する第1音から暫
くして発生する第2音を無くし、これらの相乗効果で小
音効果が得られる。According to the present invention, since the aluminum foil is pasted on the surface of the bat via the adhesive, the wave of vibration generated by the impact by the action of the adhesive and the aluminum foil is prevented from diffusing in the bat. By suppressing, the impact sound itself as the first sound is reduced, and the second sound that is generated for a while from the first sound that is generated immediately after the impact is eliminated, and the small sound effect is obtained by the synergistic effect of these.
以下、図面について本考案の実施例を詳細に説明する。 Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings.
第1図は本考案のアルミニウムの金属製バットの第1実
施例を示す一部切欠いた側面図で、バットは前記第5図
で説明したように中空アルミニウム材で本体部1を形成
し、これに同じくアルミニウム材によるグリップエンド
2を溶接するもので、前記本体部1は先端をヘッド部3
として閉塞し、その近傍はほぼ同径の打撃部4となり、
テーパー部5を介して細径のグリップ部6がある。FIG. 1 is a partially cutaway side view showing a first embodiment of an aluminum metal bat of the present invention. The bat has a main body 1 formed of a hollow aluminum material as described in FIG. Similarly, a grip end 2 made of an aluminum material is welded to the main body 1 and the tip of the main body 1 is a head 3.
As a result, the striking part 4 having almost the same diameter is formed in the vicinity thereof,
There is a small-diameter grip portion 6 via the taper portion 5.
これら本体部1とグリップエンド2とは、7000系アルミ
ニウム合金材から常法に従って形成されるもので、本体
部については抽伸管をスエージング加工してテーパー部
とグリップ部を成形した後ヘッド部をスピニング加工で
一体に閉塞し、この後熱処理して所要の強度を付与す
る。またグリップエンドは板材から絞り成形により形成
される。The main body 1 and the grip end 2 are formed from a 7000 series aluminum alloy material according to a conventional method. For the main body, the drawn portion is swaged to form the taper portion and the grip portion, and then the head portion is formed. They are closed together by spinning and then heat treated to give them the required strength. The grip end is formed by drawing a plate material.
本考案は、アルミニウム箔7を本体部1の打撃部4の外
面に円周方向に貼設した。In the present invention, the aluminum foil 7 is circumferentially attached to the outer surface of the striking portion 4 of the main body 1.
該アルミニウム箔7はテープ状のもので、一例として、
箔の厚さ:30〜200μ、テープ幅:100mmとする。また、ア
ルミニウム箔7は、アクリル系接着剤や軟質エポキシ接
着剤などの接着剤8を介して貼設するが、この接着剤8
の厚さは30〜80μが好適である。The aluminum foil 7 is tape-shaped, and as an example,
Foil thickness: 30-200μ, tape width: 100mm. The aluminum foil 7 is attached via an adhesive 8 such as an acrylic adhesive or a soft epoxy adhesive.
The thickness is preferably 30 to 80 μm.
本体部1にグリップエンド2を溶接し、バフ研摩やアル
マイト処理を経てバットの完成品を得た後で、接着剤8
を塗布してアルミニウム箔7を貼るが、バット本体部1
への印刷がすでに済んでいる場合には、アルミニウム箔
7に同様の印刷を施しておき、本体部1への印刷が箔7
で隠れても支障ないようにする。After welding the grip end 2 to the main body 1 and buffing or alumite treatment to obtain a finished bat product, the adhesive 8
Is applied and aluminum foil 7 is attached, but the bat body 1
If the printing on the aluminum foil 7 has already been performed, the same printing is performed on the aluminum foil 7, and the printing on the main body 1 is performed on the foil 7.
Make sure it doesn't matter if you hide.
また、箔7を貼った後で印刷を行ってもよく、この場合
はバットの印刷工程時に箔7の面にも同時に印刷され
る。Further, printing may be performed after the foil 7 is attached, and in this case, the surface of the foil 7 is printed at the same time as the printing process of the bat.
アルミニウム箔7の重量は接着剤8を含めて5〜15g
で、バット全体の重量からすれば非常に僅かなものであ
る。The weight of the aluminum foil 7 including the adhesive 8 is 5 to 15 g.
The weight of the entire bat is very small.
第2図は本考案の第2実施例を示すもので、アルミニウ
ム箔7は本体部1のテーパー部5の外面に長手方向に延
びるように貼設した。FIG. 2 shows a second embodiment of the present invention, in which an aluminum foil 7 is attached to the outer surface of the tapered portion 5 of the main body 1 so as to extend in the longitudinal direction.
また、第3実施例として第3図に示すように同じテーパ
ー部5の外面でもアルミニウム箔7は前記第1実施例と
同じく円周方向に貼設する。Further, as shown in FIG. 3 as the third embodiment, the aluminum foil 7 is also attached to the outer surface of the same tapered portion 5 in the circumferential direction as in the first embodiment.
さらに、図示は省略するが他の実施例として、アルミニ
ウム箔7を貼る箇所はバットの長手方向の中間部からヘ
ッド部3間の面上であれば、どの位置を選択してもよ
く、外面のみならず内側に貼ることも考えられる。この
ように内側に貼る場合は、本体部1にグリップエンド2
を溶接する前にグリップ部6端の開口から差し入れて貼
るようにする。Further, although not shown, as another embodiment, the aluminum foil 7 may be attached at any position as long as it is on the surface between the middle portion in the longitudinal direction of the bat and the head portion 3, and only the outer surface. It is also possible to stick it on the inside. When sticking on the inside like this, the grip end 2 is attached to the main body 1.
Before welding, insert it from the opening at the end of the grip 6 and stick it.
次に、本考案の金属製バットの効果を試すための実験結
果を下記表1に示す。Next, Table 1 below shows experimental results for testing the effect of the metal bat of the present invention.
また、音の時間波形は第4図に示す通りである。 The time waveform of the sound is as shown in FIG.
前記表1と第4図から知見できるように、木製バットと
同等程度の小音化効果が認められ、連続して聴音しても
打撃音が気にならないレベルとなった。As can be seen from Table 1 and FIG. 4, a sound reduction effect equivalent to that of a wooden bat was recognized, and the impact sound was at a level that was not noticeable even when continuously listening.
これはアルミニウム箔7及び接着剤8の存在により、打
撃音そのものが小音化されたこと及び打撃直後に発生す
る第1音から暫くして発生する第2音がなくなったこと
の相乗効果によるものである。This is due to the synergistic effect of reducing the impact sound itself due to the presence of the aluminum foil 7 and the adhesive 8 and eliminating the second sound generated for a while from the first sound generated immediately after the impact. Is.
なお、アルミニウム箔7は前記表1にもあるように打撃
部4に円周貼りした場合が小音化効果が一番よいが、こ
の場合は剥離し易い。実打テストでは3000回程度で剥離
するが、剥離した場合は使用者において貼り代えること
も可能である。The aluminum foil 7 has the best sound reduction effect when it is circumferentially attached to the striking portion 4 as shown in Table 1 above, but in this case, it is easily peeled off. In the actual hit test, the tape is peeled off about 3000 times, but if peeled, it can be replaced by the user.
以上述べたように本考案の金属製バットは、中空アルミ
ニウム材で形成したバットにおいて、打撃聴音は「カ
ン」という明るい音となり、不快感がなく、打撃音その
ものが小音化できるものである。As described above, the metal bat of the present invention is a bat made of a hollow aluminum material, and the hitting sound becomes a bright sound of "can" without any discomfort and the hitting sound itself can be reduced.
また、製造するに際し、現行の生産ラインを特に変更す
る必要がなくきわめて容易で、製造コストも安価であ
り、アルミニウム箔は接着剤を含めても軽量なので重量
調整も容易なものである。In addition, when manufacturing, the current production line does not need to be particularly changed, which is extremely easy, the manufacturing cost is low, and the weight of the aluminum foil is easy to adjust because it is light even if it includes an adhesive.
第1図は本考案の金属製バットの第1実施例を示す一部
切欠いた側面図、第2図は同上第2実施例を示す側面
図、第3図は同上第3実施例を示す側面図、第4図は音
の時間波形を示す波形図、第5図は従来例を示す側面図
である。 1……本体部、2……グリップエンド 3……ヘッド部、4……打撃部 5……テーパー部、6……グリップ部 7……アルミニウム箔、8……接着剤FIG. 1 is a partially cutaway side view showing a first embodiment of the metal bat of the present invention, FIG. 2 is a side view showing the same second embodiment, and FIG. 3 is a side view showing the same third embodiment. FIG. 4 is a waveform diagram showing a time waveform of sound, and FIG. 5 is a side view showing a conventional example. 1 ... Main body part, 2 ... grip end 3 ... head part, 4 ... striking part 5 ... taper part, 6 ... grip part 7 ... aluminum foil, 8 ... adhesive
Claims (2)
いて、該バットの長手方向の中間部からヘッド部間の面
上に接着剤を介してアルミニウム箔を貼設したことを特
徴とする金属製バット。1. A bat made of a hollow aluminum material, characterized in that an aluminum foil is pasted on the surface between the intermediate portion in the longitudinal direction of the bat and the head portion via an adhesive agent.
るいはテーパー部に貼設する請求項第1項記載の金属製
バット。2. The metal bat according to claim 1, wherein the aluminum foil is attached to a hitting portion or a taper portion on the outer surface of the bat.