JPH0732165A - 金属母材への硬化材溶着方法 - Google Patents

金属母材への硬化材溶着方法

Info

Publication number
JPH0732165A
JPH0732165A JP17521493A JP17521493A JPH0732165A JP H0732165 A JPH0732165 A JP H0732165A JP 17521493 A JP17521493 A JP 17521493A JP 17521493 A JP17521493 A JP 17521493A JP H0732165 A JPH0732165 A JP H0732165A
Authority
JP
Japan
Prior art keywords
hardening material
base metal
hardening
coil
frequency current
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP17521493A
Other languages
English (en)
Inventor
Koji Yokoyama
宏治 横山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NIPPON BOORUBARUBU KK
Nippon Ball Valve Co Ltd
Original Assignee
NIPPON BOORUBARUBU KK
Nippon Ball Valve Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NIPPON BOORUBARUBU KK, Nippon Ball Valve Co Ltd filed Critical NIPPON BOORUBARUBU KK
Priority to JP17521493A priority Critical patent/JPH0732165A/ja
Publication of JPH0732165A publication Critical patent/JPH0732165A/ja
Pending legal-status Critical Current

Abstract

(57)【要約】 【目的】 金属母材の表面を短時間で硬化処理する方法
を提供することである。 【構成】 金属母材1の所定位置にリング状の導電性硬
化材3を載せ、その硬化材3とコイル5を接近させ、該
コイル5に高周波電流を供給して、上記硬化材3を溶融
させて上記母材1に溶着させる。

Description

【発明の詳細な説明】
【0001】
【産業上の利用分野】この発明は金属母材への硬化材溶
着方法に関し、例えば流体輸送用バルブのジスクやシー
トの表面硬化に利用されるものである。
【0002】
【従来の技術】金属部品の部分的表面硬化方法として、
従来一般に知られている方法としては、溶射法及び肉盛
溶接法がある。溶射法は、溶融状態に加熱した硬化材料
粉末あるいは粒子を母材表面に高速度で吹付けて硬化皮
膜をつくり、更に後工程としてフュージング処理を行
い、母材に加熱溶融させる方法である。また、肉盛溶接
法は、硬化材でなる溶接棒を用いて母材表面に硬化層を
溶着する方法である。
【0003】
【発明が解決しようとする課題】上記の溶射法による
と、粉塵(金属粒子)の飛散、フュームの発生、騒音の
発生等により作業環境が汚染される問題がある。
【0004】また、上記の肉盛溶接法は、通常の溶接範
囲であっても前記溶射法の約3倍の時間を要する問題が
ある。
【0005】そこで、この発明はこれらの方法に代え
て、作業環境の汚染がなく、しかも短時間で金属母材の
表面に硬化層を形成できる硬化材の溶着方法を提供する
ことを目的とする。
【0006】
【課題を解決するための手段】上記の課題を解決するた
めに、この発明は、金属母材の所定位置にリング状の導
電性硬化材を載せ、その硬化材の部分とコイルを接近さ
せ、該コイルに高周波電流を供給して上記硬化材及び母
材の一部を溶融させ、該硬化材を母材の端面に溶着させ
ることにより、金属母材の表面に硬化層を形成するよう
にしたものである。
【0007】
【実施例】図1は、円筒状の金属母材1を昇降台2の上
に載せ、その金属母材1の上端面にリング状の硬化材3
(例えば、ステライト製)を載せ、更にその硬化材3の
上方に高周波電流発生装置4に支持されたコイル5を臨
ませた装置を示すものである。昇降台2の高さを適宜調
節したのち、上記コイル5に高周波電流を供給する。こ
のとき、昇降台2上の回転部6を回転させ、溶融の均等
化を図る。
【0008】図2の(A)の溶融前の状態から(B)の
ように硬化材3及び母材1の端部が溶融され、硬化材3
が金属母材1の表面に溶着される。
【0009】その後、高周波電流の供給を停止して冷却
固化させたのち、(C)のように機械加工を施して仕上
げる。
【0010】
【発明の効果】この発明によれば、高周波加熱電流は極
めて短時間に硬化材を母材に溶融溶着させるので、従来
の方法に比べ大幅に作業時間を短縮することができる。
【0011】また、高周波電流による加熱は、従来の方
法のように防塵の飛散、フュームの発生、騒音の発生等
がなく、作業環境を改善することができる。
【図面の簡単な説明】
【図1】溶融溶着装置の斜視図
【図2】(A)溶融前の状態を示す一部断面図 (B)溶融後の状態を示す一部断面図 (C)機械加工後の状態を示す一部断面図 〔図面の簡単な説明〕 1 金属母材 2 昇降台 3 硬化材 4 高周波発生装置 5 コイル

Claims (1)

    【特許請求の範囲】
  1. 【請求項1】 金属母材の所定位置にリング状の導電性
    硬化材を載せ、その硬化材の部分とコイルを接近させ、
    該コイルに高周波電流を供給して上記硬化材及び母材の
    一部を溶融させ、該硬化材を母材の端面に溶着させるこ
    とを特徴とする金属母材への硬化材溶着方法。
JP17521493A 1993-07-15 1993-07-15 金属母材への硬化材溶着方法 Pending JPH0732165A (ja)