JPH0784612B2 - Ca快削鋼の溶製方法 - Google Patents

Ca快削鋼の溶製方法

Info

Publication number
JPH0784612B2
JPH0784612B2 JP6368991A JP6368991A JPH0784612B2 JP H0784612 B2 JPH0784612 B2 JP H0784612B2 JP 6368991 A JP6368991 A JP 6368991A JP 6368991 A JP6368991 A JP 6368991A JP H0784612 B2 JPH0784612 B2 JP H0784612B2
Authority
JP
Japan
Prior art keywords
steel
inclusions
free
composition
machinability
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP6368991A
Other languages
English (en)
Japanese (ja)
Other versions
JPH04280911A (ja
JPH04280911A5 (mo
Inventor
明 大滝
英男 手塚
正志 吉田
光一 大木
雅人 柳瀬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP6368991A priority Critical patent/JPH0784612B2/ja
Publication of JPH04280911A publication Critical patent/JPH04280911A/ja
Publication of JPH04280911A5 publication Critical patent/JPH04280911A5/ja
Publication of JPH0784612B2 publication Critical patent/JPH0784612B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Landscapes

  • Treatment Of Steel In Its Molten State (AREA)
JP6368991A 1991-03-06 1991-03-06 Ca快削鋼の溶製方法 Expired - Lifetime JPH0784612B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP6368991A JPH0784612B2 (ja) 1991-03-06 1991-03-06 Ca快削鋼の溶製方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP6368991A JPH0784612B2 (ja) 1991-03-06 1991-03-06 Ca快削鋼の溶製方法

Publications (3)

Publication Number Publication Date
JPH04280911A JPH04280911A (ja) 1992-10-06
JPH04280911A5 JPH04280911A5 (mo) 1994-04-19
JPH0784612B2 true JPH0784612B2 (ja) 1995-09-13

Family

ID=13236599

Family Applications (1)

Application Number Title Priority Date Filing Date
JP6368991A Expired - Lifetime JPH0784612B2 (ja) 1991-03-06 1991-03-06 Ca快削鋼の溶製方法

Country Status (1)

Country Link
JP (1) JPH0784612B2 (mo)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2003293027A (ja) * 2002-04-09 2003-10-15 Daido Steel Co Ltd カルシウム快削ステンレス鋼の製造方法
JP5137082B2 (ja) * 2008-12-19 2013-02-06 新日鐵住金株式会社 機械構造用鋼材およびその製造方法

Also Published As

Publication number Publication date
JPH04280911A (ja) 1992-10-06

Similar Documents

Publication Publication Date Title
Luyckx et al. Sulfide shape control in high strength low alloy steels
Yang et al. Optimum composition of CaO-SiO2-Al2O3-MgO slag for spring steel deoxidized by Si and Mn in production
PL148685B1 (en) Ferrosilicon inoculant for cast iron
CN105734397A (zh) 一种高强度灰铸铁材料及其熔炼浇注工艺
JP6937190B2 (ja) Ni−Cr−Mo−Nb合金およびその製造方法
LU502587B1 (en) Low-cost, high-strength ferritic nodular cast iron, and preparation method and use thereof
JPH06128618A (ja) 介在物の少ない電磁鋼板の製造方法
Seidu et al. Control of chilling tendency in grey cast iron reuse
JP2991796B2 (ja) マグネシウム脱酸による薄鋼板の溶製方法
CN116516111A (zh) 一种硬线钢的高效脱硫低铝合成渣及冶炼工艺
SU1002392A1 (ru) Раскислитель
JP5199543B2 (ja) アルミキルド鋼の溶製方法
JPH04280911A (ja) Ca快削鋼の溶製方法
CN114134391A (zh) 控制含硫低合金钢硫含量的冶炼方法
JP4107801B2 (ja) 磁気特性に優れたFe−Ni系パーマロイ合金の製造方法
RU2269577C1 (ru) Способ получения стали в дуговой электросталеплавильной печи
Riposan et al. Benefits of residual aluminum in ductile iron
RU2070603C1 (ru) Модификатор для быстрорежущей стали
RU2051984C1 (ru) Сталь
SU1044653A1 (ru) Сплав дл раскислени легировани и модифицировани стали
Aydemir Use of aluminium dross for slag treatment in secondary steelmaking to decrease amount of reducible oxides in ladle furnace
SU1617031A1 (ru) Лигатура дл стали
SU1633002A1 (ru) Лигатура дл стали
RU1770438C (ru) Жаростойкий алюминиевый чугун
JP4357082B2 (ja) 含クロム溶鋼の脱炭精錬方法

Legal Events

Date Code Title Description
A01 Written decision to grant a patent or to grant a registration (utility model)

Free format text: JAPANESE INTERMEDIATE CODE: A01

Effective date: 19960227