JPH0822842A - 密閉鉛電池の充電方法 - Google Patents
密閉鉛電池の充電方法Info
- Publication number
- JPH0822842A JPH0822842A JP6180694A JP18069494A JPH0822842A JP H0822842 A JPH0822842 A JP H0822842A JP 6180694 A JP6180694 A JP 6180694A JP 18069494 A JP18069494 A JP 18069494A JP H0822842 A JPH0822842 A JP H0822842A
- Authority
- JP
- Japan
- Prior art keywords
- discharge
- amount
- charge
- charging
- sealed lead
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
ビス用途の密閉鉛電池の寿命性能を著しく改善すること
ができる密閉鉛電池の充電方法を提供する。 【構成】 サイクルサービス用途の密閉鉛電池におい
て、放電の深さに関係なく、放電後の充電量を、放電量
に一定の電気量を加えた量とすること、さらに、一定の
電気量を、常温使用時において、定格容量の5〜10%
とする密閉鉛電池の充電方法。
Description
返されるサイクルサービス用途の密閉鉛電池の充電方法
に関するもので、寿命性能の優れた密閉鉛電池を提供す
るものである。
−Ca系格子を一般に用いているため、過充電を頻繁に
受けたり、大きな電流で過充電されたりすると早期に容
量が低下する。このため、密閉鉛電池を充電する場合に
は、定電圧充電器を用いて充電を行い、放電量に一定の
比率を乗じて得られる電気量を充電するという方法が従
来から使用されている。また、この方法は放電量に応じ
て充電量が決まるため、放電が浅い場合には過充電量を
少なくでき、放電が深い場合は過充電量を多くできると
いう特徴がある。
した例を調べてみると、放電量が一定の場合は特に問題
はないが、不規則な放電が繰り返される場合には短寿命
であることが多い。即ち、負荷の形態によって、寿命性
能が著しく異なっており、この方法では、電池の有する
実力を十分に引き出せない場合がある。
な放電が繰り返されるサイクルサービス用途の密閉鉛電
池において、放電後の充電量を、放電量に一定の電気量
を加えた量とすることと、加える量を定格容量の5〜1
0%とすることである。
60Ah(3HR放電時)の密閉鉛電池を製作した。こ
の電池を放電深さの異なる充放電サイクルにかけ、本発
明による充電方法で充電した。また、比較のため、従来
の充電方法を用いた場合の性能も試験した。これらの放
電条件と充電方法とを以下に示す。なお、試験は25℃
の気相中で行った。
充電電圧が2.5V/セルに達した時点で充電電流を
0.6Aとし、充電量が放電量に定格容量の7.5%を
加えた量に達した時点で充電を打切る。すなわち、上記
の1〜4の放電に対して、放電量や放電電流の大きさに
関係なく、過充電量を4.5Ahとする。2.定電流−
定電圧充電。充電電流を10A、充電電圧を2.5Vに
設定し、放電量の115%を充電する。
従来の充電方法で充電した場合の試験結果を表1に示
す。表中の値は、放電容量が定格容量の80%を切った
時点のサイクル数である。
るが、本発明による充電と従来の充電とを比較すると、
放電条件2の場合を除いて、いずれも本発明による充電
条件で充電した場合の方が容量推移は良い。従来の方法
で充電した場合の過充電量を求めると、放電条件2の場
合は、本発明による充電方法の過充電量とほぼ同じであ
るが、放電条件1や3の場合は、それぞれ1.8Ahと
7.2Ahであり、放電条件1の場合には充電不足に、
また放電条件3の場合には充電過多になっていることが
推察される。
調査したが、推察通り放電条件3の場合には、過充電に
起因すると考えられる正極板の劣化が寿命の原因であ
り、放電条件1の場合には、充電不足に起因する負極板
への硫酸鉛の蓄積が、容量低下の原因であった。放電条
件2の場合のみ、従来の充電方法でも問題がなかったの
は、たまたま本試験で設定した充電条件が、放電条件2
に適した条件であったためと考えられる。これに対し、
本発明による充電方法では、放電条件にかかわらず、過
充電量を一定にすることにより、電池の有する実力を引
き出すことができたといえる。
験結果を以下に述べる。試験には、上記と同様の電池を
使用し、以下に示す充放電条件で寿命性能を調べた。試
験温度は上述の試験と同様である。
充電電圧が2.5V/セルに達した時点で充電電流を
0.6Aとし、充電量が放電量に定格容量の2%を加え
た量に達した時点で充電を打切る。すなわち、過充電量
を1.2Ahとする。 2.上記と同様の充電で、充電量が放電量に定格容量の
5%を加えた量に達した時点で充電を打切る。すなわ
ち、過充電量を3.0Ahとする。 3.上記と同様の充電で、充電量が放電量に定格容量の
7.5%を加えた量に達した時点で充電を打切る。すな
わち、過充電量を4.5Ahとする。 4.上記と同様の充電で、充電量が放電量に定格容量の
10%を加えた量に達した時点で充電を打切る。すなわ
ち、過充電量を6.0Ahとする。 5.上記と同様の充電で、充電量が放電量に定格容量の
15%を加えた量に達した時点で充電を打切る。すなわ
ち、過充電量を9.0Ahとする。
容量が定格容量の80%を切った時点のサイクル数であ
る。
件2〜4の場合の寿命性能が、1や5の場合のそれに比
べて良い。即ち、放電が浅い場合も、深い場合も、過充
電量としては3〜6Ah(定格容量の5〜10%)の電
気量が、適量であることを示している。
件1の場合には、充電不足に起因する負極板への硫酸鉛
の蓄積が容量低下の原因であり、充電条件5の場合に
は、過充電に起因すると考えられる正極板の劣化が容量
低下の原因であった。これに対し、放電が浅い場合に、
放電が深い場合と同様に6Ah(定格容量の10%)も
の過充電をすると充電過多になることが懸念されたが、
過充電に起因する劣化の兆候はほとんど見られなかっ
た。また、放電が深い場合に、放電が浅い場合と同様に
3Ah(定格容量の5%)の過充電量では充電不足にな
ることが懸念されたが、負極板への硫酸鉛の蓄積は見ら
れなかった。これらの結果は、過充電量を定格容量の5
〜10%とすれば、放電量がどのようであっても、電池
の有する実力を十分に引き出せることを示している。
量の如何にかかわらず適切な充電ができるので、不規則
な充放電が繰り返されるサイクルサービス用途の密閉鉛
電池の寿命性能が著しく改善され、その工業的価値は大
きい。
Claims (2)
- 【請求項1】 不規則な放電が繰り返されるサイクルサ
ービス用途の密閉鉛電池において、放電の深さに関係な
く、放電後の充電量を、放電量に一定の電気量を加えた
量とすることを特徴とする密閉鉛電池の充電方法。 - 【請求項2】 一定の電気量を、常温使用時において、
定格容量の5〜10%とする請求項1に記載の密閉鉛電
池の充電方法。