JPH09199162A5 - - Google Patents
Info
- Publication number
- JPH09199162A5 JPH09199162A5 JP8-25974A JP2597496A JPH09199162A5 JP H09199162 A5 JPH09199162 A5 JP H09199162A5 JP 2597496 A JP2597496 A JP 2597496A JP H09199162 A5 JPH09199162 A5 JP H09199162A5
- Authority
- JP
- Japan
- Prior art keywords
- electrode plate
- negative electrode
- active material
- positive electrode
- amendment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP02597496A JP3815511B2 (ja) | 1996-01-18 | 1996-01-18 | ニッケル・金属水素化物密閉形アルカリ蓄電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP02597496A JP3815511B2 (ja) | 1996-01-18 | 1996-01-18 | ニッケル・金属水素化物密閉形アルカリ蓄電池 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH09199162A JPH09199162A (ja) | 1997-07-31 |
| JPH09199162A5 true JPH09199162A5 (th) | 2003-04-11 |
| JP3815511B2 JP3815511B2 (ja) | 2006-08-30 |
Family
ID=12180709
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP02597496A Expired - Lifetime JP3815511B2 (ja) | 1996-01-18 | 1996-01-18 | ニッケル・金属水素化物密閉形アルカリ蓄電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3815511B2 (th) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP2736098B1 (en) | 2011-07-20 | 2019-01-09 | GS Yuasa International Ltd. | Cylindrically shaped battery |
| CN103474706A (zh) * | 2013-09-29 | 2013-12-25 | 赵云德 | 镍镉碱性干式电瓶 |
| CN115117466B (zh) * | 2022-06-17 | 2023-04-07 | 重庆宏辰科扬能源有限责任公司 | 圆柱形高压镍氢电池生产工艺 |
-
1996
- 1996-01-18 JP JP02597496A patent/JP3815511B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH09106810A5 (th) | ||
| JPH08321322A5 (th) | ||
| JPH11149914A5 (th) | ||
| EP1858095A3 (en) | Non-aqueous electrolyte secondary battery and positive electrode for the same | |
| JPH1040914A5 (th) | ||
| JPH09306497A5 (th) | ||
| JPH08277441A5 (th) | ||
| JPH10125335A5 (th) | ||
| JPH1125967A5 (th) | ||
| JPH06196170A5 (th) | ||
| JPH0969362A5 (th) | ||
| JPH08222281A5 (th) | ||
| JPH09115543A5 (th) | ||
| JPH0831425A5 (th) | ||
| JPH0790440A5 (th) | ||
| JPH07145454A5 (th) | ||
| JPH06111822A5 (th) | ||
| JPH0660871A5 (th) | ||
| JPH11171519A5 (th) | ||
| JPH09199128A5 (th) | ||
| JPH0835042A5 (th) | ||
| JPH08148143A5 (th) | ||
| JP2661407B2 (ja) | 鉛蓄電池用陰極板および鉛蓄電池用陰極板の製造法 | |
| JP2000058128A5 (th) | ||
| JPH10149811A5 (th) |