JPH1087332A5 - - Google Patents
Info
- Publication number
- JPH1087332A5 JPH1087332A5 JP8-242890A JP24289096A JPH1087332A5 JP H1087332 A5 JPH1087332 A5 JP H1087332A5 JP 24289096 A JP24289096 A JP 24289096A JP H1087332 A5 JPH1087332 A5 JP H1087332A5
- Authority
- JP
- Japan
- Prior art keywords
- lithium
- spherical
- composite oxide
- nickel composite
- document
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24289096A JP3429633B2 (ja) | 1996-09-13 | 1996-09-13 | 球状リチウム・ニッケル複合酸化物の製造方法とそれを正極に用いる非水電解液電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24289096A JP3429633B2 (ja) | 1996-09-13 | 1996-09-13 | 球状リチウム・ニッケル複合酸化物の製造方法とそれを正極に用いる非水電解液電池 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH1087332A JPH1087332A (ja) | 1998-04-07 |
| JPH1087332A5 true JPH1087332A5 (fr) | 2001-02-20 |
| JP3429633B2 JP3429633B2 (ja) | 2003-07-22 |
Family
ID=17095756
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP24289096A Expired - Fee Related JP3429633B2 (ja) | 1996-09-13 | 1996-09-13 | 球状リチウム・ニッケル複合酸化物の製造方法とそれを正極に用いる非水電解液電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3429633B2 (fr) |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2002203559A (ja) * | 2000-12-28 | 2002-07-19 | Sony Corp | 非水電解質二次電池及び正極活物質の製造方法 |
| JP5211416B2 (ja) * | 2001-05-17 | 2013-06-12 | 三菱化学株式会社 | 層状リチウムニッケルマンガン複合酸化物 |
| JP2003034536A (ja) * | 2001-07-19 | 2003-02-07 | Mitsubishi Chemicals Corp | 層状リチウムニッケルマンガン複合酸化物粉体の製造方法 |
| JP2003146662A (ja) * | 2001-11-13 | 2003-05-21 | Nikki Chemcal Co Ltd | リチウム・ニッケル・マンガン複合酸化物、その製造方法および用途 |
| TW200624385A (en) | 2004-10-27 | 2006-07-16 | Sumitomo Chemical Co | Nickel hydroxide powder and method for making same |
| JP2014197552A (ja) * | 2014-06-18 | 2014-10-16 | 三菱化学株式会社 | 層状リチウムニッケルマンガン複合酸化物 |
| JP7637634B2 (ja) * | 2019-12-10 | 2025-02-28 | 株式会社半導体エネルギー研究所 | キルン |
-
1996
- 1996-09-13 JP JP24289096A patent/JP3429633B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH1090222A5 (fr) | ||
| JPH08162132A5 (fr) | ||
| EP1282179A3 (fr) | Electrode négative d'une batterie rechargeable | |
| JPH06163031A5 (fr) | ||
| EP1309018A3 (fr) | Cellule électrochimique ayant un assemblage multiplaques d' électrodes dans un boitier de forme irrégulière | |
| CA2046226A1 (fr) | Pile a combustible solide, et electrode poreuse pour utilisation dans ladite pile | |
| WO2002082567A1 (fr) | Electrode negative pour accumulateur a electrolyte non aqueux et accumulateur a electrolyte non aqueux comprenant cette electrode negative | |
| JP2001167763A5 (fr) | ||
| JPH08321322A5 (fr) | ||
| JPH0778609A5 (fr) | ||
| JPH1040914A5 (fr) | ||
| EP1139479A3 (fr) | Batterie à électrolyte polymère et son procédé de fabrication | |
| JP2002119045A5 (fr) | ||
| JPH07296849A5 (fr) | ||
| JP6589802B2 (ja) | 全固体リチウム硫黄電池用正極 | |
| EP1249885A3 (fr) | Batterie nickel-métal hydrure | |
| JPH06150928A5 (fr) | ||
| JPH0969362A5 (fr) | ||
| EP1207576A3 (fr) | Composé de Cobalt utilisé dans une pile alcaline, sa méthode de fabrication, et plaque d'électrode positive de pile alcaline contenant ce composé | |
| JPH08264202A5 (fr) | ||
| JPH06196170A5 (fr) | ||
| JPH11171519A5 (fr) | ||
| JPH08111214A5 (fr) | ||
| JPH0831425A5 (fr) | ||
| JPH0574455A5 (fr) |