JPS5326932A - Method of producing sealed negative plate for alkaline battery - Google Patents
Method of producing sealed negative plate for alkaline batteryInfo
- Publication number
- JPS5326932A JPS5326932A JP10186376A JP10186376A JPS5326932A JP S5326932 A JPS5326932 A JP S5326932A JP 10186376 A JP10186376 A JP 10186376A JP 10186376 A JP10186376 A JP 10186376A JP S5326932 A JPS5326932 A JP S5326932A
- Authority
- JP
- Japan
- Prior art keywords
- negative plate
- alkaline battery
- producing sealed
- sealed negative
- producing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- Y02E60/12—
Landscapes
- Sealing Battery Cases Or Jackets (AREA)
- Primary Cells (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10186376A JPS5326932A (en) | 1976-08-26 | 1976-08-26 | Method of producing sealed negative plate for alkaline battery |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10186376A JPS5326932A (en) | 1976-08-26 | 1976-08-26 | Method of producing sealed negative plate for alkaline battery |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5326932A true JPS5326932A (en) | 1978-03-13 |
| JPS5631052B2 JPS5631052B2 (mo) | 1981-07-18 |
Family
ID=14311830
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP10186376A Granted JPS5326932A (en) | 1976-08-26 | 1976-08-26 | Method of producing sealed negative plate for alkaline battery |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5326932A (mo) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS54139229U (mo) * | 1978-03-20 | 1979-09-27 | ||
| US5306580A (en) * | 1992-03-09 | 1994-04-26 | Eveready Battery Company, Inc. | Electrochemical cell having a coated cup-shaped terminal |
| WO1995011527A1 (fr) * | 1993-10-22 | 1995-04-27 | Toyo Kohan Co., Ltd. | Feuille d'acier traite en surface pour boitier de batterie et boitier de batterie produit a l'aide de ladite feuille |
| US7914926B2 (en) | 2005-03-17 | 2011-03-29 | Hitachi Maxell, Ltd. | Flat-shaped battery |
-
1976
- 1976-08-26 JP JP10186376A patent/JPS5326932A/ja active Granted
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS54139229U (mo) * | 1978-03-20 | 1979-09-27 | ||
| US5306580A (en) * | 1992-03-09 | 1994-04-26 | Eveready Battery Company, Inc. | Electrochemical cell having a coated cup-shaped terminal |
| WO1995011527A1 (fr) * | 1993-10-22 | 1995-04-27 | Toyo Kohan Co., Ltd. | Feuille d'acier traite en surface pour boitier de batterie et boitier de batterie produit a l'aide de ladite feuille |
| KR100292173B1 (ko) * | 1993-10-22 | 2001-06-01 | 다나베 히로까즈 | 전지용 표면 처리 강판과 그 제조방법, 전지 케이스, 및 그 전지 케이스를 이용한 전지 |
| CN1090384C (zh) * | 1993-10-22 | 2002-09-04 | 东洋钢板株式会社 | 电池外壳用表面处理钢板和电池外壳 |
| US7914926B2 (en) | 2005-03-17 | 2011-03-29 | Hitachi Maxell, Ltd. | Flat-shaped battery |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5631052B2 (mo) | 1981-07-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5336641A (en) | Method of producing lead battery plate | |
| JPS5339440A (en) | Method of producing battery plate | |
| JPS531830A (en) | Method of producing lead battery plate | |
| JPS5281520A (en) | Method of producing sealed negative plate for alkaline battery | |
| JPS531827A (en) | Method of producing lead battery positive plate | |
| JPS531829A (en) | Method of producing lead battery plate | |
| JPS5342340A (en) | Method of producing battery plate | |
| JPS51116947A (en) | Method of producing cadmium negative plate for sealed alkaline battery | |
| JPS52114931A (en) | Method of manufacturing negative electrode plate for alkaline battery | |
| JPS531828A (en) | Method of producing lead battery positive plate | |
| JPS5281521A (en) | Method of producing sealed negative plate for alkaline battery | |
| JPS528435A (en) | Method of producing negative plate for alkaline battery | |
| JPS5261736A (en) | Method of producing negative plate for alkaline battery | |
| JPS51149540A (en) | Method of producing negative plate for alkaline battery | |
| JPS5271641A (en) | Method of producing lead battery plate | |
| JPS52144745A (en) | Method of producing lead battery plate | |
| JPS5358630A (en) | Method of producing lead battery paste negative plate | |
| JPS5325836A (en) | Method of producing battery plate | |
| JPS5261737A (en) | Method of producing cadmium negative plate for alkaline battery | |
| JPS5253237A (en) | Method of partially charging sealed alkaline battery negative plate | |
| JPS5340832A (en) | Method of producing lead battery positive plate | |
| JPS5353743A (en) | Method of producing lead battery positive plate | |
| JPS5220236A (en) | Method of producing negative plate for alkaline battery | |
| JPS51122738A (en) | Method of producing negative plate for alkaline battery | |
| JPS51150036A (en) | Method of producing negative plate for alkaline battery |