JPS5424A - Method of forming titanium oxide coating layer on glass surface - Google Patents
Method of forming titanium oxide coating layer on glass surfaceInfo
- Publication number
- JPS5424A JPS5424A JP6490277A JP6490277A JPS5424A JP S5424 A JPS5424 A JP S5424A JP 6490277 A JP6490277 A JP 6490277A JP 6490277 A JP6490277 A JP 6490277A JP S5424 A JPS5424 A JP S5424A
- Authority
- JP
- Japan
- Prior art keywords
- coating layer
- titanium oxide
- glass surface
- oxide coating
- forming titanium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Surface Treatment Of Glass (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6490277A JPS5424A (en) | 1977-06-03 | 1977-06-03 | Method of forming titanium oxide coating layer on glass surface |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6490277A JPS5424A (en) | 1977-06-03 | 1977-06-03 | Method of forming titanium oxide coating layer on glass surface |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5424A true JPS5424A (en) | 1979-01-05 |
| JPS5618547B2 JPS5618547B2 (en) | 1981-04-30 |
Family
ID=13271453
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6490277A Granted JPS5424A (en) | 1977-06-03 | 1977-06-03 | Method of forming titanium oxide coating layer on glass surface |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5424A (en) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5666563A (en) * | 1979-10-23 | 1981-06-05 | Transamerica Delaval Inc | Pressure seal assembly |
| JPS57172963U (en) * | 1981-04-27 | 1982-10-30 | ||
| US5403368A (en) * | 1991-11-29 | 1995-04-04 | Central Glass Company, Limited | Metal oxide film having minutely roughed surface and method of forming same on glass substrate |
| US5730771A (en) * | 1993-03-05 | 1998-03-24 | Glaverbel | Method of manufacturing a corrosion resistant pyrolytically coated glass |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6134336U (en) * | 1984-03-13 | 1986-03-03 | 開司 山口 | Cartridge type fuel tank |
-
1977
- 1977-06-03 JP JP6490277A patent/JPS5424A/en active Granted
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5666563A (en) * | 1979-10-23 | 1981-06-05 | Transamerica Delaval Inc | Pressure seal assembly |
| JPS63180773U (en) * | 1979-10-23 | 1988-11-22 | ||
| JPS57172963U (en) * | 1981-04-27 | 1982-10-30 | ||
| US5403368A (en) * | 1991-11-29 | 1995-04-04 | Central Glass Company, Limited | Metal oxide film having minutely roughed surface and method of forming same on glass substrate |
| US5730771A (en) * | 1993-03-05 | 1998-03-24 | Glaverbel | Method of manufacturing a corrosion resistant pyrolytically coated glass |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5618547B2 (en) | 1981-04-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS53100978A (en) | Method of forming tin oxide thin film coating layer on supporting body | |
| JPS5341319A (en) | Method of coating surface of glass or ceramic | |
| JPS53133236A (en) | Method of forming multiicoating layers on substrate surface | |
| JPS56152965A (en) | Method of coating surface covered with oxide whisker | |
| GB2018234B (en) | Method of coating glass surface with heatreflectice titanium oxide film | |
| JPS5458736A (en) | Method of depositing low surface energy coating layer | |
| DE2861479D1 (en) | Method of coating glass surfaces | |
| JPS53127534A (en) | Protective method of article surfaces by foullproof coating layer | |
| JPS5419435A (en) | Method of forming highhtemperature protective coating layer | |
| JPS5651268A (en) | Method of coating surface of glass | |
| JPS5425A (en) | Method of chamfering glass substrate | |
| DE2861480D1 (en) | Method of coating glass surfaces | |
| JPS5466914A (en) | Method of making metal oxide coated glass | |
| JPS51134711A (en) | Method of producing glass having coating of titanium oxide | |
| JPS5418823A (en) | Method of coating glass surface | |
| JPS537716A (en) | Method of surface treatment of glass member | |
| JPS536314A (en) | Method of forming vapourrplated coating on glass | |
| JPS5422426A (en) | Method of forming titanium oxide coating layer on glass surface | |
| JPS5453125A (en) | Method of coating on glass surface | |
| JPS52919A (en) | Method of depositing thin film of metallic oxide on glass surface | |
| JPS5421409A (en) | Method of making tungstenncarbide coating layer | |
| JPS5423614A (en) | Method of forming metal oxide coating layer on glass sheet surface | |
| JPS532517A (en) | Method of surface treatment of glass substrate | |
| JPS546876A (en) | Method of forming colored coat over metal surface | |
| JPS5437120A (en) | Method of forming metal oxide thin layer on surface of glass |