JPS552705A - As-cast metal of pearlitic spheroidal graphite cast iron - Google Patents
As-cast metal of pearlitic spheroidal graphite cast ironInfo
- Publication number
- JPS552705A JPS552705A JP7319478A JP7319478A JPS552705A JP S552705 A JPS552705 A JP S552705A JP 7319478 A JP7319478 A JP 7319478A JP 7319478 A JP7319478 A JP 7319478A JP S552705 A JPS552705 A JP S552705A
- Authority
- JP
- Japan
- Prior art keywords
- cast metal
- cast
- diameter
- amount
- spheroidal graphite
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To omit the heat treatment, and to obtain the titled cast metal stably keeping the pearlite percentage above 80%, by restricting the amount of C, Si, Mn, and residual Mg, and by controlling the amount of Cu in respect of diameter of the cast metal.
CONSTITUTION: The as-cast metal of the pearlitic spheroidal graphite cast iron is obtained with the composition as follows; 3.3%≤C≤3.6%, 2.1%≤Si≤2.6%, 0.5%≤Mn≤1.0%, 0.03%≤ residual Mg≤0.06%, (0.002D+0.1)%≤Cu≤2.0%, in which D means the diameter or equivalent wall thickness of the cast metal, and the balance Fe. In the diagram, the pearlite percentage above 80% can be obtained in the left upper region above the line B; this straight line B is formulated in respect of the diameter Dmmϕ of the cast metal and the amount of Cu, as Cu%= 0.002×D+0.05.
USE: The crank shaft of the farm engine or the automobile engine and the cylinder cover of the Diesel engine.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7319478A JPS552705A (en) | 1978-06-19 | 1978-06-19 | As-cast metal of pearlitic spheroidal graphite cast iron |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7319478A JPS552705A (en) | 1978-06-19 | 1978-06-19 | As-cast metal of pearlitic spheroidal graphite cast iron |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS552705A true JPS552705A (en) | 1980-01-10 |
Family
ID=13511079
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP7319478A Pending JPS552705A (en) | 1978-06-19 | 1978-06-19 | As-cast metal of pearlitic spheroidal graphite cast iron |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS552705A (en) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6462439A (en) * | 1987-08-31 | 1989-03-08 | Mazda Motor | Casting of spheroidal graphite cast iron having excellent machinability |
| CN103088248A (en) * | 2011-11-01 | 2013-05-08 | 张玉新 | Formula of nodular cast iron used in automotive gear ring bracket |
| CN105945235A (en) * | 2016-06-30 | 2016-09-21 | 广西玉柴机器股份有限公司 | Crankshaft casting method |
-
1978
- 1978-06-19 JP JP7319478A patent/JPS552705A/en active Pending
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6462439A (en) * | 1987-08-31 | 1989-03-08 | Mazda Motor | Casting of spheroidal graphite cast iron having excellent machinability |
| CN103088248A (en) * | 2011-11-01 | 2013-05-08 | 张玉新 | Formula of nodular cast iron used in automotive gear ring bracket |
| CN105945235A (en) * | 2016-06-30 | 2016-09-21 | 广西玉柴机器股份有限公司 | Crankshaft casting method |
| CN105945235B (en) * | 2016-06-30 | 2017-11-21 | 广西玉柴机器股份有限公司 | The casting method of bent axle |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN103602878A (en) | Preparation method of high-toughness nodular cast iron | |
| JPS56263A (en) | High-manganese-content steel for low temperature | |
| JPS56163244A (en) | Heat resistant austenite steel with superior hot workability and oxidation resistance | |
| JPS5550451A (en) | Aluminum alloy for high strength die cast | |
| JPS64246A (en) | Spheroidal graphite cast iron | |
| JPS55128563A (en) | Cast iron excellent in wear and seizure resistance | |
| JPS57194240A (en) | High-strength ductile cast iron | |
| JPS56108853A (en) | High-tensile wear-resistance sliding member | |
| JPS57116753A (en) | High carbon steel wire rod with high toughness | |
| JPS5658945A (en) | High toughness nodular graphite cast iron | |
| JPS52149212A (en) | Production of ferrite-type spheroidal graphite cast iron as cast | |
| JPS5779153A (en) | Burning resistant iron alloy for oxygen duct | |
| JPS5579856A (en) | High toughness, wear resistant steel | |
| JPS54120220A (en) | Cast iron inoculating method and inoculant | |
| SU697587A1 (en) | Modifier | |
| JPS55100949A (en) | Ni base alloy for engine valve and valve seat of internal combustion engine | |
| JPS56123348A (en) | Cast iron for casting metal mold | |
| SU490832A1 (en) | Complex modifier | |
| JPS5465116A (en) | Wear resistant cast iron | |
| JPS5767147A (en) | Material for cylinder head of engine | |
| SU1705394A1 (en) | Cast iron | |
| JPS5651552A (en) | Cast steel for low temperature member | |
| JPS64245A (en) | Spheroidal graphite cast iron | |
| SU635153A1 (en) | Steel | |
| JPS57161047A (en) | Free cutting alloy cast iron |