JPS5558330A - Heat treating method of steam turbine rotor shaft - Google Patents
Heat treating method of steam turbine rotor shaftInfo
- Publication number
- JPS5558330A JPS5558330A JP12859978A JP12859978A JPS5558330A JP S5558330 A JPS5558330 A JP S5558330A JP 12859978 A JP12859978 A JP 12859978A JP 12859978 A JP12859978 A JP 12859978A JP S5558330 A JPS5558330 A JP S5558330A
- Authority
- JP
- Japan
- Prior art keywords
- rotor shaft
- hardening
- turbine rotor
- under
- steam turbine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To impart strength being superior at high and room temperatures and toughness being superior even at room temperature respectively to the turbine rotor shaft blank constituted by 12% Cr base steel by subjecting the same to heat treatment and tempering in the respectively specific temperature ranges. CONSTITUTION:The steam turbine rotor shaft blank constituted by so-called 12% Cr base steel containing 10-12% of Cr is heated at 950-1030 deg.C, particularly 980-1010 deg.C to be made to substantially austenite structure, after which it is hardened. It is made substantially to martensite structure by this hardening, after which it is subjected to annealing at 530-700 deg.C. Here, the hardening is accomplished by ordinary hardening methods such as oil hardening, water spray hardening, etc. The rotor shaft blank is desirably the alloy composed of C; 0.1-0.3%, Si; 0.6% or under, Cr; 9-13%, Mo; 0.5-2.0%, V; 0.1-0.3%, Ni; 2.5% or under, one or more of Kb or Ta; 0.03-0.2%, N; 0.1% or under and the rest Fe in weight ratio.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP12859978A JPS5558330A (en) | 1978-10-20 | 1978-10-20 | Heat treating method of steam turbine rotor shaft |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP12859978A JPS5558330A (en) | 1978-10-20 | 1978-10-20 | Heat treating method of steam turbine rotor shaft |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS5558330A true JPS5558330A (en) | 1980-05-01 |
Family
ID=14988748
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP12859978A Pending JPS5558330A (en) | 1978-10-20 | 1978-10-20 | Heat treating method of steam turbine rotor shaft |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5558330A (en) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS56166327A (en) * | 1980-05-28 | 1981-12-21 | Hitachi Ltd | Manufacture of rotor shaft |
| JPS59179719A (en) * | 1983-03-31 | 1984-10-12 | Toshiba Corp | Manufacture of turbine rotor |
| DE102018217304A1 (en) * | 2018-10-10 | 2020-04-16 | Siemens Aktiengesellschaft | Heat treatment for a NiCrMoV steel and martensitic steel |
-
1978
- 1978-10-20 JP JP12859978A patent/JPS5558330A/en active Pending
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS56166327A (en) * | 1980-05-28 | 1981-12-21 | Hitachi Ltd | Manufacture of rotor shaft |
| JPS59179719A (en) * | 1983-03-31 | 1984-10-12 | Toshiba Corp | Manufacture of turbine rotor |
| DE102018217304A1 (en) * | 2018-10-10 | 2020-04-16 | Siemens Aktiengesellschaft | Heat treatment for a NiCrMoV steel and martensitic steel |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| GB1417435A (en) | Alloyed spheroidal graphite iron | |
| GB936872A (en) | Improvements in or relating to a process of heat treating austenitic stainless steel and austenitic stainless steels whenever prepared by the aforesaid process | |
| JP3372219B2 (en) | Manufacturing method of steel parts | |
| US2395608A (en) | Treating inherently precipitationhardenable chromium-nickel stainless steel | |
| EP0020357B1 (en) | Lower bainite alloy steel article | |
| JPS57120616A (en) | Production of parts for mechanical structure | |
| JPS5916948A (en) | Soft-nitriding steel | |
| KR830004429A (en) | Manufacturing method of spheroidized annealed steel wire | |
| JPS5763628A (en) | Production of forge hardened parts | |
| JPS5629667A (en) | Preparation of metal mold | |
| JPS54104425A (en) | Heat treating method for high chromium white cast iron | |
| SU812835A1 (en) | Method of treatment of parts | |
| JPS5550430A (en) | Turbine rotor for geothermal electric power generation | |
| SU427069A1 (en) | METHOD OF TREATMENT OF STAINLESS STEEL AUSTENITE CLASS | |
| GB1089935A (en) | Method of strengthening alloy steel | |
| JPS5655566A (en) | Production of surface nitrided steel of good toughness | |
| SU584044A1 (en) | Method of heat treatment of components made of stainless maraging steels | |
| JPS60204837A (en) | Direct hardening method of steel | |
| SU436894A1 (en) | The method of chemical-heat treatment of steel | |
| SU472985A1 (en) | The method of processing steel | |
| KR970020244A (en) | Spring Band Clip Manufacturing Method | |
| Luty | Novel Processes for Heat Treatment of End-Products from Steel with 1% C and 1. 5% Cr | |
| SU870460A2 (en) | Method of thermal treatment of rolled wire and carbon and low-alloy steel wire | |
| SU489796A1 (en) | The method of thermochemical processing of steel products | |
| JPS5444122A (en) | Manufacturing method of welded valve |