JPS5562123A - Preparation of shadow mask - Google Patents
Preparation of shadow maskInfo
- Publication number
- JPS5562123A JPS5562123A JP13324578A JP13324578A JPS5562123A JP S5562123 A JPS5562123 A JP S5562123A JP 13324578 A JP13324578 A JP 13324578A JP 13324578 A JP13324578 A JP 13324578A JP S5562123 A JPS5562123 A JP S5562123A
- Authority
- JP
- Japan
- Prior art keywords
- cold rolled
- sol
- shadow mask
- annealing
- rolling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To have a less unevenness of hole shape and not to change the hole shape by press processing, by making Al killed cold rolled steel sheet having a specific constitution, limited the value of sol. Al/N by carrying out hot and cold rolling -annealing- skin-pass rolling of slab at the time of manufacturing color TV shadow mask. CONSTITUTION:Al killed cold rolled steel sheet composed of C<=0.01%, Mn; 0.1-1%, S<=0.025%, Sol.Al; 0.01-0.12%, N<=100ppm, Fe and inevitable impurities; balance and made (Sol.Al/N)X14/27>=1.5 and also fixed a greater part of N as AlN, is obtained by carrying out hot.cold rolling -annealing- skin-pass rolling of slab. Next, the above cold rolled sheet is cold rolled (draft 40%) again and thickness of the sheet is made 0.2mm or less. Then, the last annealing is carried out at 600-800 deg.C for 1-10 minutes after perforating by photo etching in usual shadow mask manufacturing process.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13324578A JPS5830929B2 (en) | 1978-10-31 | 1978-10-31 | How to make a shadow mask |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13324578A JPS5830929B2 (en) | 1978-10-31 | 1978-10-31 | How to make a shadow mask |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5562123A true JPS5562123A (en) | 1980-05-10 |
| JPS5830929B2 JPS5830929B2 (en) | 1983-07-02 |
Family
ID=15100092
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13324578A Expired JPS5830929B2 (en) | 1978-10-31 | 1978-10-31 | How to make a shadow mask |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5830929B2 (en) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS579857A (en) * | 1980-06-20 | 1982-01-19 | Nisshin Steel Co Ltd | Flat mask for manufacturing shadow mask for cathode-ray tube of color television and its manufacture |
| EP1298227A4 (en) * | 2000-06-26 | 2005-11-09 | Toyo Kohan Co Ltd | Raw material for shadow mask for color image receiving tube |
-
1978
- 1978-10-31 JP JP13324578A patent/JPS5830929B2/en not_active Expired
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS579857A (en) * | 1980-06-20 | 1982-01-19 | Nisshin Steel Co Ltd | Flat mask for manufacturing shadow mask for cathode-ray tube of color television and its manufacture |
| EP1298227A4 (en) * | 2000-06-26 | 2005-11-09 | Toyo Kohan Co Ltd | Raw material for shadow mask for color image receiving tube |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5830929B2 (en) | 1983-07-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5569238A (en) | Steel for shadow mask of color television braun tube | |
| CA2049378A1 (en) | High strength steel sheet adapted for press forming and method of producing the same | |
| JPS5651521A (en) | Production of shadow mask | |
| MY123398A (en) | Invar alloy steel sheet for shadow mask, method for producing same, shadow mask, and color picture tube | |
| JPS5562123A (en) | Preparation of shadow mask | |
| JPS54107415A (en) | Cold rolled steel plate with baking hardenability for deep drawing | |
| GB1464131A (en) | Manufacture of shadow masks | |
| JPS5553844A (en) | Manufacturing method of shadow mask for color television braun tube | |
| JPS54102224A (en) | Steel for shadow mask | |
| JPS54100958A (en) | Acid washing of hot rolled steel plate | |
| JPS5466313A (en) | Heat hardening type aluminum alloy for forming and manufacture of sheet using the same | |
| JPS555147A (en) | Cold rolling method of thin steel hoop for drawing | |
| JPS5440223A (en) | Oriented silicon steel sheet of low iron loss and manufacture thereof | |
| JPS57137427A (en) | Production of ferritic stainless steel sheet of superior workability | |
| JPS5471717A (en) | Manufacture of hot rolled steel sheet with superior workability | |
| JPS56102520A (en) | Manufacture of nonoriented silicon steel sheet very low in iron loss | |
| JPS55141522A (en) | Manufacture of ferrite stainless steel sheet with very little ridging | |
| JPS5494425A (en) | Method of producing material for shadow mask | |
| JPS5328016A (en) | Manufacture of steel plate for line pipe remarkably superior in low temperature toughness rolled as it is | |
| JPS579857A (en) | Flat mask for manufacturing shadow mask for cathode-ray tube of color television and its manufacture | |
| JPS5348913A (en) | Preparation of steel sheet for di can | |
| JPS5249926A (en) | Process for producing hot rolled hoop of excellent hot roll cale prope rty | |
| JPS5770223A (en) | Production of ferritic stainless steel sheet excellent in workability | |
| JPS5547320A (en) | Manufacture of nondirectional silicon steel sheet excellent in magnetic characteristic | |
| JPS5544582A (en) | High tensile hot rolled steel plate |