JPS56166242A - Preparation of rubber composition having high modulus of elasticity - Google Patents
Preparation of rubber composition having high modulus of elasticityInfo
- Publication number
- JPS56166242A JPS56166242A JP6957080A JP6957080A JPS56166242A JP S56166242 A JPS56166242 A JP S56166242A JP 6957080 A JP6957080 A JP 6957080A JP 6957080 A JP6957080 A JP 6957080A JP S56166242 A JPS56166242 A JP S56166242A
- Authority
- JP
- Japan
- Prior art keywords
- rubber
- rubber composition
- isotactic
- poly
- elasticity
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To prepare a rubber composition havning high modulus of elasticity and improved tear resistance industrially advantageously, by blending a dispersion of a high-melting isotactic polyolefin in an organic solvent with a rubber solution, followed by recovering the prepared mixture.
CONSTITUTION: A dispersion, obtained by dispersing a finely divided high-melting isotactic poly-α-olefin, e.g., poly(4-methyl-1-pentene), isotactic polypropylene, having an average particle diameter ≤200μ, preferably 50μ, into an organic solvent, is blended with a solution of rubber, e.g., polyisoprene rubber, polybutadiene rubber, styrene-butadiene rubber, etc. with stirring, and the prepared polymer mixture is recovered. Preferably the content of isotactic poly-α-olefin in the rubber composition is 20W40wt%, especially 3W25wt%.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (4)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6957080A JPS56166242A (en) | 1980-05-27 | 1980-05-27 | Preparation of rubber composition having high modulus of elasticity |
| US06/256,921 US4380607A (en) | 1980-04-28 | 1981-04-23 | Rubber composition having high modulus of elasticity and process for preparing same |
| DE8181301878T DE3175852D1 (en) | 1980-04-28 | 1981-04-28 | Process for the preparation of rubber compositions having a high modulus of elasticity |
| EP19810301878 EP0039240B1 (en) | 1980-04-28 | 1981-04-28 | Process for the preparation of rubber compositions having a high modulus of elasticity |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6957080A JPS56166242A (en) | 1980-05-27 | 1980-05-27 | Preparation of rubber composition having high modulus of elasticity |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS56166242A true JPS56166242A (en) | 1981-12-21 |
| JPS6255542B2 JPS6255542B2 (en) | 1987-11-20 |
Family
ID=13406567
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6957080A Granted JPS56166242A (en) | 1980-04-28 | 1980-05-27 | Preparation of rubber composition having high modulus of elasticity |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS56166242A (en) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2004263046A (en) * | 2003-02-28 | 2004-09-24 | Sumitomo Rubber Ind Ltd | Rubber composition for tire and pneumatic tire using the same |
| JP2004263045A (en) * | 2003-02-28 | 2004-09-24 | Sumitomo Rubber Ind Ltd | Rubber composition for tire and pneumatic tire using the same |
| JP2004339287A (en) * | 2003-05-13 | 2004-12-02 | Sumitomo Rubber Ind Ltd | Rubber composition for bead apex and pneumatic tire using the same |
-
1980
- 1980-05-27 JP JP6957080A patent/JPS56166242A/en active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2004263046A (en) * | 2003-02-28 | 2004-09-24 | Sumitomo Rubber Ind Ltd | Rubber composition for tire and pneumatic tire using the same |
| JP2004263045A (en) * | 2003-02-28 | 2004-09-24 | Sumitomo Rubber Ind Ltd | Rubber composition for tire and pneumatic tire using the same |
| JP2004339287A (en) * | 2003-05-13 | 2004-12-02 | Sumitomo Rubber Ind Ltd | Rubber composition for bead apex and pneumatic tire using the same |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6255542B2 (en) | 1987-11-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR860002542A (en) | Manufacturing method of powdered rubber | |
| JPS5638338A (en) | Thermoplastic resin composition | |
| DE2823156C2 (en) | ||
| JPS56166242A (en) | Preparation of rubber composition having high modulus of elasticity | |
| JPS54133588A (en) | Preparation of high-impact resin | |
| DE1569003A1 (en) | Process for dispersing rubss in polymers | |
| US3157609A (en) | Treatment of synthetic rubber | |
| DE1595293A1 (en) | Process for the production of copolymers | |
| JPS57187345A (en) | Rubber-modified styrene resin composition | |
| JPS5770137A (en) | Improved rubber composition | |
| JPS5730738A (en) | Production of rubber composition | |
| RU94046264A (en) | Elastosol, method for preparation thereof, and method of preparing homogeneous rubber-like product | |
| DE3937799A1 (en) | Preserving flowing qualities of elastomer granules on storage - granules are coated with small amt. of wollastonite, kaolinite, or mica to prevent clumping | |
| DE1669867C3 (en) | Vulcanizable molding compounds | |
| EP0272541A3 (en) | Conductive thermoplastic moulding composition, its preparation and use | |
| JPS55145744A (en) | Tire tread rubber composition | |
| SU1677046A1 (en) | Rubber mixture | |
| JPS5773033A (en) | Talc-containing propylene polymer composition | |
| JPS56166240A (en) | Preparation of rubber composition | |
| GB1128212A (en) | Method for the manufacture of vulcanizable polymer compositions | |
| JPS5578031A (en) | Softening and reclamation of vulcanized rubber | |
| JPS5529535A (en) | Preparation of reinforced rubber composition | |
| JPS5798544A (en) | Block copolymer resin composition | |
| DE2215413B2 (en) | Isolation of rubbers | |
| GB1151679A (en) | Improvement of Green Strength of Rubber Compounds |