JPS564676A - Adherent aluminum foil - Google Patents
Adherent aluminum foilInfo
- Publication number
- JPS564676A JPS564676A JP8185079A JP8185079A JPS564676A JP S564676 A JPS564676 A JP S564676A JP 8185079 A JP8185079 A JP 8185079A JP 8185079 A JP8185079 A JP 8185079A JP S564676 A JPS564676 A JP S564676A
- Authority
- JP
- Japan
- Prior art keywords
- aluminum foil
- foil
- water
- paste
- dried
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To provide an adherent aluminum foil which readily adheres to a table for a gas range or to wall surface around the gas rage in a kitchen and by which cleanness in the kitchen is kept by removing an oil foil and replacing it with a new one when the foil is stained, by a method wherein the back of the aluminum foil is coated with a water-soluble paste and then dried.
CONSTITUTION: The back of an aluminum foil 1 having an appropriate length and width is coated with a water-soluble paste 2 and then dried. The dried aluminum foil is rolled up to obtain the desired adherent aluminum foil 3. Wall surface 5 around a gas range 4 and the surface of a table 6 for the gas range are cleaned and then slightly wetted with water. The aluminum foil 3 rolled up is pulled out. The back thereof is put on the wall surface 5 or the surface of the table 6 to bond the foil by means of the paste 2. When the aluminum foil 1 is stained, the foil is removed and the paste 2 is wiped up with water.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8185079A JPS564676A (en) | 1979-06-26 | 1979-06-26 | Adherent aluminum foil |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8185079A JPS564676A (en) | 1979-06-26 | 1979-06-26 | Adherent aluminum foil |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS564676A true JPS564676A (en) | 1981-01-19 |
Family
ID=13757948
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP8185079A Pending JPS564676A (en) | 1979-06-26 | 1979-06-26 | Adherent aluminum foil |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS564676A (en) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS57165060A (en) * | 1981-04-04 | 1982-10-09 | Toyo Maintenance Kk | Cleaning method for high-temperature chamber where sticky substance or dust is generated in and adheres to |
| JPS57162836U (en) * | 1981-04-06 | 1982-10-14 | ||
| JP2016199764A (en) * | 2016-07-20 | 2016-12-01 | 日東電工株式会社 | Fire-resistant pressure-sensitive adhesive tape |
| CN108893075A (en) * | 2018-07-10 | 2018-11-27 | 深圳市有钱科技有限公司 | A kind of fire prevention aluminium foil paster for kitchen |
-
1979
- 1979-06-26 JP JP8185079A patent/JPS564676A/en active Pending
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS57165060A (en) * | 1981-04-04 | 1982-10-09 | Toyo Maintenance Kk | Cleaning method for high-temperature chamber where sticky substance or dust is generated in and adheres to |
| JPS57162836U (en) * | 1981-04-06 | 1982-10-14 | ||
| JP2016199764A (en) * | 2016-07-20 | 2016-12-01 | 日東電工株式会社 | Fire-resistant pressure-sensitive adhesive tape |
| CN108893075A (en) * | 2018-07-10 | 2018-11-27 | 深圳市有钱科技有限公司 | A kind of fire prevention aluminium foil paster for kitchen |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5354035A (en) | Method of forming protective layer on roll | |
| JPS51130074A (en) | Apparatus for cleaning off substances adhering to vessels or construct ions below the water surface | |
| JPS564676A (en) | Adherent aluminum foil | |
| EP0328746A3 (en) | Drying method for precision washing | |
| JPS5549225A (en) | Method for lining of inner surface of tube | |
| JPS52118613A (en) | Removal method for high viscosity fluid | |
| JPS5313653A (en) | Method of coating high-viscosity material and equipment therefor | |
| JPS55124573A (en) | Coating of object having uncoated portion | |
| JPS53129972A (en) | Parts supplying method in clean room | |
| JPS55128494A (en) | Preparing method for support body for lithographic printing | |
| JPS5583509A (en) | Machining method of engine cylinder | |
| JPS57187069A (en) | Rotary painting method | |
| JPS51133847A (en) | Drying apparatus for pipe | |
| JPS522069A (en) | Method of manufacturing wiper | |
| JPS5624193A (en) | Plate material for printing | |
| JPS5347697A (en) | Method of forming film of coating under the water | |
| JPS5235464A (en) | Rust getting off wallsurface in pipe and apparatus | |
| JPS53120749A (en) | Coating device of exterior surfaces of pipes with solvents | |
| JPS55144098A (en) | Production of resin-coated aluminum article | |
| JPS5483036A (en) | Coating antifouling in water | |
| JPS5326788A (en) | Method and apparatus for coating inner surfaces of many pores of porous element | |
| JPS57127475A (en) | Painting method for sheet | |
| JPS5535904A (en) | Formation of polyvinyl alcohol film on surface of instrument | |
| JPS5464862A (en) | Cleaning apparatus | |
| JPS5439701A (en) | Method of forming anti-oxidation protective film in condenser/water supply system |