JPS5648070A - Preparation of negative plate for lead acid battery - Google Patents
Preparation of negative plate for lead acid batteryInfo
- Publication number
- JPS5648070A JPS5648070A JP12440779A JP12440779A JPS5648070A JP S5648070 A JPS5648070 A JP S5648070A JP 12440779 A JP12440779 A JP 12440779A JP 12440779 A JP12440779 A JP 12440779A JP S5648070 A JPS5648070 A JP S5648070A
- Authority
- JP
- Japan
- Prior art keywords
- paste
- plate
- negative plate
- additive
- acid battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP54124407A JPS5945186B2 (ja) | 1979-09-27 | 1979-09-27 | 鉛蓄電池用陰極板の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP54124407A JPS5945186B2 (ja) | 1979-09-27 | 1979-09-27 | 鉛蓄電池用陰極板の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5648070A true JPS5648070A (en) | 1981-05-01 |
| JPS5945186B2 JPS5945186B2 (ja) | 1984-11-05 |
Family
ID=14884690
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP54124407A Expired JPS5945186B2 (ja) | 1979-09-27 | 1979-09-27 | 鉛蓄電池用陰極板の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5945186B2 (ja) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO1998031061A1 (en) * | 1997-01-10 | 1998-07-16 | Geo Specialty Chemicals, Inc. | Battery paste dispersant |
| JPH10261431A (ja) * | 1997-03-18 | 1998-09-29 | Shin Kobe Electric Mach Co Ltd | シール鉛蓄電池 |
| CN101937991A (zh) * | 2010-05-07 | 2011-01-05 | 张家口保胜新能源科技有限公司 | 一种高能铅酸蓄电池负极板铅膏及其制作方法 |
-
1979
- 1979-09-27 JP JP54124407A patent/JPS5945186B2/ja not_active Expired
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO1998031061A1 (en) * | 1997-01-10 | 1998-07-16 | Geo Specialty Chemicals, Inc. | Battery paste dispersant |
| US5948567A (en) * | 1997-01-10 | 1999-09-07 | Geo Specialty Chemicals, Inc. | Battery paste dispersant |
| JPH10261431A (ja) * | 1997-03-18 | 1998-09-29 | Shin Kobe Electric Mach Co Ltd | シール鉛蓄電池 |
| CN101937991A (zh) * | 2010-05-07 | 2011-01-05 | 张家口保胜新能源科技有限公司 | 一种高能铅酸蓄电池负极板铅膏及其制作方法 |
| CN101937991B (zh) | 2010-05-07 | 2012-12-26 | 张家口保胜新能源科技有限公司 | 一种高能铅酸蓄电池负极板铅膏及其制作方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5945186B2 (ja) | 1984-11-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5213539A (en) | Preparation of aqueous dispersion of polyolefin composition | |
| JPS527800A (en) | Processing equipment for paper forms | |
| JPS5648070A (en) | Preparation of negative plate for lead acid battery | |
| JPS528035A (en) | Preparation of polyolefin composition for coating | |
| JPS5249254A (en) | Novel iorganic filler | |
| GB1186245A (en) | Filler. | |
| JPS539841A (en) | Method and apparatus for coating water paint | |
| JPS5313650A (en) | Method of electrostatic coating | |
| JPS5518206A (en) | Spraying apparatus | |
| JPS569958A (en) | Metal vapour discharge lamp | |
| JPS5527827A (en) | Coating method for low melting point glass | |
| JPS5616605A (en) | Manufacture of ferromagnetic iron-cobalt alloy powder | |
| JPS53124565A (en) | Preparation of powdered resin | |
| JPS5379707A (en) | Preparation of porous sintered product of zinc | |
| JPS5577651A (en) | Supersonic humidifier with air cleaner | |
| JPS52155956A (en) | Cathode | |
| JPS5576569A (en) | Cadmium cathode plate for enclosed type alkali battery | |
| JPS5550575A (en) | Iron electrode for alkaline battery | |
| JPS5239950A (en) | Air conditioning method | |
| JPS5330639A (en) | Composition for coating inner surface of can | |
| JPS54145390A (en) | Cathode ray tube internal coating graphite | |
| JPS5239606A (en) | Process for dehydrogensulfide of acetylene containing hydrogen sulfide | |
| JPS55154344A (en) | Binder glass composition for coating fluorescent substance | |
| JPS5635369A (en) | Preparation of paste cadmium electrode for alkaline storage battery | |
| JPS53124542A (en) | Bulking agent for aquous adhesive |