JPS5666376A - Multielectrode arc welding method - Google Patents
Multielectrode arc welding methodInfo
- Publication number
- JPS5666376A JPS5666376A JP14149779A JP14149779A JPS5666376A JP S5666376 A JPS5666376 A JP S5666376A JP 14149779 A JP14149779 A JP 14149779A JP 14149779 A JP14149779 A JP 14149779A JP S5666376 A JPS5666376 A JP S5666376A
- Authority
- JP
- Japan
- Prior art keywords
- beads
- succeeding
- composite wire
- welding
- heat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To make possible welding of superior efficiency and the toughness of weld-heat-affected zone by employing an AC MIG welding method and performing multilayer welding of a plural pool system. CONSTITUTION:Preceding beads W3 are formed by the molten pool W1 relating to a preceding composite wire 1f, and the succeeding beads W4 are successively formed on the upper layer of the preceding beads W3 by the molten pool W2 relating to a succeeding composite wire 1r. Slag W5 is formed on the preceding beads W3 in front of the succeeding composite wire 1r, but since this slag W5 is thin, it is melted away without any problem by the arc of the succeeding composite wire 1r. In this way, the preceding and succeeding beads are formed approximately simultaneously by the respectively independent plural molten pools W1, W2 and the multilayer welding in one run is performed, hence the quantity of heat input is dispersed to the wires 1f, 1r and the low temperature toughness of the weld-heat affected zone is improved.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14149779A JPS5666376A (en) | 1979-10-31 | 1979-10-31 | Multielectrode arc welding method |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14149779A JPS5666376A (en) | 1979-10-31 | 1979-10-31 | Multielectrode arc welding method |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5666376A true JPS5666376A (en) | 1981-06-04 |
| JPS6333941B2 JPS6333941B2 (en) | 1988-07-07 |
Family
ID=15293305
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14149779A Granted JPS5666376A (en) | 1979-10-31 | 1979-10-31 | Multielectrode arc welding method |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5666376A (en) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS57202981A (en) * | 1981-06-05 | 1982-12-13 | Nippon Steel Corp | Highly tenacious ac mig welding method |
| JPS58103967A (en) * | 1981-12-15 | 1983-06-21 | Sumikin Yousetsubou Kk | Butt welding that enables all position welding |
| JP2007283363A (en) * | 2006-04-17 | 2007-11-01 | Nippon Steel Corp | UOE steel pipe manufacturing method |
| JP5966107B1 (en) * | 2016-02-02 | 2016-08-10 | 新日鉄住金エンジニアリング株式会社 | Automatic welding method and automatic welding apparatus |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0247063A (en) * | 1988-08-09 | 1990-02-16 | Nippon Baldwin Kk | Device for automatic cleaning of blanket cylinder |
| JPH02202451A (en) * | 1989-01-31 | 1990-08-10 | Nippon Baldwin Kk | Washing of web guide roller and its device |
| JPH03177257A (en) * | 1989-12-04 | 1991-08-01 | Tokyo Kikai Seisakusho Ltd | Web paper guiding device |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4996944A (en) * | 1973-01-20 | 1974-09-13 | ||
| JPS50129448A (en) * | 1974-03-30 | 1975-10-13 | ||
| JPS53149144A (en) * | 1977-05-31 | 1978-12-26 | Lincoln Electric Co | Arc welding method of metallic plate from one side surface and its device |
-
1979
- 1979-10-31 JP JP14149779A patent/JPS5666376A/en active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4996944A (en) * | 1973-01-20 | 1974-09-13 | ||
| JPS50129448A (en) * | 1974-03-30 | 1975-10-13 | ||
| JPS53149144A (en) * | 1977-05-31 | 1978-12-26 | Lincoln Electric Co | Arc welding method of metallic plate from one side surface and its device |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS57202981A (en) * | 1981-06-05 | 1982-12-13 | Nippon Steel Corp | Highly tenacious ac mig welding method |
| JPS58103967A (en) * | 1981-12-15 | 1983-06-21 | Sumikin Yousetsubou Kk | Butt welding that enables all position welding |
| JP2007283363A (en) * | 2006-04-17 | 2007-11-01 | Nippon Steel Corp | UOE steel pipe manufacturing method |
| JP5966107B1 (en) * | 2016-02-02 | 2016-08-10 | 新日鉄住金エンジニアリング株式会社 | Automatic welding method and automatic welding apparatus |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6333941B2 (en) | 1988-07-07 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE3481103D1 (en) | METHOD FOR JOINING METAL LAYERS. | |
| JPS5666376A (en) | Multielectrode arc welding method | |
| FR2345664A1 (en) | HEAT RECOVERY FROM MELTED SLAG FROM METALLURGIC TREATMENTS | |
| JPS5630080A (en) | One-side welding method of joint made of pure copper and copper-nickel base alloy clad steel | |
| JPS5626687A (en) | Production for copper-aluminum composite material | |
| NO168121C (en) | PROCEDURE FOR MELTING METAL SCRAP | |
| JPS53130241A (en) | Welding method for manufacture of thick walled steel pipe | |
| JPS55161591A (en) | Weld crack preventing method of alloy steel | |
| JPS57134277A (en) | Temper bead welding method | |
| Malinovska et al. | Present State in Submerged Arc Welding Processes with Increased Productivity | |
| Shigaev | Modulated-Current Welding | |
| JPS54109041A (en) | Electroslag welding method for thick metal | |
| FR2271045A1 (en) | Welded composite tube - having a layer of stainless steel and copper | |
| JPS5626689A (en) | Production for low-melting point metal composite string | |
| JPS6462279A (en) | Mig welding method for al and al alloy | |
| JPS5714181A (en) | Heat panel and manufacture thereof | |
| JPS5725281A (en) | Thick plate welding method | |
| JPS57156879A (en) | Manufacture of clad material | |
| JPS5519460A (en) | Horizontal position narrow groove welding method | |
| JPS53115642A (en) | Parallel mig welding method | |
| JPS5519444A (en) | Welding method of low temperature steel | |
| JPS53119236A (en) | Highly effecient welding method to obtain bond zone of high toughness | |
| LUCAS | Exploiting MIG-welding developments(Book) | |
| JPS5330408A (en) | Electro-slag refining process with composite electrode | |
| JPS55156668A (en) | End face treating method in nonconsumable electrode system arc welding |