JPS5729530A - Preparation of austenite-containing alloy pipe having excellent high temperature steam oxidation resistance and high temperature long duration strength - Google Patents
Preparation of austenite-containing alloy pipe having excellent high temperature steam oxidation resistance and high temperature long duration strengthInfo
- Publication number
- JPS5729530A JPS5729530A JP10239280A JP10239280A JPS5729530A JP S5729530 A JPS5729530 A JP S5729530A JP 10239280 A JP10239280 A JP 10239280A JP 10239280 A JP10239280 A JP 10239280A JP S5729530 A JPS5729530 A JP S5729530A
- Authority
- JP
- Japan
- Prior art keywords
- high temperature
- pipe
- austenite
- less
- oxidation resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To improve the high temperature steam oxidation resistance and high temperature long duration strength, by carrying out the nitriding treatment at a low temperature of an austenite-containing alloy pipe made of Cr-Ni steel having a specific composition and further by carrying out the solution treatment of the alloy pipe. CONSTITUTION:Pipes made of austenite-containing alloy steel containing 15-26% Cr, 8-35% Ni, 1.0% or less Si, 2.0% or less Mn and 0.2% or less Ti and, if necessary, further at least one element of 3% or less Mo and 0.6% or less Al are mitrided at a relatively low temperature of 500-1.000 deg.C. Subsequently, the solution treatment of the pipe is carried out at a temperature of 1,100 deg.C or higher to form a fine grain layer 50-500mu thick having a grain size mumber of 7 or finer on the inner surface of the pipe and to provide the pipe with a structure comprising the residual part having a grain size of 3-7. As the nitriding treatment is carried out at a low temperature, the evaporation of Cr in the alloy steel and the formation of an oxide film on the inner surface of the pipe are prevented so that the high temperature steam oxidation resistance and the high temperature long duration strength are improved.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10239280A JPS5729530A (en) | 1980-07-28 | 1980-07-28 | Preparation of austenite-containing alloy pipe having excellent high temperature steam oxidation resistance and high temperature long duration strength |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10239280A JPS5729530A (en) | 1980-07-28 | 1980-07-28 | Preparation of austenite-containing alloy pipe having excellent high temperature steam oxidation resistance and high temperature long duration strength |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS5729530A true JPS5729530A (en) | 1982-02-17 |
Family
ID=14326167
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP10239280A Pending JPS5729530A (en) | 1980-07-28 | 1980-07-28 | Preparation of austenite-containing alloy pipe having excellent high temperature steam oxidation resistance and high temperature long duration strength |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5729530A (en) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62278230A (en) * | 1986-05-26 | 1987-12-03 | Nippon Steel Corp | Manufacture of seam welded stainless steel pipe |
| US7014720B2 (en) | 2002-03-08 | 2006-03-21 | Sumitomo Metal Industries, Ltd. | Austenitic stainless steel tube excellent in steam oxidation resistance and a manufacturing method thereof |
| US20160289812A1 (en) * | 2010-02-04 | 2016-10-06 | Oda Industries Co., Ltd. | Process for manufacturing high-nitrogen stainless steel pipe with high strength, high ductility, and excellent corrosion and heat resistance |
-
1980
- 1980-07-28 JP JP10239280A patent/JPS5729530A/en active Pending
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62278230A (en) * | 1986-05-26 | 1987-12-03 | Nippon Steel Corp | Manufacture of seam welded stainless steel pipe |
| US7014720B2 (en) | 2002-03-08 | 2006-03-21 | Sumitomo Metal Industries, Ltd. | Austenitic stainless steel tube excellent in steam oxidation resistance and a manufacturing method thereof |
| US20160289812A1 (en) * | 2010-02-04 | 2016-10-06 | Oda Industries Co., Ltd. | Process for manufacturing high-nitrogen stainless steel pipe with high strength, high ductility, and excellent corrosion and heat resistance |
| US11015238B2 (en) * | 2010-02-04 | 2021-05-25 | Harumatu Miura | Process for manufacturing high-nitrogen stainless steel pipe with high strength, high ductility, and excellent corrosion and heat resistance |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5723050A (en) | Heat resistant steel with excellent high temp. strength | |
| JPS5681658A (en) | Austenitic alloy pipe with superior hot steam oxidation resistance | |
| JPS5716153A (en) | Stainless alloy having few flaw formed by rolling in hot rolling | |
| JPS54141310A (en) | Austentic stainless steel with superior corrosion resistance and hot workability | |
| JPS5558329A (en) | Production of iron base alloy pipe of superior oxidation resistance to high temperature steam | |
| JPS5693859A (en) | Ball alloy for grinding | |
| JPS552775A (en) | High manganese heat resistant steel | |
| JPS5713152A (en) | Steel for seamless steel pipe with superior corrosion resistance | |
| JPS5544528A (en) | High strength ferrite austenite two-phase stainless steel | |
| JPS56102554A (en) | Low strain case hardening steel | |
| JPS56108860A (en) | Super-high tensile steel with superior corrosion resistance | |
| JPS5589458A (en) | Austenite stainless steel for use in environment of high temperature and low chlorine concentration | |
| JPS5270924A (en) | Heat-resisting austenite casting alloy | |
| JPS5616654A (en) | Austenitic alloy for electric heating | |
| JPS5558354A (en) | Pipe material with superior high temperature steam oxidation resistance and superior high temperature long- time strength and manufacture thereof | |
| JPS5613466A (en) | Heat resistant steel | |
| JPS5644756A (en) | Steel for break disk excellent in resistance to cracking | |
| JPS5729563A (en) | Austenite type stainless steel with excellent corrosion resistance | |
| JPS57110656A (en) | Free cutting austenite stainless steel | |
| JPS5798658A (en) | Runner of water turbine with superior cavitation erosion resistance | |
| JPS5484818A (en) | Heat-resistant high-chrome steel having excellent processability and weldability | |
| JPS5589457A (en) | Pitting-resistant martensite stainless cast steel | |
| JPS563651A (en) | High toughness intermetallic compound material and its manufacture | |
| JPS5392323A (en) | Stainless steel product with excellent high temperature corrosion resistance | |
| JPS56150159A (en) | Chromium molybdenum steel with excellent corrosion resistance and erosion resistance |