JPS575817A - Stainless steel having excellent anticorrosion and preparation thereof - Google Patents
Stainless steel having excellent anticorrosion and preparation thereofInfo
- Publication number
- JPS575817A JPS575817A JP7874880A JP7874880A JPS575817A JP S575817 A JPS575817 A JP S575817A JP 7874880 A JP7874880 A JP 7874880A JP 7874880 A JP7874880 A JP 7874880A JP S575817 A JPS575817 A JP S575817A
- Authority
- JP
- Japan
- Prior art keywords
- superficial layer
- heating
- iron
- treated
- stainless steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To prepare the stainless steel being cheap and having excellent strength, toughness, anticorrosion and durability, by heating only a superficial layer to transform it into the form of α iron.
CONSTITUTION: About 100μ of the superficial layer of a material to be treated is transformed into the form of α iron by heating only the superficial layer of the material by e.g. a high frequency heating method. With a type of steel that requires a relatively long heating time for transforming into the form of α iron or a piece of steel having such a special shape that the heating of only the superficial layer is not applicable, the superficial layer of the material to be treated is given a work strain by shot peening or roll hammering in advance. Subsequently, the heating of only the superficial layer is carried out in a short time or the material to be treated is wholly heated and the heating is finished at the time when the superficial layer is transformed into the form of α iron.
COPYRIGHT: (C)1982,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7874880A JPS575817A (en) | 1980-06-10 | 1980-06-10 | Stainless steel having excellent anticorrosion and preparation thereof |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7874880A JPS575817A (en) | 1980-06-10 | 1980-06-10 | Stainless steel having excellent anticorrosion and preparation thereof |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS575817A true JPS575817A (en) | 1982-01-12 |
Family
ID=13670503
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP7874880A Pending JPS575817A (en) | 1980-06-10 | 1980-06-10 | Stainless steel having excellent anticorrosion and preparation thereof |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS575817A (en) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH04182081A (en) * | 1990-11-14 | 1992-06-29 | Sumitomo Metal Ind Ltd | Manufacture of wear resistant member |
| JP2013241635A (en) * | 2012-05-18 | 2013-12-05 | National Institute Of Advanced Industrial Science & Technology | Iron chromium alloy |
-
1980
- 1980-06-10 JP JP7874880A patent/JPS575817A/en active Pending
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH04182081A (en) * | 1990-11-14 | 1992-06-29 | Sumitomo Metal Ind Ltd | Manufacture of wear resistant member |
| JP2013241635A (en) * | 2012-05-18 | 2013-12-05 | National Institute Of Advanced Industrial Science & Technology | Iron chromium alloy |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5421917A (en) | Method of manufacturing non-quenched high-tensile steel having high toughness | |
| JPS56163248A (en) | Manufacture of drawn material of beryllium-copper alloy | |
| JPS54145335A (en) | Surface reforming of metal molding | |
| JPS575817A (en) | Stainless steel having excellent anticorrosion and preparation thereof | |
| JPS527879A (en) | Method of forming high hardness film on carbon tool steel or alloy too l steel | |
| JPS54138814A (en) | Thermo-mechanical treatment method for austenitic stainless steel pipe to give hot steam oxidation resistance | |
| JPS57171470A (en) | Production of coated spring | |
| JPS57207119A (en) | Surface-hardening method for pinion | |
| JPS5794516A (en) | Method for heat treatment on low-carbon boron steel | |
| JPS53104531A (en) | Surface processing method decreasing stress corrosion cracking | |
| JPS5719325A (en) | Production of steel product | |
| JPS5597421A (en) | Preparation of colored iron plate with excellent roll moldability | |
| JPS57209670A (en) | Rust-inhibiting treatment of clad steel plate | |
| JPS54160513A (en) | Manufacture of non-heat treated tough h-shaped steel | |
| JPS52125409A (en) | Chrome treated and direct quenched steel wire and its preparation | |
| Zhang et al. | A New Method to Evaluate the Hardening of Ion Implantation Into Metals by X-Ray Diffraction Technique | |
| Liebisch | Increase of Fatigue Resistance of Case Hardened Gears by Roll Strengthening | |
| Sumina et al. | Effect of the Mechanical Properties and Structure of Steel on its Wear Resistance | |
| JPS5322809A (en) | Heat treating method of piping | |
| JPS5538983A (en) | Production of high density powder molding by powder hot forging process | |
| JPS5465119A (en) | Manufacture of welded stainless steel tube with corrosion resistance | |
| JPS57203748A (en) | Alloy for composite magnetic material | |
| JPS5461981A (en) | Embrittlement judgement method of austenite base stainless steel welding metal | |
| JPS56116823A (en) | Production of connecting rod | |
| JPS5576046A (en) | Ultra low carbon nitriding steel |