JPS5961476U - 液循環式酸化銀電池 - Google Patents
液循環式酸化銀電池Info
- Publication number
- JPS5961476U JPS5961476U JP1982157904U JP15790482U JPS5961476U JP S5961476 U JPS5961476 U JP S5961476U JP 1982157904 U JP1982157904 U JP 1982157904U JP 15790482 U JP15790482 U JP 15790482U JP S5961476 U JPS5961476 U JP S5961476U
- Authority
- JP
- Japan
- Prior art keywords
- liquid circulation
- silver oxide
- oxide battery
- electrolyte
- battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
第1図は本考案によりスペーサーを貼付は正極板の平面
図である。第2図はスペーサーを貼付けた極板の側面図
である。 1・・・・・・極板、2・・・・・・スペーサー、3・
・・・・・電解液の流れ。
図である。第2図はスペーサーを貼付けた極板の側面図
である。 1・・・・・・極板、2・・・・・・スペーサー、3・
・・・・・電解液の流れ。
Claims (1)
- 電解液出入口部分の正・負極間に耐アルカリ性の絶縁物
質をスペーサーとして介在させる際、電解液出口部分が
電解液入口部会よりも密になるように配置したことを特
徴とする液循環式酸化銀電池。