JPS5983968A - コンクリ−ト組成物 - Google Patents
コンクリ−ト組成物Info
- Publication number
- JPS5983968A JPS5983968A JP19238982A JP19238982A JPS5983968A JP S5983968 A JPS5983968 A JP S5983968A JP 19238982 A JP19238982 A JP 19238982A JP 19238982 A JP19238982 A JP 19238982A JP S5983968 A JPS5983968 A JP S5983968A
- Authority
- JP
- Japan
- Prior art keywords
- concrete
- water
- early
- strengthening
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Curing Cements, Concrete, And Artificial Stone (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19238982A JPS5983968A (ja) | 1982-11-04 | 1982-11-04 | コンクリ−ト組成物 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19238982A JPS5983968A (ja) | 1982-11-04 | 1982-11-04 | コンクリ−ト組成物 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5983968A true JPS5983968A (ja) | 1984-05-15 |
| JPS623793B2 JPS623793B2 (it) | 1987-01-27 |
Family
ID=16290483
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP19238982A Granted JPS5983968A (ja) | 1982-11-04 | 1982-11-04 | コンクリ−ト組成物 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5983968A (it) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5478521A (en) * | 1992-09-01 | 1995-12-26 | W. R. Grace & Co.-Conn. | Method for making bughole-free hardened cement structural units using bughole-reducing cement admixtures |
-
1982
- 1982-11-04 JP JP19238982A patent/JPS5983968A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5478521A (en) * | 1992-09-01 | 1995-12-26 | W. R. Grace & Co.-Conn. | Method for making bughole-free hardened cement structural units using bughole-reducing cement admixtures |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS623793B2 (it) | 1987-01-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA1187908A (en) | Additive for hydraulic cement mixes | |
| US5156679A (en) | Air-detrainer for hydraulic cement compositions | |
| EP0202281B1 (en) | Additive for hydraulic cement mixes | |
| EP0558336A1 (en) | Hydraulic cement set-accelerating admixtures incorporating amino acid derivatives | |
| EP0101723A1 (en) | PROCESS FOR IMPROVING HYDRAULIC CEMENT MIXTURES. | |
| KR20010034109A (ko) | 분말상 수경성 조성물용 분산제의 제조방법 | |
| JP2002518283A (ja) | オキシアルキレンsraを用いた処理を受けさせるコンクリートのためのポリオキシアルキレン共重合体による空気連行 | |
| NZ199063A (en) | Additive composition for hydraulic cement containing alignin water reducing agent and an ethoxylated alkylphenol | |
| JPH10324550A (ja) | セメント系材料の添加剤、及びセメント系材料 | |
| CA1258474A (en) | Chloride-free hardening accelerator for portland cement, and preparation thereof | |
| AU2016265709B2 (en) | Polyalkoxylated polyamine oxide defoaming compositions | |
| JPH01108138A (ja) | ポルトランドセメント含有建築材料の収縮を減少するための添加剤 | |
| AU648002B2 (en) | Cement admixture and defoaming agent | |
| JPS6071561A (ja) | セメント組成物 | |
| JPS623793B2 (it) | ||
| JP2022515964A (ja) | セメント質組成物中の収縮低減剤としての変性オキシアルキルアミン | |
| JP2567322B2 (ja) | 現場打ち用の高充填性フレッシュコンクリート | |
| WO1999002465A1 (en) | Set-accelerating mixture for concrete | |
| JPS61117142A (ja) | セメント組成物 | |
| AU7670481A (en) | Additive grinding aid for granular blast furnace slag | |
| JP5378752B2 (ja) | セメント質組成物のウオッシュアウトを防止するための方法 | |
| HUT67591A (en) | Method for improving properties of hydraulic cements and building material | |
| JPS6461339A (ja) | 高強度セメント組成物 | |
| CA2495828C (en) | Fluidising composition | |
| KR100725030B1 (ko) | 초기강도 증진용 콘크리트 액상 혼화제 및 콘크리트 조성물 |