JPS61236635A - ガラスの表面処理法 - Google Patents

ガラスの表面処理法

Info

Publication number
JPS61236635A
JPS61236635A JP7715685A JP7715685A JPS61236635A JP S61236635 A JPS61236635 A JP S61236635A JP 7715685 A JP7715685 A JP 7715685A JP 7715685 A JP7715685 A JP 7715685A JP S61236635 A JPS61236635 A JP S61236635A
Authority
JP
Japan
Prior art keywords
gas
glass
amount
sulfur dioxide
glass product
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP7715685A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0454628B2 (de
Inventor
Morio Kimura
守男 木村
Noriyuki Fujita
則行 藤田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toyo Glass Co Ltd
Original Assignee
Toyo Glass Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toyo Glass Co Ltd filed Critical Toyo Glass Co Ltd
Priority to JP7715685A priority Critical patent/JPS61236635A/ja
Publication of JPS61236635A publication Critical patent/JPS61236635A/ja
Publication of JPH0454628B2 publication Critical patent/JPH0454628B2/ja
Granted legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C03GLASS; MINERAL OR SLAG WOOL
    • C03CCHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
    • C03C23/00Other surface treatment of glass not in the form of fibres or filaments

Landscapes

  • Chemical & Material Sciences (AREA)
  • Life Sciences & Earth Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • General Chemical & Material Sciences (AREA)
  • Geochemistry & Mineralogy (AREA)
  • Materials Engineering (AREA)
  • Organic Chemistry (AREA)
  • Surface Treatment Of Glass (AREA)
JP7715685A 1985-04-11 1985-04-11 ガラスの表面処理法 Granted JPS61236635A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP7715685A JPS61236635A (ja) 1985-04-11 1985-04-11 ガラスの表面処理法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP7715685A JPS61236635A (ja) 1985-04-11 1985-04-11 ガラスの表面処理法

Publications (2)

Publication Number Publication Date
JPS61236635A true JPS61236635A (ja) 1986-10-21
JPH0454628B2 JPH0454628B2 (de) 1992-08-31

Family

ID=13625928

Family Applications (1)

Application Number Title Priority Date Filing Date
JP7715685A Granted JPS61236635A (ja) 1985-04-11 1985-04-11 ガラスの表面処理法

Country Status (1)

Country Link
JP (1) JPS61236635A (de)

Cited By (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH02120256A (ja) * 1988-10-27 1990-05-08 Central Glass Co Ltd ガラス表面の処理方法
WO1992009303A1 (fr) * 1990-11-30 1992-06-11 The Green Cross Corporation Preparation d'albumine et sa conservation
WO2002051767A1 (fr) * 2000-12-26 2002-07-04 Nippon Sheet Glass Co.,Ltd. Verre a glace avec film protecteur et son procede de fabrication
JP2005170736A (ja) * 2003-12-11 2005-06-30 Ishizuka Glass Co Ltd 酸化反応抑制ガラス材及び酸化反応抑制ガラス容器
WO2011068225A1 (ja) * 2009-12-04 2011-06-09 旭硝子株式会社 ガラス板およびその製造方法
WO2011121811A1 (ja) * 2010-03-30 2011-10-06 東洋ガラス株式会社 ガラス容器及びガラス容器の内面処理方法
US8389052B2 (en) 2010-03-30 2013-03-05 Toyo Glass Co., Ltd. Method for treating inside surface of glass container and glass container
JP2013047111A (ja) * 2011-08-29 2013-03-07 Ishizuka Glass Co Ltd カルシウムイオン溶出抑制ガラス容器
WO2014104302A1 (ja) * 2012-12-27 2014-07-03 旭硝子株式会社 化学強化用フロートガラス

Cited By (12)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH02120256A (ja) * 1988-10-27 1990-05-08 Central Glass Co Ltd ガラス表面の処理方法
WO1992009303A1 (fr) * 1990-11-30 1992-06-11 The Green Cross Corporation Preparation d'albumine et sa conservation
US5372997A (en) * 1990-11-30 1994-12-13 The Green Cross Corporation Albumin preparation and method for preserving the same
WO2002051767A1 (fr) * 2000-12-26 2002-07-04 Nippon Sheet Glass Co.,Ltd. Verre a glace avec film protecteur et son procede de fabrication
JP2005170736A (ja) * 2003-12-11 2005-06-30 Ishizuka Glass Co Ltd 酸化反応抑制ガラス材及び酸化反応抑制ガラス容器
WO2011068225A1 (ja) * 2009-12-04 2011-06-09 旭硝子株式会社 ガラス板およびその製造方法
WO2011121811A1 (ja) * 2010-03-30 2011-10-06 東洋ガラス株式会社 ガラス容器及びガラス容器の内面処理方法
US8389052B2 (en) 2010-03-30 2013-03-05 Toyo Glass Co., Ltd. Method for treating inside surface of glass container and glass container
JP2013047111A (ja) * 2011-08-29 2013-03-07 Ishizuka Glass Co Ltd カルシウムイオン溶出抑制ガラス容器
WO2014104302A1 (ja) * 2012-12-27 2014-07-03 旭硝子株式会社 化学強化用フロートガラス
JPWO2014104302A1 (ja) * 2012-12-27 2017-01-19 旭硝子株式会社 化学強化用フロートガラス
US9714193B2 (en) 2012-12-27 2017-07-25 Asahi Glass Company, Limited Float glass for chemical strengthening

Also Published As

Publication number Publication date
JPH0454628B2 (de) 1992-08-31

Similar Documents

Publication Publication Date Title
EP0196075B1 (de) Reinigungssystem für Kontaktlinsen und Verfahren zu deren Reinigung
JPS61236635A (ja) ガラスの表面処理法
RU2707210C2 (ru) Способы термической обработки стеклянных изделий
US12251743B2 (en) Method of preventing lamellar silica formation in glass container
EP3755669A1 (de) Glasfläschchen mit geringer migrationslast
Taylor et al. Kinetics of dextrose degradation under autoclaving conditions
Piret et al. Influence of glass composition on the kinetics of glass etching and frosting in concentrated HF solutions
EP3755670A1 (de) Glasfläschchen mit erhöhter chemischer beständigkeit
US6187553B1 (en) Method of using additive formulation and method for making a tube with an additive formulation
US3249246A (en) Treatment of newly formed glass articles
Bender The stability of vitamin C in a commercial fruit squash
US3615319A (en) Ion exchange strengthening of glasses with lithium vapor
Cable et al. Theoretical analysis of the dissolution of multi-component gas bubbles
Fairbrother et al. CLXV.—The swelling of agar-agar
US3171768A (en) Method of detecting flaws in glass surfaces and solution used therefor
Evangelou et al. Correlation of Wine’s Main Components’ Concentration with the Density of Model Aqueous Solutions and Wine Samples
US3489546A (en) Strengthening of oxidized soda-lime glass articles
US2261689A (en) Treatment of glass containers to improve their chemical durability
EP0172698A1 (de) Verfahren zur Erhöhung der chemischen Beständigkeit von Rohren aus Borsilikatglas und hieraus hergestellte Artikel
CN120445785B (zh) 一种食用油过氧化值检测用标准样品的制备方法
CN114423719B (zh) 可以限制玻璃中含有的铅迁移到溶液中的处理含铅玻璃的方法
US2758040A (en) Process for producing colorless sterile invert sugar solution
US2261690A (en) Treatment of glass containers to improve their chemical durability
JPS632906B2 (de)
Jominy et al. Equilibrium in the Iron-Oxygen-Hydrogen System at Temperatures above 1000deg; C