JPS6129909Y2 - - Google Patents

Info

Publication number
JPS6129909Y2
JPS6129909Y2 JP5163480U JP5163480U JPS6129909Y2 JP S6129909 Y2 JPS6129909 Y2 JP S6129909Y2 JP 5163480 U JP5163480 U JP 5163480U JP 5163480 U JP5163480 U JP 5163480U JP S6129909 Y2 JPS6129909 Y2 JP S6129909Y2
Authority
JP
Japan
Prior art keywords
shoji
paper
muntin
adhesive
fine powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP5163480U
Other languages
Japanese (ja)
Other versions
JPS56151485U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP5163480U priority Critical patent/JPS6129909Y2/ja
Publication of JPS56151485U publication Critical patent/JPS56151485U/ja
Application granted granted Critical
Publication of JPS6129909Y2 publication Critical patent/JPS6129909Y2/ja
Expired legal-status Critical Current

Description

【考案の詳細な説明】 この考案は紙障子の組格子を構成する組子の構
造に関する。
[Detailed Description of the Invention] This invention relates to the structure of the kumiko that constitutes the latticework of paper shoji screens.

従来、紙障子の紙の貼り付けは紙の貼り付けの
たびに組格子の一面にでんぷん等の糊を付けてか
ら行なつている。ところがこのように紙を貼るの
に1回1回糊付けを行なうということは、その準
備および作業が非常に面倒であり、それにまた組
子にハケにより糊を付ける組子の側面に糊がはみ
出して見苦しくなるなどの問題もあり、糊付けも
なかなか面倒なものであつた。
Conventionally, each time paper is pasted on a paper shoji, glue such as starch is applied to one side of the latticework. However, the preparation and work involved in pasting paper one time at a time is extremely troublesome, and in addition, the glue tends to protrude from the sides of the muntin where the glue is applied by brushing onto the muntin. There were problems such as unsightliness, and gluing was also quite troublesome.

この考案は、このような問題点を解決するため
に考案されたもので、その目的は、障子に紙を貼
着するに際して糊付けなどの面倒なことをする必
要がなく、簡単にしかも綺麗に障子紙を貼ること
ができる障子用組子を提供することにある。
This invention was devised to solve these problems, and its purpose was to eliminate the need for troublesome things such as gluing when pasting paper on shoji, and to make it easy and beautiful to affix paper to shoji. The purpose is to provide a shoji kumiko to which paper can be pasted.

以下、この考案を図示する一実施例によつて説
明する。
This invention will be explained below with reference to an illustrative embodiment.

図中、符号1は組子、符号2は組格子、符号3
は障子枠、符号4は障子紙である。
In the figure, code 1 is a muntin, code 2 is a set lattice, code 3
is a shoji frame, and numeral 4 is shoji paper.

組子1は従来の組子と同様にアルミ等の金属製
型材で成形され、その一表面に組子1の長手方向
に連続する凹溝5が形成されている。凹溝5内に
は、再湿性接着剤6と木粉、金属粉またはその混
合物からなる不溶性微粉7とを圧縮混合した同形
状の層が長手方向に連続して形成されている。
The muntin 1 is molded from a metal mold material such as aluminum like the conventional muntin, and has grooves 5 continuous in the longitudinal direction of the muntin 1 formed on one surface thereof. In the groove 5, a layer of the same shape is formed continuously in the longitudinal direction, by compressing and mixing a rewetting adhesive 6 and an insoluble fine powder 7 made of wood powder, metal powder, or a mixture thereof.

再湿性接着剤6としては、アクリル酸エステル
に酢酸ビニルアクリル共重合体樹脂を酢酸ビニル
樹脂とを加えた混合体があり、水により膨〓し接
着性を生じ、乾燥すると強固に接着する特微を有
している。また、これは水に溶解して液出してし
まうこともないものである。
The rewetting adhesive 6 is a mixture of acrylic acid ester, vinyl acetate acrylic copolymer resin, and vinyl acetate resin, which has the characteristic that it swells with water to create adhesive properties, and when it dries, it forms a strong bond. have. Moreover, it does not dissolve in water and will not bleed out.

不溶性微粉7として、たとえばおがくず等の木
粉短繊維状の植物質微粉のように吸水性のあるも
のを使用すれば該微粉に接着剤が含浸し、接着剤
と微粉との一体性が強くなる。
If a water-absorbing material is used as the insoluble fine powder 7, such as a vegetable fine powder in the form of short wood fibers such as sawdust, the fine powder will be impregnated with the adhesive, and the integrity of the adhesive and the fine powder will be strengthened. .

なお、凹溝5底部には、再湿性接着剤6または
再湿性接着剤6と不溶性微粉7との混合物が組子
1の凹溝5内に確実に固着するように凹部8が多
数形成されている。
Note that a large number of recesses 8 are formed at the bottom of the groove 5 so that the rewetting adhesive 6 or the mixture of the rewetting adhesive 6 and the insoluble fine powder 7 is firmly fixed in the groove 5 of the muntin 1. There is.

このように成形された複数本の組子1を格子状
に組んで組格子2が構成され、組格子2は障子枠
3内に配されている。
A latticework 2 is constructed by assembling a plurality of muntins 1 formed in this manner in a lattice shape, and the latticework 2 is arranged within a shoji frame 3.

障子紙4の貼付けに際しては、組子1の再湿性
接着剤6と不溶性微粉との混合物の層の表面を水
でぬららし、再湿性接着剤6が溶けだして接着性
を帯びてきたら順次障子紙4を貼付ける。また、
障子紙4の貼換えに際しては、貼付けられた障子
紙4の前記混合の層に対応する部分を水でぬら
し、再湿性接着剤6が溶けだしたら障子紙4を剥
がし速やかに新しい障子紙4に貼換える。
When attaching the shoji paper 4, wet the surface of the layer of the mixture of rewetting adhesive 6 and insoluble fine powder of the kumiko 1 with water, and when the rewetting adhesive 6 begins to melt and become adhesive, apply the shoji paper one by one. Paste paper 4. Also,
When replacing the shoji paper 4, wet the part of the pasted shoji paper 4 corresponding to the above-mentioned mixed layer with water, and when the rewetting adhesive 6 begins to melt, peel off the shoji paper 4 and immediately paste it on a new shoji paper 4. exchange.

この考案は以上の構成からなり、以下に示す効
果が期待できる。
This invention consists of the above configuration, and the following effects can be expected.

組子凹溝内にある層の表面を水でぬらすと、
接着剤の一部が溶けだして接着性を帯び、乾燥
すると強固に接着するものであるから、組子を
水に浸したハケ等でぬらすだけで障子紙の貼付
けならびに貼換えが簡単にしかも綺麗に障子紙
を貼付けることができる。
When the surface of the layer inside the muntin groove is wetted with water,
A portion of the adhesive melts and becomes adhesive, and when it dries it becomes a strong bond, so pasting and replacing shoji paper is easy and clean just by wetting the kumiko with a brush soaked in water. You can attach shoji paper.

再湿性接着剤と不溶性の微粉、たとえば木
粉、金属粉またはこれらの混合物、その他木粉
等の植物質微粉とが混合され、接着剤間のつな
ぎ材になつているから再湿性接着剤の必要以上
の溶解が防止され、再湿性接着剤の反復利用が
可能である。
The rewetting adhesive is necessary because the rewetting adhesive is mixed with insoluble fine powder, such as wood flour, metal powder, a mixture thereof, and other vegetable fine powder such as wood flour, and is used as a binder between the adhesives. Further dissolution is prevented, and the rewetting adhesive can be used repeatedly.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図〜第3図はこの考案の実施例を示すもの
であり、第1図は障子の一部破断正面図、第2図
は組子の一部斜視図、第3図は障子紙の貼着状態
を示す組子の断面図、第4図は組子の従来例を示
す断面図である。 1……組子、2……組格子、3……障子枠、4
……障子紙、5……凹溝、6……再湿性接着剤、
7……微粉、8……凹部、9……組子、10……
凹溝、11……組子目地材。
Figures 1 to 3 show examples of this invention. Figure 1 is a partially cutaway front view of a shoji screen, Figure 2 is a partially perspective view of a shoji piece, and Figure 3 is a partially cutaway view of a shoji paper. FIG. 4 is a sectional view of a conventional example of a muntin. 1... Kumiko, 2... Kumiko lattice, 3... Shoji frame, 4
... Shoji paper, 5 ... Concave groove, 6 ... Rewetting adhesive,
7... Fine powder, 8... Concavity, 9... Kumiko, 10...
Concave groove, 11... Kumiko joint material.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 金属製の組子の一表面に前記組子の長手方向に
連続する凹溝を形成するととみに、該凹溝内に不
溶性微粉と再湿性接着剤とを混合した固形状の層
を形成してあることを特徴とする障子用組子。
When forming grooves continuous in the longitudinal direction of the metal muntin on one surface of the muntin, a solid layer of a mixture of insoluble fine powder and rewetting adhesive is formed in the groove. Kumiko for shoji screens is characterized by:
JP5163480U 1980-04-15 1980-04-15 Expired JPS6129909Y2 (en)