JPS6185065U - - Google Patents

Info

Publication number
JPS6185065U
JPS6185065U JP17064284U JP17064284U JPS6185065U JP S6185065 U JPS6185065 U JP S6185065U JP 17064284 U JP17064284 U JP 17064284U JP 17064284 U JP17064284 U JP 17064284U JP S6185065 U JPS6185065 U JP S6185065U
Authority
JP
Japan
Prior art keywords
solid electrolyte
peripheral edge
negative electrode
electrolyte layer
power generation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP17064284U
Other languages
Japanese (ja)
Other versions
JPH0243096Y2 (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP17064284U priority Critical patent/JPH0243096Y2/ja
Publication of JPS6185065U publication Critical patent/JPS6185065U/ja
Application granted granted Critical
Publication of JPH0243096Y2 publication Critical patent/JPH0243096Y2/ja
Expired legal-status Critical Current

Description

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は本考案の扁平形固体電解質電池の一実
施例を示す断面図であり、第2図は第1図に示す
電池に使用された負極側の封口板を示す斜視図で
ある。第3図は従来の扁平形固体電解質電池を示
す断面図である。 1…発電要素、2…正極、3…固体電解質層、
4…負極、5…金属基板、6…セラミツク製スペ
ーサ、7,8…封口板、9…ハンダ、10…耐熱
性樹脂絶縁被膜。
FIG. 1 is a sectional view showing an embodiment of a flat solid electrolyte battery of the present invention, and FIG. 2 is a perspective view showing a sealing plate on the negative electrode side used in the battery shown in FIG. 1. FIG. 3 is a sectional view showing a conventional flat solid electrolyte battery. 1... Power generation element, 2... Positive electrode, 3... Solid electrolyte layer,
4... Negative electrode, 5... Metal substrate, 6... Ceramic spacer, 7, 8... Sealing plate, 9... Solder, 10... Heat resistant resin insulation coating.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 2枚の金属製封口板7,8間に、少なくとも発
電要素1とリング状のセラミツク製スペーサ6と
を配置し、発電要素1の周縁部外方で封口板7,
8の周縁部とセラミツク製スペーサ1とをハンダ
9で接合して封止する扁平形固体電解質電池であ
つて、上記発電要素1が金属基板5上に正極2、
固体電解質層3および負極4の順に形成され、固
体電解質層3の周縁部が負極4の周縁部より外方
に突出し、正極2の周縁部が固体電解質層3の周
縁部より外方に突出していて、負極側の封口板8
の内面に短絡防止用の耐熱性樹脂絶縁被膜10を
形成していることを特徴とする扁平形固体電解質
電池。
At least the power generation element 1 and a ring-shaped ceramic spacer 6 are arranged between the two metal sealing plates 7 and 8, and the sealing plates 7 and 8 are disposed outside the periphery of the power generation element 1.
8 and a ceramic spacer 1 are bonded and sealed with solder 9, and the power generating element 1 is arranged on a metal substrate 5 with a positive electrode 2,
A solid electrolyte layer 3 and a negative electrode 4 are formed in this order, the peripheral edge of the solid electrolyte layer 3 protruding outward from the peripheral edge of the negative electrode 4, and the peripheral edge of the positive electrode 2 protruding outward from the peripheral edge of the solid electrolyte layer 3. Then, sealing plate 8 on the negative electrode side
A flat solid electrolyte battery characterized in that a heat-resistant resin insulation coating 10 for short circuit prevention is formed on the inner surface of the battery.
JP17064284U 1984-11-09 1984-11-09 Expired JPH0243096Y2 (en)