JPS6360503B2 - - Google Patents
Info
- Publication number
- JPS6360503B2 JPS6360503B2 JP56031059A JP3105981A JPS6360503B2 JP S6360503 B2 JPS6360503 B2 JP S6360503B2 JP 56031059 A JP56031059 A JP 56031059A JP 3105981 A JP3105981 A JP 3105981A JP S6360503 B2 JPS6360503 B2 JP S6360503B2
- Authority
- JP
- Japan
- Prior art keywords
- scandium
- halide
- arc
- lamp
- sodium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【発明の詳細な説明】
この発明は金属ハロゲン化物アーク放電ラン
プ、特にスカンジウムを含む発光管を有する金属
ハロゲン化物アーク放電ランプに関する。
プ、特にスカンジウムを含む発光管を有する金属
ハロゲン化物アーク放電ランプに関する。
金属ハロゲン化物アーク放電ランプの発光管充
填物にハロゲン化物又は単体の形によるスカンジ
ウムの使用が知られている。米国特許第3351798
号及び3979624号明細書はハロゲン化物としての
使用を開示し、米国特許第3407327号明細書は単
体としての使用を開示するのに対して米国特許第
3577029号明細書はそれらのいずれかの形での使
用を開示し、更に米国特許第3911308号明細書は
その両者の使用を開示する。
填物にハロゲン化物又は単体の形によるスカンジ
ウムの使用が知られている。米国特許第3351798
号及び3979624号明細書はハロゲン化物としての
使用を開示し、米国特許第3407327号明細書は単
体としての使用を開示するのに対して米国特許第
3577029号明細書はそれらのいずれかの形での使
用を開示し、更に米国特許第3911308号明細書は
その両者の使用を開示する。
金属ハロゲン化物アーク放電ランプの発光管充
填物には白色発光のためにスカンジウムが含めら
れる。これはしばしばハロゲン化物の形、例えば
よう化スカンジウムとして添加される。こうした
ハロゲン化物のみでの使用上の欠点はスカンジウ
ム単体による使用に比べて光束及びその維持で低
下を招くことにある。例えば、単体のスカンジウ
ムと同時によう化スカンジウムを含む175Wラン
プは13400ルーメンの光束を呈し、2000時間での
維持が82.8%であるのに対して、金属スカンジウ
ムなしでよう化スカンジウムのみを含む同様なラ
ンプは11000ルーメン光束を生じ、2000時間での
維持が61.8%であつた。しかしながら、単体のス
カンジウムの使用による欠点はライフ中にランプ
電圧の上昇が生じ、それが短寿命などの早期欠陥
を招く。
填物には白色発光のためにスカンジウムが含めら
れる。これはしばしばハロゲン化物の形、例えば
よう化スカンジウムとして添加される。こうした
ハロゲン化物のみでの使用上の欠点はスカンジウ
ム単体による使用に比べて光束及びその維持で低
下を招くことにある。例えば、単体のスカンジウ
ムと同時によう化スカンジウムを含む175Wラン
プは13400ルーメンの光束を呈し、2000時間での
維持が82.8%であるのに対して、金属スカンジウ
ムなしでよう化スカンジウムのみを含む同様なラ
ンプは11000ルーメン光束を生じ、2000時間での
維持が61.8%であつた。しかしながら、単体のス
カンジウムの使用による欠点はライフ中にランプ
電圧の上昇が生じ、それが短寿命などの早期欠陥
を招く。
従つて、本発明の目的は上記問題を解消する改
良された金属ハロゲン化物アーク放電ランプの提
供を目的とするものである。
良された金属ハロゲン化物アーク放電ランプの提
供を目的とするものである。
スカンジウム単体を含むランプにおけるランプ
電圧上昇の問題は予め決められたミニマム量のス
カンジウムハロゲン化物とナトリウムハロゲン化
物を添加することにより緩和できることが見い出
された。すなわち、発光管におけるアーク長の単
位センチメートル当りのミニマム量は、スカンジ
ウムハロゲン化物が約2.6×10-6グラム原子であ
り、ナトリウムハロゲン化物が約3.0×10-5グラ
ム原子である。本発明に係るこのミニマム値の規
制は、従来の単体スカンジウムとスカンジウムハ
ロゲン化物と共にナトリウムハロゲン化物を含む
金属ハロゲン化物アーク放電ランプの封入量より
大きいものである。また、従来のこの種金属ハロ
ゲン化物アーク放電ランプは4000時間正常点灯後
に20V以上のランプ電圧上昇となつていた。
電圧上昇の問題は予め決められたミニマム量のス
カンジウムハロゲン化物とナトリウムハロゲン化
物を添加することにより緩和できることが見い出
された。すなわち、発光管におけるアーク長の単
位センチメートル当りのミニマム量は、スカンジ
ウムハロゲン化物が約2.6×10-6グラム原子であ
り、ナトリウムハロゲン化物が約3.0×10-5グラ
ム原子である。本発明に係るこのミニマム値の規
制は、従来の単体スカンジウムとスカンジウムハ
ロゲン化物と共にナトリウムハロゲン化物を含む
金属ハロゲン化物アーク放電ランプの封入量より
大きいものである。また、従来のこの種金属ハロ
ゲン化物アーク放電ランプは4000時間正常点灯後
に20V以上のランプ電圧上昇となつていた。
本発明に係る金属ハロゲン化物ランプは通常の
ランプ構造であり、両端に電極を備え充填物とし
て水銀と始動ガス、例えばアルゴンに加えて、ス
カンジウム、スカンジウムハロゲン化物及びナト
リウムハロゲン化物を封入した溶融シリカ発光管
により構成される。充填物には他の金属ハロゲン
化物、例えばセシウムハロゲン化物も封入でき
る。
ランプ構造であり、両端に電極を備え充填物とし
て水銀と始動ガス、例えばアルゴンに加えて、ス
カンジウム、スカンジウムハロゲン化物及びナト
リウムハロゲン化物を封入した溶融シリカ発光管
により構成される。充填物には他の金属ハロゲン
化物、例えばセシウムハロゲン化物も封入でき
る。
要約すると、本発明の金属ハロゲン化物アーク
放電ランプは両端に電極を備え、水銀、始動ガ
ス、スカンジウム単体、及びアーク長の単位セン
チメートル当り少なくとも約2.6×10-6グラム原
子のスカンジウムハロゲン化物と3.0×10-5グラ
ム原子のナトリウムハロゲン化物を含む発光管に
より構成される。
放電ランプは両端に電極を備え、水銀、始動ガ
ス、スカンジウム単体、及びアーク長の単位セン
チメートル当り少なくとも約2.6×10-6グラム原
子のスカンジウムハロゲン化物と3.0×10-5グラ
ム原子のナトリウムハロゲン化物を含む発光管に
より構成される。
以下本発明に係る実施例について図面を参照し
つつ詳述する。
つつ詳述する。
図は本発明に係る金属ハロゲン化物アーク放電
ランプの発光管を示す。すなわち、具体的に正常
動作電圧が130Vである175Wの金属ハロゲン化物
ランプとして両端に電極2を有し、この電極間距
離で26cmのアーク長を形成する外径1mmの溶融シ
リカチユーブ1から構成された発光管が示され
る。この発光管の充填物には水銀、アルゴン、ス
カンジウム金属の小片と少量のセシウムよう化物
が含まれる。これらの充填物に加えて本発明の特
徴として11.52mgのナトリウムよう化物と2.88mg
のスカンジウムよう化物が含まれる。これらのよ
う化物の封入量は発光管のアーク長1cm当りで
3.0×10-5グラム原子のナトリウムよう化物と2.6
×10-9グラム原子のスカンジウムよう化物にそれ
ぞれ対応している。このような封入量でナトリウ
ムよう化物とスカンジウムよう化物を封入したラ
ンプ4000時間正常点灯動作後にランプ電圧の上昇
を20V以下に抑止できた。この種ランプの10本に
対する試験で4000時間の電圧上昇は僅か2Vにす
ぎなかつた。これに対して従来の175Wの金属ハ
ロゲン化物ランプではアーク長1cm当りで1.5×
10-5グラム原子のナトリウムよう化物と1.3×
10-6グラム原子のスカンジウムよう化物を封入し
ていたが、4000時間正常点灯動作後に23Vの電圧
上昇であつた。
ランプの発光管を示す。すなわち、具体的に正常
動作電圧が130Vである175Wの金属ハロゲン化物
ランプとして両端に電極2を有し、この電極間距
離で26cmのアーク長を形成する外径1mmの溶融シ
リカチユーブ1から構成された発光管が示され
る。この発光管の充填物には水銀、アルゴン、ス
カンジウム金属の小片と少量のセシウムよう化物
が含まれる。これらの充填物に加えて本発明の特
徴として11.52mgのナトリウムよう化物と2.88mg
のスカンジウムよう化物が含まれる。これらのよ
う化物の封入量は発光管のアーク長1cm当りで
3.0×10-5グラム原子のナトリウムよう化物と2.6
×10-9グラム原子のスカンジウムよう化物にそれ
ぞれ対応している。このような封入量でナトリウ
ムよう化物とスカンジウムよう化物を封入したラ
ンプ4000時間正常点灯動作後にランプ電圧の上昇
を20V以下に抑止できた。この種ランプの10本に
対する試験で4000時間の電圧上昇は僅か2Vにす
ぎなかつた。これに対して従来の175Wの金属ハ
ロゲン化物ランプではアーク長1cm当りで1.5×
10-5グラム原子のナトリウムよう化物と1.3×
10-6グラム原子のスカンジウムよう化物を封入し
ていたが、4000時間正常点灯動作後に23Vの電圧
上昇であつた。
上記具体例から明らかな通り、特定された充填
物の封入量を従来の封入量を越えて約2倍以上と
することは点灯動作中のランプ電圧上昇を抑止す
る点で実用的であり、従来の動作電圧上昇に伴な
つて生ずる短寿命や早期欠陥ランプの発生を防止
する。
物の封入量を従来の封入量を越えて約2倍以上と
することは点灯動作中のランプ電圧上昇を抑止す
る点で実用的であり、従来の動作電圧上昇に伴な
つて生ずる短寿命や早期欠陥ランプの発生を防止
する。
図は本発明に係る金属ハロゲン化物アーク放電
ランプの発光管の正面図である。 1……溶融シリカチユーブ(発光管)、2……
電極。
ランプの発光管の正面図である。 1……溶融シリカチユーブ(発光管)、2……
電極。
Claims (1)
- 1 両端に電極を備え、充填物として水銀、始動
ガス、スカンジウム単体、スカンジウムハロゲン
化物及びナトリウムハロゲン化物を封入した発光
管から成り、前記ナトリウムハロゲン化物及び前
記スカンジウムハロゲン化物の封入量をアーク長
1cm当りのミニマム量でそれぞれ3.0×10-5グラ
ム原子及び2.6×10-6グラム原子として4000時間
正常点灯動作後のランプ電圧上昇値を20V以下に
することを特徴とする金属ハロゲン化物アーク放
電ランプ。