JPS6436734A - Composite material - Google Patents

Composite material

Info

Publication number
JPS6436734A
JPS6436734A JP19098487A JP19098487A JPS6436734A JP S6436734 A JPS6436734 A JP S6436734A JP 19098487 A JP19098487 A JP 19098487A JP 19098487 A JP19098487 A JP 19098487A JP S6436734 A JPS6436734 A JP S6436734A
Authority
JP
Japan
Prior art keywords
composite
alloy
powder
composite material
reinforcing fibers
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
JP19098487A
Other languages
Japanese (ja)
Inventor
卓哉 鈴木
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Furukawa Electric Co Ltd
Original Assignee
Furukawa Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Furukawa Electric Co Ltd filed Critical Furukawa Electric Co Ltd
Priority to JP19098487A priority Critical patent/JPS6436734A/en
Publication of JPS6436734A publication Critical patent/JPS6436734A/en
Ceased legal-status Critical Current

Abstract

PURPOSE:To obtain a composite material having excellent strength and toughness by extruding the mixture of Al (alloy) powders and the composite powders of Al and ceramics grains or reinforcing fibers. CONSTITUTION:The powders of Al or Al alloy and the composite powders of Al and ceramics grains or reinforcing fibers are mixed. Said mixture is subjected to green compacting and is thereafter extruded, by which the composite material in which the composite body of Al and ceramics grains or reinforcing fibers is present, as the staple fibrous state, in the matrix metal consisting of Al or Al alloy is obtd. Said composite material has excellent strength and toughness.

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は、強度及び靭性に優れた複合材料に関するもの
である。
[Detailed Description of the Invention] [Industrial Field of Application] The present invention relates to a composite material with excellent strength and toughness.

〔従来の技術及びその問題点〕[Conventional technologies and their problems]

最近材料の軽量化、耐摩耗性の向上等を狙って1.71
.At合金等のマトリックス金属中にセラミックス粒子
や強化繊維を分散させた金属基複合材料(MMC)が注
目されている。
Recently, with the aim of reducing the weight of materials and improving wear resistance, 1.71
Metal matrix composites (MMCs), in which ceramic particles or reinforcing fibers are dispersed in a matrix metal such as At alloy, are attracting attention.

前記MMCの製造方法は、長、短繊維からなるプリフォ
ームを予め作成しておき、これにマトリックス金属のA
l等を圧力をかけて圧入する溶湯鍛造法と短繊維又は粒
子をマトリックス金属の粉末に混合して、均一に分散さ
せたものについて、圧粉、焼結、熱間加工等の工程をと
る粉末冶金法に大別される。而して溶湯鍛造法の場合は
強化物質とマトリックス金属との間の濡れ及び反応の問
題があり、種々の工夫が必要であるのに対して、粉末冶
金法の場合は強化物質とマトリックス金属はほぼ任意に
選ぶ事が可能であって、広範囲に渡うて利用さている。
The manufacturing method of the aforementioned MMC involves first creating a preform consisting of long and short fibers, and then adding a matrix metal A to it.
Metallurgy is broadly classified into two methods: molten metal forging, which involves injecting materials under pressure, and powder metallurgy, which involves mixing short fibers or particles with a matrix metal powder, uniformly dispersing the mixture, and then performing processes such as compaction, sintering, and hot working. In molten metal forging, there are issues of wetting and reaction between the reinforcing material and the matrix metal, requiring various ingenious methods. In contrast, in powder metallurgy, the reinforcing material and matrix metal can be selected almost arbitrarily, and it is used in a wide range of applications.

前記粉末冶金法では、強化物質をマトリックス金属中に
均一に分散させる事が最も重要であり、且つ強化物質が
粒子状である場合は微細である事が望まれる。又強化物
質とマトリックス金属粉末との混合には、ボールミル、
アトライター等が用いられており、特にアトライターの
場合は強化粒子がマトリックス金属の組織中に取り込ま
れて、非常に細かく且つ均一に分散し、所謂メカニカル
アロイとなって、強度が向上する。
In the aforementioned powder metallurgy method, the most important thing is to uniformly disperse the reinforcing material in the matrix metal, and if the reinforcing material is in particulate form, it is desirable that it be fine. Furthermore, for mixing the reinforcing material and the matrix metal powder, a ball mill is used.
Attritors are used, and in the case of attritors in particular, reinforcing particles are incorporated into the structure of the matrix metal, dispersed very finely and uniformly, forming a so-called mechanical alloy, which improves strength.

以上の樺に粉末冶金法によれば、任意の強化物質及びマ
トリックス金属の組合せに対して優れた強度を得る事が
出来、特にAl又はA4合金をマトリックス金属とする
MMCは軽量で強度、耐摩耗性等に優れており、摺動部
材等に広範囲な用途が期待されている。
As described above, powder metallurgy can be used to obtain excellent strength for any combination of reinforcing material and matrix metal. In particular, MMC with Al or A4 alloy as the matrix metal is lightweight and has excellent strength and wear resistance, and is expected to have a wide range of applications in sliding components and the like.

然しながら、前記粉末冶金法によるMMCは強度を向上
させる為に強化粒子又は強化繊維の体積含有率V、を増
すと延びが著しく低下するという問題が有り、例えばv
tが30%位になると、伸びは1%以下になってしまう
。
However, the MMC produced by the aforementioned powder metallurgy method has a problem in that increasing the volume content V of reinforcing particles or reinforcing fibers to improve strength significantly reduces elongation, for example v
When t reaches around 30%, the growth rate drops to less than 1%.

C問題点を解決する為の手段〕 本発明は上記の点に鑑み鋭意検討の結果なされたもので
あり、その目的とするところは、強度及び靭性に優れた
複合材料を提供する事である。
[Means for solving the problem] This invention was made in view of the above points and as a result of diligent study, and its purpose is to provide a composite material with excellent strength and toughness.

即ち本発明による第1の発明は、Al又はAl合金から
なるマトリックス金属中に、Afとセラミックス粒子又
は強化繊維との複合体が短繊維状に存在する事を特徴と
する複合材料であり、又第2の発明は、Aj!又はAl
合金の粉末と、Affiとセラミックス粒子又は強化繊
維との複合粉末を混合した後、熱間で圧粉後、押出加工
する事を特徴とするAl又はAl合金からなるマトリッ
クス金属中に、Alとセラミックス粒子又は強化繊維と
の複合体が短繊維状に存在する複合材料の製造方法であ
る。更に本発明による第3の発明は、Af又はAl1合
金とセラミックス粒子又は強化繊維とからなる複合体の
組織中に、AIlが短繊維状に存在するる事を特徴とす
る複合材料であり、更に又第4の発明は、Al2又はA
ffi合金とセラミックス粒子又は強化繊維とからなる
複合粉末と、Ajl!粉末を混合した後、熱間で圧粉後
、押出加工する事を特徴とするAJ又はAl合金とセラ
ミックス粒子又は強化繊維とからなる複合体の組織中に
、Alが短繊維状に存在する複合材料の製造方法である
。
In other words, the first invention according to the present invention is a composite material characterized in that a composite of Af and ceramic particles or reinforcing fibers exists in the form of short fibers in a matrix metal made of Al or an Al alloy, and the second invention is Aj! or Al
A method for producing a composite material in which a composite of Al and ceramic particles or reinforcing fibers exists in the form of short fibers in a matrix metal made of Al or an Al alloy, characterized by mixing alloy powder with a composite powder of Affi and ceramic particles or reinforcing fibers, hot-pressing the powder, and then extruding it. Furthermore, a third invention according to the present invention is a composite material characterized in that Al is present in the form of short fibers in the structure of a composite made of Af or Al1 alloy and ceramic particles or reinforcing fibers, and furthermore, a fourth invention is Al2 or A
This method for producing a composite material in which Al is present in the structure of a composite made of AJ or Al alloy and ceramic particles or reinforcing fibers is characterized by mixing a composite powder consisting of ffi alloy and ceramic particles or reinforcing fibers with Al powder, hot-pressing the powder, and then extruding it.

〔作用〕[Effect]

本発明による複合材料は、純Alを含む混合粉末を熱間
で圧粉後、押出加工して製造されているので、前記純A
lの粒子が押出方向に引き伸ばされて、短繊維状に存在
している。而して前記純Alの短繊維が亀裂の進行を阻
止する役割を果たす為、靭性が向上し、強化粒子又は強
化繊維の体積含有率V、を増して強度を向上さセても、
比較的大きな伸びを得る事が出来る。
The composite material according to the present invention is manufactured by hot-pressing a mixed powder containing pure Al and then extruding it, so the pure A
The particles l are stretched in the extrusion direction and exist as short fibers. Thus, the short fibers of pure Al play a role in preventing crack propagation, improving toughness, and even if the volume content V of reinforcing particles or reinforcing fibers is increased to improve strength,
It is possible to achieve relatively large growth.

〔実施例〕[Examples]

次に本発明を実施例により更に具体的に説明する。平均
粒径50amの7075合金粉と平均粒径1μmのSI
C粉末を原料とし、SiC粉末のVrニア0%として、
アトライターで5hr混合粉砕した。この様にして得ら
れた複合粉末をSEMで調べたところ、前記Al合金粉
は微粉化し、又粒内に平均粒径0,8μm位のSiC粉
子を取り込んでいた。前記複合粉末をN2雰囲気中で、
2ton/C4の圧力で圧粉してベレット状にし、酸化
を防止した。このペレットと平均粒径8oμmの純Al
粉末を、該純Affi粉末のV、が3o%になる様にし
て、アトライターで15分間混合し、比較的大きな純A
j!粒子を、SIC/A42合金複合粉末中に均一に分
散させた。この混合粉末を脱気用アルミニウム缶に充填
し、加熱脱気−熱間圧粉−缶体除去→熱間押出の工程に
より、全体とし”t’sicのVt:49%、Al及び
Al合金(7)V。
Next, the present invention will be described in more detail by reference to examples. 7075 alloy powder with an average particle size of 50 a m and SI with an average particle size of 1 μm
Using C powder as a raw material, with Vr nearly 0% of SiC powder,
The mixture was mixed and ground for 5 hours using an attritor. When the resulting composite powder was examined by SEM, it was found that the Al alloy powder had been pulverized, and that SiC particles with an average particle size of about 0.8 μm had been incorporated into the particles. The composite powder was then subjected to an N2 atmosphere.
The material was compacted into pellets at a pressure of 2 tons/C4 to prevent oxidation. These pellets were then mixed with pure aluminum with an average particle size of 80 μm.
The powder is mixed in an attritor for 15 minutes so that the V of the pure Affi powder is 30%, and relatively large pure A
The particles were uniformly dispersed in a SiC/A42 alloy composite powder. This mixed powder was filled into a degassing aluminum can, and the process of heating and degassing, hot compaction, can removal, and hot extrusion was carried out to obtain a mixture consisting of SiC Vt: 49%, Al and Al alloy (7) V.

:51%のMMCを得た。: A 51% MMC was obtained.

前記MMCについて、T、処理をした後強度を調べたと
ころ、引張強さは85 k g /ms”であり、伸び
は確実に2%以上であった。又組織的には、SiC/A
I!合金マトリックス中に、純Afの短いI&維が押出
方向に並んだ組織になっており、この純ANが亀裂の進
行を阻止する役割を果たしている為、全体として伸びが
向上している事が分かった。
Regarding the aforementioned MMC, after treatment, its strength was examined and found to be 85 kg/ms with an elongation of definitely more than 2%. Furthermore, its microstructure is SiC/A
I! It was found that the alloy matrix has a structure in which short pure Af I& fibers are aligned in the extrusion direction, and since this pure AN plays a role in inhibiting crack propagation, the overall elongation is improved.

〔発明の効果〕[Effects of the invention]

本発明による複合材料は、強度及び靭性に優れており、
工業上顕著な効果を奏するものである。
The composite material according to the present invention has excellent strength and toughness.
It will have a significant industrial effect.

Claims (4)

【特許請求の範囲】[Claims] (1)Al又はAl合金からなるマトリックス金属中に
、Alとセラミックス粒子又は強化繊維との複合体が短
繊維状に存在する事を特徴とする複合材料。
(1) A composite material characterized in that a composite of Al and ceramic particles or reinforcing fibers exists in the form of short fibers in a matrix metal made of Al or an Al alloy.
(2)Al又はAl合金の粉末と、Alとセラミックス
粒子又は強化繊維との複合粉末を混合した後、熱間で圧
粉後、押出加工する事を特徴とするAl又はAl合金か
らなるマトリックス金属中に、Alとセラミックス粒子
又は強化繊維との複合体が短繊維状に存在する複合材料
の製造方法。
(2) A method for producing a composite material in which a composite of Al and ceramic particles or reinforcing fibers exists in the form of short fibers in a matrix metal made of Al or an Al alloy, characterized by mixing Al or Al alloy powder with a composite powder of Al and ceramic particles or reinforcing fibers, hot-pressing the powder, and then extruding it.
(3)Al又はAl合金とセラミックス粒子又は強化繊
維とからなる複合体の組織中に、Alが短繊維状に存在
する事を特徴とする複合材料。
(3) A composite material characterized in that Al is present in the form of short fibers in the structure of a composite consisting of Al or an Al alloy and ceramic particles or reinforcing fibers.
(4)Al又はAl合金とセラミックス粒子又は強化繊
維とからなる複合粉末と、Al粉末を混合した後、熱間
で圧粉後、押出加工する事を特徴とするAl又はAl合
金とセラミックス粒子又は強化繊維とからなる複合体の
組織中に、Alが短繊維状に存在する複合材料の製造方
法。
(4) A method for producing a composite material in which Al is present in the structure of a composite made of Al or Al alloy and ceramic particles or reinforcing fibers, characterized by mixing Al powder with Al powder, hot-pressing the powder, and then extruding it.
JP19098487A 1987-07-30 1987-07-30 Composite material Ceased JPS6436734A (en)