MX3018E - Metodo mejorado de des oxidacion y/o de carburacion de un baño metalico - Google Patents
Metodo mejorado de des oxidacion y/o de carburacion de un baño metalicoInfo
- Publication number
- MX3018E MX3018E MX10010475U MX10010475U MX3018E MX 3018 E MX3018 E MX 3018E MX 10010475 U MX10010475 U MX 10010475U MX 10010475 U MX10010475 U MX 10010475U MX 3018 E MX3018 E MX 3018E
- Authority
- MX
- Mexico
- Prior art keywords
- gas
- nozzle
- deoxidation
- during
- carburation
- Prior art date
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21C—PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C21C7/00—Treating molten ferrous alloys, e.g. steel, not covered by groups C21C1/00 - C21C5/00
- C21C7/0025—Adding carbon material
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21C—PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C21C5/00—Manufacture of carbon-steel, e.g. plain mild steel, medium carbon steel or cast steel or stainless steel
- C21C5/28—Manufacture of steel in the converter
- C21C5/30—Regulating or controlling the blowing
- C21C5/34—Blowing through the bath
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Manufacturing & Machinery (AREA)
- Treatment Of Steel In Its Molten State (AREA)
- Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
- Investigating And Analyzing Materials By Characteristic Methods (AREA)
- Carbon Steel Or Casting Steel Manufacturing (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| FR7438955A FR2292771A1 (fr) | 1974-11-28 | 1974-11-28 | Methode d'injection d'une poudre apportant du carbone dans un bain metallique |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| MX3018E true MX3018E (es) | 1980-02-07 |
Family
ID=9145325
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| MX10010475U MX3018E (es) | 1974-11-28 | 1975-11-27 | Metodo mejorado de des oxidacion y/o de carburacion de un baño metalico |
Country Status (13)
| Country | Link |
|---|---|
| JP (1) | JPS51142411A (2) |
| BE (1) | BE836110A (2) |
| BR (1) | BR7507824A (2) |
| CA (1) | CA1067293A (2) |
| DD (1) | DD121650A5 (2) |
| DE (1) | DE2550467B2 (2) |
| ES (1) | ES442800A1 (2) |
| FR (1) | FR2292771A1 (2) |
| GB (1) | GB1510500A (2) |
| HU (1) | HU174689B (2) |
| IT (1) | IT1050909B (2) |
| LU (1) | LU73871A1 (2) |
| MX (1) | MX3018E (2) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4330326A (en) * | 1979-08-24 | 1982-05-18 | Eisenwerk-Gesellschaft Maximilianshutte Mbh. | Method and a means for introducing close-grained carbonaceous fuels into a molten iron bath |
| JPS57110608A (en) * | 1980-12-26 | 1982-07-09 | Kawasaki Steel Corp | Method for deoxidation in bottom blown converter |
| DE3143795C2 (de) * | 1981-11-04 | 1983-10-20 | Klöckner Stahlforschung GmbH, 8458 Sulzbach-Rosenberg | "Ventil zur Strömungsmittelzufuhr" |
| JPS5884916A (ja) * | 1981-11-13 | 1983-05-21 | Kawasaki Steel Corp | 底吹転炉加炭方法 |
| CN112226576B (zh) * | 2020-09-27 | 2023-07-14 | 甘肃酒钢集团宏兴钢铁股份有限公司 | 一种利用挡渣系统喷碳脱氧的装置及方法 |
-
1974
- 1974-11-28 FR FR7438955A patent/FR2292771A1/fr active Granted
-
1975
- 1975-11-05 HU HU75CE1062A patent/HU174689B/hu unknown
- 1975-11-10 DE DE19752550467 patent/DE2550467B2/de not_active Ceased
- 1975-11-18 IT IT6984375A patent/IT1050909B/it active
- 1975-11-19 GB GB4763975A patent/GB1510500A/en not_active Expired
- 1975-11-19 ES ES442800A patent/ES442800A1/es not_active Expired
- 1975-11-21 JP JP14009975A patent/JPS51142411A/ja active Granted
- 1975-11-26 CA CA240,539A patent/CA1067293A/fr not_active Expired
- 1975-11-26 DD DD18971075A patent/DD121650A5/xx unknown
- 1975-11-26 BR BR7507824A patent/BR7507824A/pt unknown
- 1975-11-26 LU LU73871A patent/LU73871A1/xx unknown
- 1975-11-27 MX MX10010475U patent/MX3018E/es unknown
- 1975-11-28 BE BE162310A patent/BE836110A/xx unknown
Also Published As
| Publication number | Publication date |
|---|---|
| ES442800A1 (es) | 1977-04-16 |
| DE2550467B2 (de) | 1977-10-20 |
| HU174689B (hu) | 1980-03-28 |
| BE836110A (fr) | 1976-05-28 |
| LU73871A1 (2) | 1976-06-11 |
| JPS5518765B2 (2) | 1980-05-21 |
| FR2292771A1 (fr) | 1976-06-25 |
| GB1510500A (en) | 1978-05-10 |
| JPS51142411A (en) | 1976-12-08 |
| BR7507824A (pt) | 1976-08-10 |
| IT1050909B (it) | 1981-03-20 |
| FR2292771B1 (2) | 1977-03-25 |
| DD121650A5 (2) | 1976-08-12 |
| CA1067293A (fr) | 1979-12-04 |
| DE2550467A1 (de) | 1976-08-12 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| MX168124B (es) | Mejoras en una mezcla de cuatro gases para usarse en un proceso de soldadura | |
| ES442956A1 (es) | Un metodo de soldadura electrica de arco protegido con gas, de gran intensidad de corriente. | |
| GB1305426A (2) | ||
| MX3018E (es) | Metodo mejorado de des oxidacion y/o de carburacion de un baño metalico | |
| FR2366373A1 (fr) | Alliage ferritique a haute resistance | |
| GB999799A (en) | Purification of gases | |
| GB897608A (en) | Improvements in and relating to oxygen detecting electrodes and methods employing the same | |
| GB546961A (en) | Improvements in or relating to electric arc welding | |
| ES445034A1 (es) | Metodo de soldadura con arco sumergido. | |
| GB1532217A (en) | Welding and a steel suitable for use therein | |
| GB934112A (en) | An improved blowing lance | |
| GB1007241A (en) | Improvements in or relating to a blowing device for carrying out metallurgical processes particularly for refining crude iron | |
| JPS545837A (en) | Seamless wire with high toughness for arc welding | |
| BE752632A (en) | Pneumatically converting cast iron to low - carbon steel | |
| SU427083A1 (ru) | Смесь для раскисления стали | |
| SU148171A1 (ru) | Шихта порошковой проволоки | |
| FR2162567A1 (en) | Arc welding pipes internally - with parallel leads to avoid magnetic disturbance of arc | |
| ES431671A1 (es) | Un metodo para refinar metal ferroso fundido. | |
| SU80437A1 (ru) | Способ стыковой сварки | |
| JPS51140814A (en) | Decarburization of molten steel at reduced pressur | |
| ES302274A1 (es) | Un procedimiento para el afino de hierro. | |
| GB791974A (en) | Improvements in or relating to the welding of ferrous metals | |
| SU562403A1 (ru) | Электродное покрытие | |
| ES328388A1 (es) | Un procedimiento para la soldadura por arco sumergido de aceros al niquel. | |
| GB872995A (en) | Process for purifying silicon or a ferro-silicon alloy |