A MOLTEN GLASS MATERIAL (10) WHICH IS DISCHARGED OUTWARD FROM A GLASS MELTING FURNACE AND USED TO MOLD A GLASSWORK PIECE, AND A METHOD AND APPARATUS FOR MANUFACTURING THE SAME, WHEREIN THE GLASS MELTING FURNACE INCLUDES A FURNACE MAIN BODY (1) HAVING AN OPENING PORTION FOR INTRODUCING A SOLID GLASS MATERIAL IN A SOLID STATE TO THE FURNACE MAIN BODY, A HEATER (82,88) FOR MAINTAINING AN INTERIOR OF THE FURNACE MAIN BODY AT A PREDETERMINED SET TEMPERATURE TO HEAT AND MELT THE SOLID GLASS MATERIAL, A GLASS MELTING TANK (5) DISPOSED IN THE FURNACE MAIN BODY TO STORE THE MOLTEN GLASS MATERIAL MOLTEN BY THE HEATER, AND A COMMUNICATION MEMBER (13) FOR ISOLATING A GAP BETWEEN A LIQUID SURFACE OF THE MOLTEN GLASS MATERIAL IN THE GLASS MELTING TANK AND THE OPENING PORTION FROM THE LIQUID SURFACE( 11), AND THE MOLTEN GLASS MATERIAL IS OBTAINED BY INTRODUCING THE SOLID GLASS MATERIAL TO THE GLASS MELTING TANK THROUGH THE COMMUNICATION MEMBER.(FIG 1)
MYPI96000814A1995-03-071996-03-05Molten glass material and method and apparatus for manufacturing the same
MY133524A