MY137675A - Control of hot rolled product cross section under localized temperature disturbances - Google Patents

Control of hot rolled product cross section under localized temperature disturbances

Info

Publication number
MY137675A
MY137675A MYPI20061814A MY137675A MY 137675 A MY137675 A MY 137675A MY PI20061814 A MYPI20061814 A MY PI20061814A MY 137675 A MY137675 A MY 137675A
Authority
MY
Malaysia
Prior art keywords
weld joint
roll
control
hot rolled
rolled product
Prior art date
Application number
Inventor
Pong David Teng
Maylor Thomas George
Raftsjo Erik Mats
Original Assignee
Pong David Teng
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Pong David Teng filed Critical Pong David Teng
Priority to MYPI20061814 priority Critical patent/MY137675A/en
Publication of MY137675A publication Critical patent/MY137675A/en

Abstract

A METHOD OF ROLLING A CONTINUOUS WELDED BILLET HAVING WELD JOINTS AT SUCCESSIVE LOCATIONS ALONG THE BILLET AND WHEREIN THE CONTINUOUS WELDED BILLET IS ADVANCED THROUGH ROLL PAIRS OF SUCCESSIVE ROLL STANDS. THE ROLLING CONDITIONS IN TWO SUCCESSIVE STANDS ARE ADJUSTED SO THAT WHEN A WELD JOINT IS BETWEEN THE TWO STANDS COMPRESSION IS PRODUCED AT THE WELD JOINT CAUSING AN INCREASE OF CROSS-SECTIONAL AREA AT THE WELD JOINT; THE ROLLING CONDITION INVOLVES SUPERIMPOSING AN INCREASE IN ROLL SPEED IN THE UPSTREAM ROLL STAND COMPARED TO THE DOWNSTREAM ROLL STAND BASED ON TRACKING INFORMATION OF THE WELD JOINT.
MYPI20061814 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances MY137675A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
MYPI20061814 MY137675A (en) 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
MYPI20061814 MY137675A (en) 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances

Publications (1)

Publication Number Publication Date
MY137675A true MY137675A (en) 2009-02-27

Family

ID=45689176

Family Applications (1)

Application Number Title Priority Date Filing Date
MYPI20061814 MY137675A (en) 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances

Country Status (1)

Country Link
MY (1) MY137675A (en)

Similar Documents

Publication Publication Date Title
CN106311754B (en) Emulsion flow dynamics integrated optimization and setting method suitable for tandem mills
PL1694449T3 (en) Control of hot rolled product cross section under localized temperature disturbances
MY180966A (en) Winding/unwinding device and method for winding/unwinding a metal product in a rolling line
EP0738548B1 (en) Hot-rolling method of steel piece joint during continuous hot-rolling
CN104772344B (en) Hot rolling synchronous mode heavy side press tracking
CN102581031A (en) Inner-source driven comprehensive shape and thickness regulation mill
WO2011018217A3 (en) Device and method for producing a thin hot-rolled strip
WO2012013456A3 (en) Apparatus and method for production of metal elongated products.
US10464111B2 (en) Method of forming tailored cast blanks
ZA200709611B (en) Method of continuously rolling a product exiting from an upstream roll stand at a velocity higher than the take in velocity of a downstream roll stand
ATE247534T1 (en) METHOD FOR REDUCING THE LENGTH OF SCRAP WHEN ROLLING METAL STRIPS CONNECTED BY WELDS AND TANDEM LINE FOR IMPLEMENTING THE METHOD
UA99295C2 (en) Rolling mill with cooling device and rolling method
IN2012DN02260A (en)
CN102755999A (en) Interstand cooling device for hot-rolled H-shaped steel
CN106269913B (en) Method for preventing strip steel from deviating for working roll transverse moving rolling mill
WO2008142803A1 (en) Method, and apparatus, for piercing and rolling seamless pipe
WO2009056712A8 (en) Method and equipment for secondary descaling of metallic strips by hydraulic low-pressure spraying of water
WO2010066230A3 (en) Method for producing seamless tubes by means of a three-roll bar rolling mill
CN104324952B (en) Hot continuous rolling thin specification rolling machine frame load relay control method
Lestani et al. Technology and benefits of the endless welding rolling process for the production of hot-rolled long products
UA71395U (en) Method of production of cold rolled strips
CA2427097A1 (en) Uninterrupted continuous rolling of bar and rod products
TW200722749A (en) Device for the ultrasonic testing of hot rolled material
UA92241C2 (en) Method of continuous longitudinal rolling of pipes in multiple-stand mill on mandrel
TW200611760A (en) Method of continuously hot rolling a heated billet into a plurality of finished products